Corrosion performance of iron aluminides in mixed-oxidant environments

被引:84
|
作者
Natesan, K [1 ]
机构
[1] Argonne Natl Lab, Div Energy Technol, Argonne, IL 60439 USA
关键词
corrosion; iron aluminides; mixed-oxidant; electrospark deposition; gasification; combustion;
D O I
10.1016/S0921-5093(98)00925-3
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Iron aluminide intermetallics are being developed for use as structural materials and/or as cladding for conventional engineering alloys. In addition to their strength advantages, these materials exhibit excellent resistance to corrosion in single- and multi-oxidant environments at elevated temperatures through the formation of slow-growing, adherent alumina scales. Even though these intermetallics develop protective oxide scales in single-oxidant environments, the simultaneous presence of several reactants in the environment (typical of practical systems) can lead to development of oxide scales that are non-protective and undergo breakaway corrosion or to non-oxide scales that are detrimental to the performance of underlying ahoy. This paper describes the corrosion performance of Fe-Al intermetallics in environments that contain sulfur, carbon, chlorine, and oxygen and that are typical of industrial applications and power generation systems. Emphasis is on mechanisms of scale development/breakdown, performance envelopes for long-term usage of these materials, approaches to modifying the surfaces of engineering alloys by cladding or coating them with intermetallics, and corrosion experience in practical environments. (C) 1998 Published by Elsevier Science S.A. All rights reserved.
引用
收藏
页码:126 / 134
页数:9
相关论文
共 50 条
  • [31] Inactivation of Cryptosporidium parvum oocysts and Clostridium perfringens spores by a mixed-oxidant disinfectant and by free chlorine (vol 63, pg 1600, 1997)
    Venczel, LV
    Arrowood, M
    Hurd, M
    Sobsey, MD
    APPLIED AND ENVIRONMENTAL MICROBIOLOGY, 1997, 63 (11) : 4625 - 4625
  • [32] BREAKAWAY CORROSION IN MIXED-GAS ENVIRONMENTS
    NATESAN, K
    BAXTER, DJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1983, 130 (08) : C336 - C336
  • [33] Research Progress on Sulfidation Corrosion Behavior of Iron-Aluminides Intermetallics at High Temperature
    Tan Ping
    Chen Jinmei
    Tang Huiping
    Li Yanjun
    Yang Baojun
    Wang Jian
    Li Yaning
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 : 817 - 821
  • [34] Toxicity of mixed-oxidant electrolyzed oxidizing water to in vitro and leaf surface populations of vegetable bacterial pathogens and control of bacterial diseases in the greenhouse
    Pernezny, K
    Raid, RN
    Havranek, N
    Sanchez, J
    CROP PROTECTION, 2005, 24 (08) : 748 - 755
  • [35] The corrosion resistance of Fe3Al-based iron aluminides in molten glasses
    Hotar, A.
    Kratochvil, P.
    Hotar, V.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2009, 47 (04): : 247 - 252
  • [36] REACTION OF IRON-CHROMIUM ALLOYS IN MIXED OXIDANT GASES
    COLWELL, JA
    COREY, RG
    RAPP, RA
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1978, 125 (03) : C117 - C117
  • [37] CORROSION OF IRON IN GASEOUS ENVIRONMENTS AND IN GAS-SATURATED AQUEOUS ENVIRONMENTS
    RAMANARAYANAN, TA
    SMITH, SN
    CORROSION, 1990, 46 (01) : 66 - 74
  • [38] Hot corrosion of carbon-alloyed Fe3Al-based iron aluminides
    Das, D
    Balasubramaniam, R
    Mungole, MN
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 338 (1-2): : 24 - 32
  • [39] Analysis of Corrosion Growth of Ductile Iron in Different Environments
    Oke, P. K.
    Ukoba, O. K.
    ADVANCES IN MATERIALS AND SYSTEMS TECHNOLOGIES IV, 2013, 824 : 327 - +
  • [40] CORROSION FATIGUE BEHAVIOR OF IRON IN DIFFERENT AQUEOUS ENVIRONMENTS
    CERISOLA, G
    BUSCA, G
    DEANNA, PL
    MATERIALS CHEMISTRY AND PHYSICS, 1983, 9 (04) : 387 - 403