Microstructure and mechanical properties of Al/Ti/Al laminated composites prepared by roll bonding

被引:120
|
作者
Ma, M. [1 ]
Huo, P. [1 ]
Liu, W. C. [1 ]
Wang, G. J. [2 ]
Wang, D. M. [2 ]
机构
[1] Yanshan Univ, Coll Mat Sci & Engn, Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[2] Northeast Light Alloy Co Ltd, Harbin 150060, Heilongjiang, Peoples R China
基金
国家高技术研究发展计划(863计划);
关键词
Laminated metal composites; Roll bonding; Microstructure; Mechanical properties; THICKNESS TEXTURE GRADIENTS; ALUMINUM-ALLOY; SHEAR STRAIN; CARBON STEEL; DEFORMATION; EVOLUTION; CU; INHOMOGENEITY; STRENGTH; REFINEMENT;
D O I
10.1016/j.msea.2015.03.086
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Al 6061/Ti-6Al-4V/Al 6061 laminated composites were fabricated by hot-roll bonding. The effect of rolling temperature and reduction on the microstructure and mechanical properties of Al/Ti/Al laminated composites was investigated. The results show that the Al/Ti/Al laminated composites exhibited a good Al/Ti interfacial bonding. The reduction ratio of Ti to Al layer decreased with increasing rolling temperature and reduction. The development of microstructure through the thickness of Al layer was inhomogeneous. The number of high-angle boundaries and the misorientation angle across lowangle boundaries increased as the thickness position moved towards the surface of Al layer from the interface of Al/Ti. The initial grains near the surface of Al layer were markedly elongated at a certain angle to the RD and then fragmented into the equiaxed fine grains at larger rolling reductions. This inhomogeneity of microstructure can be attributed to the effect of the friction between the roll and sheet surface and the uncoordinated deformation between Al and Ti layers. The deformation inhomogeneity increased with increasing rolling reduction. For the laminated composites fabricated with rolling reductions of 27% and 38%, the yield and tensile strength increased to a maximum value at about 400 degrees C and then decreased with increasing rolling temperature. The laminated composites fabricated with a 45% reduction possessed lower strength in the temperature range from 400 degrees C to 450 degrees C than those with a 38% reduction due to the fracture of Ti layer. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:301 / 310
页数:10
相关论文
共 50 条
  • [11] Microstructures and mechanical properties of Mg/Mg and Mg/Al/Mg laminated composites prepared via warm roll bonding
    Liu, C. Y.
    Wang, Q.
    Jia, Y. Z.
    Jing, R.
    Zhang, B.
    Ma, M. Z.
    Liu, R. P.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 1 - 8
  • [12] Microstructure and mechanical properties of Tr-metal Al/Ti/Mg laminated composite processed by accumulative roll bonding
    Motevalli, Parisa Darvish
    Eghbali, Beitallah
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 628 : 135 - 142
  • [13] Effect of TiC content on the microstructure, texture and mechanical properties of the 6061Al-TiC/6061Al laminated composites prepared by spark plasma sintering and roll bonding
    Sun, Haiyang
    Ou, Junfei
    Cheng, Liang
    Sun, Lingyan
    Lu, Yalin
    Liu, Wenchang
    JOURNAL OF MATERIALS SCIENCE, 2024, 59 (31) : 14367 - 14382
  • [14] Microstructure and mechanical behaviors of Al/Cu laminated composites fabricated by accumulative roll bonding and intermediate annealing
    Xu, Runrun
    Liang, Ningning
    Zhuang, Limin
    Wei, Dajie
    Zhao, Yonghao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 832
  • [15] Microstructure and mechanical properties of laminated Al–Cu–Mg composite fabricated by accumulative roll bonding
    Parisa Darvish Motevalli
    Beitallah Eghbali
    Bulletin of Materials Science, 2017, 40 : 1481 - 1488
  • [16] Microstructure and mechanical properties of the Mg/Al laminated composite fabricated by accumulative roll bonding (ARB)
    Wu, K.
    Chang, H.
    Maawad, E.
    Gan, W. M.
    Brokmeier, H. G.
    Zheng, M. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (13-14): : 3073 - 3078
  • [17] Comparison of Rolling and Transverse Direction Properties of Al/Ti Laminated Metal Composites Prepared by Cold Roll Bonding and Subsequent Annealing
    Chen, Chu
    Hu, Meijun
    Hong, Weiwei
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2024, : 3739 - 3749
  • [18] Effect of Interface on Mechanical Properties of Ti/Al/Mg/Al/Ti Laminated Composites
    Cao, Miao
    Wang, Cui-ju
    Deng, Kun-kun
    Nie, Kai-bo
    Liang, Wei
    Wu, Yu-cheng
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2020, 23 (01):
  • [19] Microstructure and mechanical properties of laminated Al-Cu-Mg composite fabricated by accumulative roll bonding
    Motevalli, Parisa Darvish
    Eghbali, Beitallah
    BULLETIN OF MATERIALS SCIENCE, 2017, 40 (07) : 1481 - 1488
  • [20] Effects of Sinusoidal Vibration of Crystallization Roller on Microstructure and Mechanical Properties of Ti/Al Laminated Composites by Twin-Roll Casting
    Li, Li
    Du, Fengshan
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2023, 76 (08) : 2073 - 2083