Fracture bone healing and biodegradation of AZ31 implant in rats

被引:29
|
作者
Iglesias, C. [1 ]
Bodelon, O. G. [2 ]
Montoya, R.
Clemente, C. [3 ]
Garcia-Alonso, M. C. [2 ]
Rubio, J. C. [4 ]
Escudero, M. L. [2 ]
机构
[1] Hosp Univ La Paz, Dept Plast Surg, Madrid 28046, Spain
[2] CSIC, Dept Surface Engn Corros & Durabil, Natl Ctr Met Res CENIM, E-28040 Madrid, Spain
[3] Univ Alcala de Henares, Sch Med, Dept Human Anat & Embryol, Madrid, Spain
[4] Hosp Univ La Paz, Dept Trauma & Orthoped Surg, Madrid 28046, Spain
关键词
AZ31 magnesium alloy; fracture healing; biodegradation; tomography; histomorphometry; in vivo; IN-VIVO CORROSION; MAGNESIUM ALLOYS; MECHANICAL-PROPERTIES; VITRO CORROSION; GRAIN-SIZE; MG ALLOYS; CA ALLOY; DEGRADATION; BEHAVIOR; BIOCOMPATIBILITY;
D O I
10.1088/1748-6041/10/2/025008
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The ideal temporary implant should offer enough mechanical support to allow healing of the fracture and then biodegrade and be resorbed by metabolic mechanisms without causing any toxic effect. The aim of this research has been to simultaneously study in situ bone healing and the biodegradation of AZ31 Mg alloy as an osteosynthesis material. The in vivo study was carried out in AZ31 implants with and without Mg-fluoride coating inserted in un-fractured and fractured femurs of Wistar rats for long experimentation time, from 1 to 13 months, by means of computed tomography, histological and histomorphometric analysis. Tomography analysis showed the bone healing and biodegradation of AZ31 implants. The fracture is healed in 100% of the animals, and AZ31 maintains its mechanical integrity throughout the healing process. Biodegradation was monitored, quantifying the evolution of gas over time by 3D composition of tomography images. In all the studied groups, gas pockets disappear with time as a result of the diffusion process through soft tissues. Histomorphometric studies reveal that after 13 months the 46.32% of AZ31 alloy has been resorbed. The resorption of the coated and uncoated AZ31 implants inserted in fractured femurs after 1, 9 and 13 months does not have statistically significant differences. There is a balance between the biodegradation of AZ31 and bone healing which allows the use of AZ31 to be proposed as an osteosynthesis material.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Ketorolac Loaded Poly(lactic-co-glycolic acid) Coating of AZ31 in the Treatment of Bone Fracture Pain
    Puccetti, Matteo
    Cusati, Eleonora
    Antognelli, Cinzia
    Ricci, Maurizio
    Ambrogi, Valeria
    Schoubben, Aurelie
    POLYMERS, 2023, 15 (10)
  • [42] Friction stir processing of AZ31 alloy to improve the mechanical, biodegradation, and in vitro biocompatible characteristics
    Sonia, Pankaj
    Jain, Jinesh K.
    Alla, Naveenkrishna
    Gupta, Manish
    Siddiqui, Md Irfanul Haque
    Salem, Karrar Hazim
    Ahmed, Farooq
    Abdullaev, Sherzod Shukhratovich
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2024, 38 (11) : 1974 - 1999
  • [43] Development of an active intramedullary implant in bone fracture healing
    Beier, Th.
    Richard, H.A.
    Kullmer, G.
    VDI Berichte, 2001, (1631): : 331 - 352
  • [44] Extrusion of AZ31 Magnesium Sheet
    Gall, Sven
    Mueller, Soeren
    Reimers, Walter
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 1530 - +
  • [45] Direct and indirect extrusion of AZ31
    Mueller, KB
    MAGNESIUM TECHNOLOGY 2002, 2002, : 187 - 192
  • [46] XRD studies of electrochemically hydrided-dehydrided thin films of the alloy AZ31 and AZ31 with Ti
    Juskenas, R.
    Kapocius, V.
    Miecinskas, P.
    Karpaviciene, V.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 467 (1-2) : 524 - 527
  • [47] Microstructure and Mechanical Properties of AZ31/SiC and AZ31/CNT Composites Produced by Friction Stir Processing
    Nia, A. Alavi
    Nourbakhsh, S. H.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (07) : 1435 - 1442
  • [48] Microstructure and Mechanical Properties of AZ31/SiC and AZ31/CNT Composites Produced by Friction Stir Processing
    A. Alavi Nia
    S. H. Nourbakhsh
    Transactions of the Indian Institute of Metals, 2016, 69 : 1435 - 1442
  • [49] Fracture behavior of AZ31 magnesium alloy sheet in deep drawing at room temperature
    Cheng, Yong-Qi
    Chen, Zhen-Hua
    Xia, Wei-Jun
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2009, 30 (06): : 89 - 93
  • [50] Plasticity and fracture mechanism of refine-grain AZ31 magnesium alloys sheet
    Wang Bo-jian
    Zhang Yao-dan
    Li Shan
    ADVANCED MATERIALS, PTS 1-3, 2012, 415-417 : 1096 - +