Effect of pre-ageing on natural secondary ageing and paint bake hardening in Al-Mg-Si alloys

被引:22
|
作者
Zi, Yang [1 ]
Liang Zeqin [2 ]
Leyvraz, David [2 ]
Banhart, John [1 ]
机构
[1] Helmholtz Ctr Berlin, Hahn Meitner Pl 1, D-14109 Berlin, Germany
[2] Novelis R&T Ctr, Rte Laminoirs 15, CH-3960 Sierre, Switzerland
关键词
Aluminium alloys; Al-Mg-Si; Age hardening; Pre-ageing; CU ALLOY; CO-CLUSTERS; EARLY-STAGE; PRECIPITATION; BEHAVIOR; KINETICS; PREPRECIPITATION; THERMODYNAMICS; NANOCLUSTERS; TEMPERATURE;
D O I
10.1016/j.mtla.2019.100413
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of pre-ageing (PA) time and temperature on subsequent natural secondary ageing (NSA) and paint bake (PB) hardening of an Al-Mg-Si alloy was systematically investigated, especially when both parameters change. A wide range of PA conditions was covered, including temperatures from 80 degrees C to 160 degrees C and times from several minutes to several days depending on the PA temperature. Hardness and electrical resistivity measurements, positron annihilation lifetime spectroscopy, and differential scanning calorimetry were used to characterise the alloy after various ageing stages. It is found that both the delay of NSA clustering and PB hardening are closely related to the PA conditions. PB hardness can be enhanced primarily by increasing PA temperature, whereas NSA stability (resistance to clustering) is improved by prolonging PA time or by lowering PA temperature. In particular, when PA hardness is constant, one can use PA temperature to trade PB hardness for NSA stability and vice versa. One can also tailor PA conditions to minimise hardness after a given NSA time while maximising PB response, which is a way to improve industrial practices.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] HARDENING OF AL-MG-SI ALLOYS AND EFFECT OF PARTICLE STRUCTURE
    Gulbrandsen-Dahl, Sverre
    Marioara, C. D.
    Pedersen, Ketill Olav
    Marthinsen, Knut
    [J]. THERMEC 2011, PTS 1-4, 2012, 706-709 : 283 - +
  • [42] Hardening of Al-Mg-Si alloys: Effect of trace elements and prolonged natural aging
    Werinos, M.
    Antrekowitsch, H.
    Ebner, T.
    Prillhofer, R.
    Uggowitzer, P. J.
    Pogatscher, S.
    [J]. MATERIALS & DESIGN, 2016, 107 : 257 - 268
  • [43] A combination of severe plastic deformation and ageing phenomena in Al-Mg-Si Alloys
    Vaseghi, Majid
    Kim, Hyoung Seop
    [J]. MATERIALS & DESIGN, 2012, 36 : 735 - 740
  • [44] A systematic comparison of static and dynamic ageing of two Al-Mg-Si alloys
    Cai, M
    Field, DP
    Lorimer, GW
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 373 (1-2): : 65 - 71
  • [45] Effect of Sn contents on natural aging and precipitation hardening in Al-Mg-Si alloys
    Weng, Yaoyao
    Xu, Yaqi
    Ding, Lipeng
    Jia, Zhihong
    Zhang, Zongqing
    Chen, Jiahao
    Xie, Maoxuan
    Liu, Qing
    [J]. MATERIALS CHARACTERIZATION, 2021, 179
  • [46] Effects of natural aging on bake hardening behavior of Al-Mg-Si alloys with multi-step aging process
    Kobe Steel, Ltd., 15 Kinugaoka, Moka-shi, Tochigi
    321-4367, Japan
    不详
    不详
    [J]. Keikinzoku J Jpn Inst Light Met, 3 (86-93):
  • [47] Effects of Natural Aging on Bake Hardening Behavior of Al-Mg-Si Alloys with Multi-Step Aging Process
    Takaki, Yasuo
    Masuda, Tetsuya
    Kobayashi, Equo
    Sato, Tatsuo
    [J]. MATERIALS TRANSACTIONS, 2014, 55 (08) : 1257 - 1265
  • [48] The combined effect of pre-aging and Mg/Si ratio on the natural aging and bake hardening in Al-Mg-Si-0.7Cu alloys
    Zang, Ruojin
    Wan, Bin
    Ding, Lipeng
    Ehlers, Flemming J. H.
    Jia, Zhihong
    Cao, Lingfei
    Li, Yanjun
    [J]. MATERIALS CHARACTERIZATION, 2024, 212
  • [49] Influence of interrupted quenching and pre-aging on the bake hardening of Al-Mg-Si Alloy
    Ding, Lipeng
    Weng, Yaoyao
    Wu, Sainan
    Sanders, Robert E.
    Jia, Zhihong
    Liu, Qing
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 651 : 991 - 998
  • [50] Effect of natural ageing and pre-straining on the hardening behaviour and microstructural response during artificial ageing of an Al-Mg-Si-Cu alloy
    Yin, Deyan
    Xiao, Qiao
    Chen, Yuqiang
    Liu, Huiqun
    Yi, Danqing
    Wang, Bin
    Pan, Suping
    [J]. MATERIALS & DESIGN, 2016, 95 : 329 - 339