Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting

被引:78
|
作者
Xiang, Nan [1 ]
Xin, Xian-Zhen [1 ]
Chen, Jie [1 ]
Wei, Bin [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Med, Peoples Hosp 9,Shanghai Key Lab Stomat, Stomatol Special Consultat Clin,Dept Prosthodont, Shanghai 200011, Peoples R China
关键词
Co-Cr; Selective laser melting (Slm); Metal-ceramic; Bonding; Sem; Bending test; PORCELAIN ADHERENCE; FRACTURE; GOLD;
D O I
10.1016/j.jdent.2012.02.006
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: This study was to evaluated the metal-ceramic bond strength of a Co-Cr dental alloy prepared using a selective laser melting (SLM) technique. Methods: Two groups comprised of twenty Co-Cr metal bars each were prepared using either a SLM or traditional lost-wax casting method. Ten bars from each group were moulded into standard ISO 9693:1999 dimensions of 25 mm x 3 mm x 0.5 mm with 1.1 mm of porcelain fused onto an 8 mm x 3 mm rectangular area in the centre of each bar. Metal-ceramic bonding was assessed using a three-point bending test. Fracture mode analysis and area fraction of adherence porcelain (AFAP) were determined by measuring Si content of specimens by SEM/EDS. Results: Student's t-test within the groups demonstrated no significant difference for the mean bond strength between the SLM and traditional cast sample groups. While SEM/EDS analysis indicated a mixed fracture mode on the debonding interface of both the SLM and the cast groups, the SLM group showed significantly more porcelain adherence than the control group (p < 0.05). Conclusions: The SLM metal-ceramic system exhibited a bonding strength that exceeds the requirement of ISO 9691: 1999(E) and it even showed a better behaviour in porcelain adherence test comparable to traditional cast methods. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:453 / 457
页数:5
相关论文
共 50 条
  • [31] Microstructure and Mechanical Properties of Co-Cr Alloy Fabricated by Selective Laser Melting Technology for Removable Partial Denture Frameworks
    Konstantinos Dimitriadis
    Georgios Foteinidis
    Maria Kosarli
    Dimitrios Moschovas
    Alkiviadis S. Paipetis
    Simeon Agathopoulos
    Journal of Materials Engineering and Performance, 2023, 32 : 8637 - 8646
  • [32] Microstructure and Mechanical Properties of Co-Cr Alloy Fabricated by Selective Laser Melting Technology for Removable Partial Denture Frameworks
    Dimitriadis, Konstantinos
    Foteinidis, Georgios
    Kosarli, Maria
    Moschovas, Dimitrios
    Paipetis, Alkiviadis S.
    Agathopoulos, Simeon
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (19) : 8637 - 8646
  • [33] Effect of Selective Laser Melting Process Parameters on Microstructure and Properties of Co-Cr Alloy
    Wang, Jian-Hong
    Ren, Jie
    Liu, Wei
    Wu, Xiao-Yu
    Gao, Ming-Xiang
    Bai, Pei-Kang
    MATERIALS, 2018, 11 (09)
  • [34] Effects of repeated firing on the marginal accuracy of Co-Cr copings fabricated by selective laser melting
    Zeng, Li
    Zhang, Yong
    Liu, Zheng
    Wei, Bin
    JOURNAL OF PROSTHETIC DENTISTRY, 2015, 113 (02): : 135 - 139
  • [35] Effect of Subsequent Heat Treatment on Nano-Tribological Behavior of the Co-Cr Medical Alloy Fabricated by Selective Laser Melting
    Xiao, Jichang
    Zhu, Jinxuan
    Wang, Jiaxu
    He, Xiaofei
    Wei, Wei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 9864 - 9877
  • [36] Effect of Subsequent Heat Treatment on Nano-Tribological Behavior of the Co-Cr Medical Alloy Fabricated by Selective Laser Melting
    Jichang Xiao
    Jinxuan Zhu
    Jiaxu Wang
    Xiaofei He
    Wei Wei
    Journal of Materials Engineering and Performance, 2022, 31 : 9864 - 9877
  • [37] Effect of Laser Power and Scanning Speed on Microstructure and Properties of Co-Cr Alloy by Selective Laser Melting
    Deng Y.-H.
    Li Z.-H.
    Yao B.-B.
    Teng B.-R.
    Li H.
    Surface Technology, 2023, 52 (01): : 325 - 335
  • [38] Metal-ceramic bond strength - Response
    Persson, M
    Bergman, M
    ACTA ODONTOLOGICA SCANDINAVICA, 1996, 54 (06) : 399 - 400
  • [39] Metal-ceramic bond strength - Comment
    Lenz, J
    ACTA ODONTOLOGICA SCANDINAVICA, 1996, 54 (06) : 398 - 399
  • [40] Evaluation of metal-ceramic bond characteristics of three dental Co-Cr alloys prepared with different fabrication techniques
    Wang, Hongmei
    Feng, Qing
    Li, Ning
    Xu, Sheng
    JOURNAL OF PROSTHETIC DENTISTRY, 2016, 116 (06): : 916 - 923