Effects of sintering temperature and V2O5 additive on the properties of SiC-Al2O3 ceramic foams

被引:58
|
作者
Ren, Xinming [1 ]
Ma, Beiyue [1 ]
Zhang, Yaran [1 ]
Zhu, Qiang [2 ]
Li, Dongxu [1 ]
Li, Shiming [1 ]
Yuan, Lei [1 ]
Yu, Jingkun [1 ]
Liu, Guoqi [3 ]
Li, Hongxia [3 ]
机构
[1] Northeastern Univ, Sch Met, Shenyang 110819, Liaoning, Peoples R China
[2] Univ New South Wales, Electron Microscope Unit, Mark Wainwright Analyt Ctr, Sydney, NSW 2032, Australia
[3] Sinosteel Luoyang Inst Refractories Res Co Ltd, State Key Lab Adv Refractories, Luoyang 471039, Peoples R China
基金
中国国家自然科学基金;
关键词
SiC-Al2O3; V2O5; Sintering; Porosity; Strength; Polymeric foam replication method; Y2O3; ADDITION;
D O I
10.1016/j.jallcom.2017.10.170
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, a series of SiC-Al2O3 ceramic foams (SACFs) were fabricated from the powders of commercial silicon carbide and fused white corundum by polymeric foam replication method combined with reaction sintering process. Effects of sintering temperature (1250 degrees C-1350 degrees C) and addition amounts of V2O5 (0-3 wt%) on the sintering properties and post-sintering properties of as-prepared SACFs such as appearances, microstructures, phase compositions, apparent porosity, bulk density, cold compressive strength and thermal shock resistance have been investigated. During the sintering process, SiC was oxidized in air and formed SiO2, then part of as-formed SiO2 reacted with Al2O3 to produce Al6Si2O13 ceramic phase. The mechanical properties of as-prepared SACFs were found to be remarkably increased due to the increase of the sintering temperature and the introduction of V2O5. The phase transformation towards mullite was also found to be promoted, and the mullitization temperature was reduced because of the formation of Si-rich liquid phase due to the addition of V2O5. The improvements in sintering properties, cold compressive strength and thermal shock resistance of as-prepared SACFs were attributed to the formation of mullite and silica ceramic bonding phases in the ceramic matrix during the sintering process in air. The SACFs doped with 1 wt% V2O5 and sintered at 1450 degrees C for 2 h, achieved their maximum cold compressive strength of 2.45 MPa, and the apparent porosity was still 69.08%. Crown Copyright (C) 2017 Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:716 / 724
页数:9
相关论文
共 50 条
  • [21] Adsorption of benzene on the V2O5/γ-Al2O3 catalyst
    L. D. Asnin
    A. A. Fedorov
    Yu. S. Chekryshkin
    Russian Chemical Bulletin, 2003, 52 : 889 - 892
  • [22] ACTIVITIES OF V2O5/TIO2 AND V2O5/AL2O3 CATALYSTS FOR THE REACTION OF NO AND NH3 IN THE PRESENCE OF O2
    INOMATA, M
    MIYAMOTO, A
    UI, T
    KOBAYASHI, K
    MURAKAMI, Y
    INDUSTRIAL & ENGINEERING CHEMISTRY PRODUCT RESEARCH AND DEVELOPMENT, 1982, 21 (03): : 424 - 428
  • [23] Adsorption of benzene on the V2O5/γ-Al2O3 catalyst
    Asnin, LD
    Fedorov, AA
    Chekryshkin, YS
    RUSSIAN CHEMICAL BULLETIN, 2003, 52 (04) : 889 - 892
  • [24] INTERACTION OF PROPYLENE WITH A V2O5/AL2O3 CATALYST
    DAVYDOV, AA
    BUDNEVA, AA
    REACTION KINETICS AND CATALYSIS LETTERS, 1982, 20 (1-2): : 107 - 112
  • [25] ETCHING OF AL2O3 SURFACES WITH MOLTEN V2O5
    SAFDAR, M
    FRISCHAT, GH
    SALGE, H
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1974, 57 (02) : 106 - 106
  • [26] Adsorption of chlorobenzene on V2O5/γ-Al2O3 catalyst
    Asnin, LD
    Fedorov, AA
    Chekryshkin, YS
    Yakushev, RM
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2001, 74 (09) : 1458 - 1460
  • [27] Electrostatically assembled SiC-Al2O3 composite particles for direct selective laser sintering
    Tan, Wai Kian
    Kuwana, Takaya
    Yokoi, Atsushi
    Kawamura, Go
    Matsuda, Atsunori
    Muto, Hiroyuki
    ADVANCED POWDER TECHNOLOGY, 2021, 32 (06) : 2074 - 2084
  • [28] SiC-Al2O3 nanocomposites superfast densified by SPS
    Gao, LA
    Wang, HZ
    Hong, JS
    Miyamoto, H
    De la Torre, SD
    JOURNAL OF INORGANIC MATERIALS, 1999, 14 (01) : 55 - 60
  • [29] Production of abrasive materials in the SiC-Al2O3 system
    Pushkarev, OI
    REFRACTORIES AND INDUSTRIAL CERAMICS, 2002, 43 (11-12) : 371 - 373
  • [30] Production of abrasive materials in system of SiC-Al2O3
    Pushkarev, O.I.
    Ogneupory i Tekhnicheskaya Keramika, 2002, (12): : 8 - 10