The corrosion of Fe-15 wt% Y and Fe-30 wt% Y in sulfidizing-oxidizing atmospheres at 600-800°C

被引:4
|
作者
Niu, Y
Gesmundo, F
Yan, R
Wu, W
机构
[1] Univ Genoa, Ist Chim, I-16129 Genoa, Italy
[2] State Key Lab Corros & Protect, Shenyang 110015, Peoples R China
基金
中国国家自然科学基金;
关键词
iron; yttrium; alloys; sulfidation; oxidation;
D O I
10.1016/S0010-938X(98)00170-X
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion of two iron-based alloys containing 15 and 30 wt% yttrium and of pure yttrium has been studied at 600-800 degrees C in H-2-H2S-CO2 mixtures under a sulfur pressure of 10(-8) atm and an oxygen pressure of 10(-24) atm at 600 degrees C and of 10(-20) atm at 700-800 degrees C to establish the effect of yttrium additions on the resistance of pure iron to mixed sulfidizing-oxidizing atmospheres of high sulfur potential. The presence of yttrium is only slightly beneficial, since even a yttrium content of 30 wt% can only reduce the corrosion rate of iron to a limited extent at 600 and 800 degrees C, but not at 700 degrees C. More precisely, at 600 and 700 degrees C, when yttrium shows breakaway, the alloys corrode more rapidly than pure yttrium at short times, but presumably more slowly at long times. On the contrary, at 800 degrees C, when yttrium behaves protectively, the two alloys corrode considerably more rapidly than pure yttrium. Under all conditions the two alloys form an external FeS layer overlying a very complex intermediate region containing a mixture of the compounds of the two metals and an innermost zone of internal attack containing compounds of yttrium with both oxygen and sulfur, Thus, iron can still diffuse through the intermediate region at nonnegligible rates to form the outer FeS layer. The scaling behavior of these alloys is discussed by taking into account the limited solubility of yttrium in iron as well as the presence of intermetallic Fe-Y compounds. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:989 / 1012
页数:24
相关论文
共 50 条
  • [41] The Oxidation of Four Co-20Ni-xCr-yAl (x=8,15 wt.%; y=3,5 wt.%) Alloys Under 1 atm O2 at 800 °C and 900 °C
    Lv, Y. L.
    Ren, Y. J.
    Zhou, M. N.
    Feng, K. K.
    Chen, J.
    Niu, Y.
    OXIDATION OF METALS, 2022, 97 (5-6): : 599 - 627
  • [42] The Oxidation of Four Co-20Ni-xCr-yAl (x = 8,15 wt.%; y = 3,5 wt.%) Alloys Under 1 atm O2 at 800 °C and 900 °C
    Y. L. Lv
    Y. J. Ren
    M. N. Zhou
    K. K. Feng
    J. Chen
    Y. Niu
    Oxidation of Metals, 2022, 97 : 599 - 627
  • [43] THE CORROSION OF FE, CO AND NI-ALLOYS CONTAINING 15 AND 30 WT-PERCENT NB IN H2-H2S MIXTURES UNDER 10(-8) ATM S2 AT 600-DEGREES-C
    NIU, Y
    GESMUNDO, F
    VIANI, F
    SOLID STATE IONICS, 1993, 63-5 : 765 - 771
  • [44] Corrosion of Fe-(4.8, 9.2, 14.3) Wt%Al alloys at 700 and 800 °C in N2/H2O/H2S gases
    Min Jung Kim
    Dong Bok Lee
    Metals and Materials International, 2013, 19 : 975 - 982
  • [45] Corrosion of Fe-(4.8,9.2,14.3) Wt%Al alloys at 700 and 800 A°C in N2/H2O/H2S gases
    Kim, Min Jung
    Lee, Dong Bok
    METALS AND MATERIALS INTERNATIONAL, 2013, 19 (05) : 975 - 982
  • [46] Corrosion behavior of Fe41Co7Cr15Mo14C15B6Y2 bulk metallic glass in NaCl solution
    Wang, Li
    Chao, Yuesheng
    MATERIALS LETTERS, 2012, 69 : 76 - 78
  • [47] Corrosion Behaviors of Bulk Amorphous Fe41Co7Cr15Mo14C15B6Y2 Alloy in HCl Solution
    Wang Li
    Fan Hongbo
    Li Jing
    Zheng Wei
    Chao Yuesheng
    Shen Jun
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 (11) : 1992 - 1996
  • [48] Corrosion of Fe-(9∼37) wt. %Cr Alloys at 700-800 °C in (N2, H2O, H2S)-Mixed Gas
    Kim, Min Jung
    Abro, Muhammad Ali
    Lee, Dong Bok
    METALS, 2016, 6 (11):
  • [49] Corrosion Behavior of Fe41Co7Cr15Mo14C15B6Y2 Bulk Metallic Glass in Sulfuric Acid Solutions
    Fan, H. B.
    Zheng, W.
    Wang, G. Y.
    Liaw, P. K.
    Shen, J.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (06): : 1524 - 1533
  • [50] Corrosion behaviors of bulk amorphous Fe41Co7Cr15 Mo14C15B6Y2 alloy in HCl solution
    Wang, Li
    Fan, Hongbo
    Li, Jing
    Zheng, Wei
    Chao, Yuesheng
    Shen, Jun
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2009, 38 (11): : 1992 - 1996