Pressureless sintering of Al2O3/Ni nanocomposites

被引:65
|
作者
Chen, RZ [1 ]
Tuan, WH [1 ]
机构
[1] Natl Taiwan Univ, Inst Mat Sci & Engn, Taipei 10764, Taiwan
关键词
sintering; Al2O3; strength; microstructure-final; nanocomposites;
D O I
10.1016/S0955-2219(98)00213-1
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the present study, an Al2O3/Ni nanocomposite containing 5 vol% Ni is prepared by pressureless sintering at 1400 degrees C for 2 h. Most nickel inclusions, around 70% in the sintered nanocomposite, locate at the intergranular sites, the triple junctions and Al2O3/Al2O3 grain boundaries. The average size of the nickel inclusions at the triple junctions, grain boundaries and intragranular locations is 145, 131 and 73 nm, respectively. The average size of all nickel inclusions is 118 nm. The presence of nickel inclusions can prohibit the grain growth of matrix grains. The size of Al2O3 grains in the sintered nanocomposite is only 490 nm. The strength of the nanocomposite is thus high for the refined microstructure. The matrix Al2O3 grains and Ni inclusions at triple junctions underwent considerable coarsening during a post-annealing treatment at 1300 degrees C for 2 h. The strength of the annealed composites is thus reduced significantly after annealing. (C) 1999 Elsevier Science Limited. All rights reserved.
引用
收藏
页码:463 / 468
页数:6
相关论文
共 50 条
  • [41] Investigation of Al2O3/Cr3C2 composites prepared by pressureless sintering .2.
    Huang, JL
    Twu, KC
    Lii, DF
    Li, AK
    MATERIALS CHEMISTRY AND PHYSICS, 1997, 51 (03) : 211 - 215
  • [42] Investigation of Al2O3/Cr3C2 composites prepared by pressureless sintering (Part 2)
    Natl Cheng-Kung Univ, Tainan, Taiwan
    Mater Chem Phys, 3 (211-215):
  • [43] PRESSURELESS SINTERING OF TIC-AL2O3 COMPOSITES
    ISHIGAKI, T
    SATO, K
    MORIYOSHI, Y
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1989, 8 (06) : 678 - 680
  • [44] Spark plasma sintering of layered γ-Al2O3/graphene reinforced nanocomposites
    Shamshirgar, Ali Saffar
    Ivanov, Roman
    Hussainova, Irina
    PROCEEDINGS OF THE ESTONIAN ACADEMY OF SCIENCES, 2019, 68 (02) : 140 - 144
  • [45] Fabrication and characterization of nano-Y2O3 and Al2O3 dispersed W-Ni alloys by mechanical alloying and pressureless conventional sintering
    Talekar, V. R.
    Patra, A.
    Karak, S. K.
    7TH NATIONAL CONFERENCE ON PROCESSING AND CHARACTERIZATION OF MATERIALS (NCPCM 2017), 2018, 338
  • [46] SINTERING MECHANISMS IN AL2O3
    DYNYS, JM
    CANNON, RM
    COBLE, RL
    AMERICAN CERAMIC SOCIETY BULLETIN, 1977, 56 (03): : 291 - 291
  • [47] MICROWAVE SINTERING OF AL2O3
    VODEGEL, S
    HANNAPPEL, C
    WILLERTPORADA, M
    METALL, 1994, 48 (03): : 206 - 210
  • [48] Pixelated sintering of ?-Al2O3
    Cornu, Inaki
    Cheype, Maxime
    Baudier-Pons, Marion
    Leon, Jean-Francois
    Couillaud, Samuel
    Rossignol, Fabrice
    Heintz, Jean-Marc
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (13) : 5885 - 5892
  • [49] Multistage sintering approach to prepare Ni3Al/α-Al2O3 composites
    Chen-Ti Hu
    Wen-Chih Chiou
    Metallurgical and Materials Transactions A, 2001, 32 : 407 - 415
  • [50] Multistage sintering approach to prepare Ni3Al/α-Al2O3 composites
    Hu, CT
    Chiou, WC
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (02): : 407 - 415