Evaluation on Tensile and Fatigue Crack Growth Performances of Ti6A14V Alloy Produced by Selective Laser Melting

被引:39
|
作者
Jiao, Z. H. [1 ]
Xu, R. D. [1 ]
Yu, H. C. [1 ]
Wu, X. R. [1 ]
机构
[1] Beijing Inst Aeronaut Mat, Aviat Key Lab Sci & Technol Mat Testing & Evaluat, Sci & Technol Adv High Temp Struct Mat Lab, Beijing Key Lab Aeronaut Mat Testing & Evaluat, Beijing 100095, Peoples R China
关键词
SLM; tensile properties; fatigur crack growth; anisotropy; elevated temperature; FRACTURE-TOUGHNESS; PROPAGATION; TITANIUM;
D O I
10.1016/j.prostr.2017.11.069
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Additive manufacturing (AM) technologies are increasing in importance for aerospace application, where the demand for a fundamental understanding and predictability of static and dynamic material properties are high. As the most widely used and studied alloy for this technology, Selective laser melting (SLM) produced Ti6A14V alloy is evaluated on tensile and fatigue crack growth (FCG) performances at RT and 400 degrees C. Conventionally manufactured Ti6A14V alloys are concerned for comparison. Different orientations are considered to investigate the anisotropy of tensile and FCG behavior. The results show that, the tensile properties at RT and 400 degrees C are highly dependent on the specimen orientation relative to build direction. The FCG resistance is related to specimen orientation in the near threshold region but no relationship with specimen orientation in the steady growth stage at RT. The FCG resistance is much less influenced by specimen orientation at 400 degrees C. The tensile strength at RT and 400 C of SLM alloy reaches even exceeds the strength level of conventionally manufactured alloys such as forging, bar and casting. The steady stage FCG resistance under stress ratio of 0.1 of SLM alloy is also comparable to conventionally manufactured alloys. The SLM alloy shows higher FCG resistance under stress ratio of 0.1 than 0.5, but the da/dN-AK curves of the two stress ratios are very close to each other. The steady stage FCG rate at RT is slower than 400 degrees C in the lower AK region and faster in the higher AK region. Copyright (C) 2017 The Authors. Published by Elsevier B.V.
引用
收藏
页码:124 / 132
页数:9
相关论文
共 50 条
  • [41] Temperature field calculation on cold crucible continuous melting and directional solidification of Ti6A14V alloy
    Chen Ruirun
    Ding Hongsheng
    Guo Jingjie
    Liang Fuzhen
    Zhang Ziqin
    Bi Weisheng
    Liu Lin
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 (10) : 1722 - 1727
  • [42] Fatigue limit prediction model and fatigue crack growth mechanism for selective laser melting Ti6Al4V samples with inherent defects
    Xu, Zhongwei
    Liu, An
    Wang, Xishu
    Liu, Bin
    Guo, Minghai
    INTERNATIONAL JOURNAL OF FATIGUE, 2021, 143
  • [43] Fatigue limit prediction model and fatigue crack growth mechanism for selective laser melting Ti6Al4V samples with inherent defects
    Xu, Zhongwei
    Liu, An
    Wang, Xishu
    Liu, Bin
    Guo, Minghai
    International Journal of Fatigue, 2021, 143
  • [44] On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance
    Lenders, S.
    Thoene, M.
    Riemer, A.
    Niendorf, T.
    Troester, T.
    Richard, H. A.
    Maier, H. J.
    INTERNATIONAL JOURNAL OF FATIGUE, 2013, 48 : 300 - 307
  • [45] Coatings on Ti6A14V as palliatives for fretting fatigue in cryogenic environment
    Caron, I.
    Gras, R.
    Ganne, T.
    De Monicault, J. M.
    TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1045 - 1051
  • [46] Fatigue of Ti6Al4V Structural Health Monitoring Systems Produced by Selective Laser Melting
    Strantza, Maria
    Vafadari, Reza
    de Baere, Dieter
    Vrancken, Bey
    van Paepegem, Wim
    Vandendael, Isabelle
    Terryn, Herman
    Guillaume, Patrick
    van Hemelrijck, Danny
    MATERIALS, 2016, 9 (02)
  • [47] Small fatigue crack growth behavior of Ti-6Al-4V produced via selective laser melting: In situ characterization of a 3D crack tip interactions with defects
    Waddell, Michael
    Walker, Kevin
    Bandyopadhyay, Ritwik
    Kapoor, Kartik
    Mallory, Alexandra
    Xiao, Xianghui
    Chuang, Andrew C.
    Liu, Qianchu
    Nam Phan
    Sangid, Michael D.
    INTERNATIONAL JOURNAL OF FATIGUE, 2020, 137
  • [48] Microstructure of Ti-6Al-4V produced by selective laser melting
    Simonelli, M.
    Tse, Y. Y.
    Tuck, C.
    ELECTRON MICROSCOPY AND ANALYSIS GROUP CONFERENCE 2011 (EMAG 2011), 2012, 371
  • [49] Influence of processing parameters on internal porosity and types of defects formed in Ti6A14V lattice structure fabricated by selective laser melting
    Salem, H.
    Carter, L. N.
    Attallah, M. M.
    Salem, H. G.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 767
  • [50] Fatigue strength of blunt V-notched specimens produced by selective laser melting of Ti-6Al-4V
    Razavi, N.
    Ferro, P.
    Berto, F.
    Torgersen, J.
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2018, 97 : 376 - 384