Low temperature degradation of single layers of multilayered zirconia in comparison to conventional unshaded zirconia: Phase transformation and flexural strength

被引:46
|
作者
Wille, Sebastian [1 ]
Zumstrull, Paul [1 ]
Kaidas, Victor [2 ]
Jessen, Lea Katharina [2 ]
Kern, Matthias [1 ]
机构
[1] Christian Albrechts Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, Kiel, Germany
[2] Christian Albrechts Univ Kiel, Fac Engn, Inst Mat Sci, Funct Nanomat, Kiel, Germany
关键词
zirconia; Biaxial flexural strength; Phase transformation; Shading particles; CERAMIC FEMORAL-HEAD; Y-TZP ZIRCONIA; MONOLITHIC ZIRCONIA; DENTAL ZIRCONIA; AIR-ABRASION; SURFACE CHARACTERISTICS; MECHANICAL-PROPERTIES; TRANSLUCENT ZIRCONIA; CATASTROPHIC FAILURE; FRACTURE STRENGTH;
D O I
10.1016/j.jmbbm.2017.09.010
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: The aim of this study was to evaluate the transformation of yttrium stabilized tetragonal zirconia (YTZP) to monoclinic phase and its change in flexural strength of the various layers of multilayered zirconia (enamel layer, transition layer 1, transition layer 2 and body layer) in comparison to two conventional zirconia ceramics. Additionally, the ball-on-three-balls test was compared with a conventional biaxial flexural strength test. Methods: The crystallographic structure of the four layers of Katana Zirconia ML (Kuraray), e.max ZirCAD (Ivoclar Vivadent) and Lava Plus (3M ESPE) was investigated by x-ray-diffraction before and after hydrothermal aging in an autoclave for 5, 10, 15 and 20 h. The biaxial flexural strength was examined with a piston-on-three ball test and a ball-on-three-balls test. Results: There was a significant difference of the ratio of transformation with respect to the tested materials, also between the four different layers of multilayered zirconia. After 20 h of hydrothermal aging the mean ratio of monoclinic phase ranged from 9.9 vol% (LAVA Plus) to 44.2 vol% (Katana Zirconia ML, enamel layer). However, hydrothermal aging had no significant influence on the flexural strength of any material. Furthermore, the flexural strength measured by the ball-on-three-balls test was higher than that measured by the piston-on-three ball test. Conclusion: A ratio of 40% monoclinic phase at the surface did not significantly influence the biaxial flexural strength. Both test methods provide reliable results. However, as the ball-on-three balls test is less dependent on surface roughness, it might be preferred for investigations adapted to clinical reality.
引用
收藏
页码:171 / 175
页数:5
相关论文
共 45 条
  • [41] Influence of crystalline phase transformation induced by airborne-particle abrasion and low-temperature degradation on mechanical properties of dental zirconia ceramics stabilized with over 5 mol% yttria
    Nakamura, Keisuke
    Tarkeshi, Aria
    Niklasson, Alexander
    Shishido, Shunichi
    Svanborg, Per
    Barkarmo, Sargon
    Ortengren, Ulf
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 125
  • [42] One-step synthesis and low-temperature rapid sintering of alumina-zirconia ceramics by flash sintering combined with phase transformation
    Wang, Jianglin
    Li, Jie
    Li, Yu
    Li, Linlin
    Su, Xinghua
    Hu, Yongbiao
    Xu, Xiqing
    MATERIALS CHARACTERIZATION, 2024, 209
  • [43] Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia (vol 118, pg 658, 2017)
    Mohammadi-Bassir, M.
    Babasafari, M.
    Rezvani, M. B.
    Jamshidian, Mahdieh
    JOURNAL OF PROSTHETIC DENTISTRY, 2019, 121 (02): : 365 - 365
  • [44] Comparative effects of tungsten, diamond burs and laser for residual adhesive removal after orthodontic debonding on flexural strength, surface roughness and phase transformation of high-translucent zirconia: An in vitro study
    Hemmati, Yasamin Babaee
    Asil, Hamid Neshandar
    Falahchai, Mehran
    Safari, Nika
    INTERNATIONAL ORTHODONTICS, 2022, 20 (03)
  • [45] Low temperature zirconia thin film synthesis by a chemical vapour deposition process involving ZrCl4 and O-2-H-2-Ar microwave post-discharges. Comparison with a conventional CVD hydrolysis process
    Gavillet, J
    Belmonte, T
    Hertz, D
    Michel, H
    THIN SOLID FILMS, 1997, 301 (1-2) : 35 - 44