Two-body abrasive wear of electroless nickel composite coatings

被引:7
|
作者
Subramanian, C. [1 ]
Pallotta, E. [1 ]
机构
[1] Univ S Australia, Ian Wark Res Inst, The Levels, SA 5095, Australia
关键词
abrasion; electroless nickel; composite coatings; wear; scratch testing; two-body abrasion;
D O I
10.1007/BF00160971
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The two-body abrasive wear of electroless nickel (EN), EN-silicon carbide, and EN-alumina composite coatings have been investigated using a scratch test with a diamond indenter. The coatings were heat treated at temperatures of 100-500 degrees C The hardness of the coatings increased with heat treatment temperature from 500 HV100 for the as-deposited condition to 1008 HV100 when fully hardened. Scratch testing showed that the as-deposited coating had scratch tracks with a high degree of plasticity, signs of microploughing and tensile cracking and was characterised as a ductile failure. On the other hand, the heat-treated coatings showed chipping and cracking on the edge of the scratch tracks, failing in a brittle manner. The heat-treated EN-silicon carbide coatings, however, exhibited no cracking nor chipping, believed to be due to its higher fracture toughness than the other heat-treated coatings, attributable to its lower phosphorus content. The volume of material removed from the silicon carbide scratch track was 1/3 of the volume removed from the steel substrate at a 20 N load, and showed the best wear/scratch resistance of any of the coatings tested.
引用
下载
收藏
页码:133 / 150
页数:18
相关论文
共 50 条
  • [21] STRUCTURE AND WEAR OF ELECTROLESS NICKEL COATINGS
    GAWNE, DT
    MA, U
    MATERIALS SCIENCE AND TECHNOLOGY, 1987, 3 (03) : 228 - 239
  • [22] Electroless nickel composite coatings
    Ploof, Lloyd
    ADVANCED MATERIALS & PROCESSES, 2008, 166 (05): : 36 - 38
  • [23] Two-body abrasive wear of nano- and microcrystalline TiC-Ni-based thermal spray coatings
    Qi, X
    Eigen, N
    Aust, E
    Gärtner, F
    Klassen, T
    Bormann, R
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (16-17): : 5037 - 5047
  • [24] Microstructure, mechanical properties and two-body abrasive wear behaviour of hypereutectic Al-Si-SiC composite
    Singh, Raj Kumar
    Telang, Amit
    Das, Satyabrata
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2020, 30 (01) : 65 - 75
  • [25] Two-body Abrasive Wear Behavior of Nylon 6 and Glass Fiber Reinforced (GFR) Nylon 6 Composite
    Kumar, Sudhir
    Panneerselvam, K.
    1ST GLOBAL COLLOQUIUM ON RECENT ADVANCEMENTS AND EFFECTUAL RESEARCHES IN ENGINEERING, SCIENCE AND TECHNOLOGY - RAEREST 2016, 2016, 25 : 1129 - 1136
  • [26] On the mechanism of two-body abrasive wear in turning "the spin-split theory"
    Svenningsson, Inge
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 92 (9-12): : 3337 - 3348
  • [27] Effect of particle characteristics on the two-body abrasive wear behaviour of a pearlitic steel
    Narayanaswamy, Balaji
    Hodgson, Peter
    Beladi, Hossein
    WEAR, 2016, 354-355 : 41 - 52
  • [28] On the mechanism of two-body abrasive wear in turning “the spin-split theory”
    Inge Svenningsson
    The International Journal of Advanced Manufacturing Technology, 2017, 92 : 3337 - 3348
  • [29] ABRASION WEAR OF ELECTROLESS NICKEL COMPOSITE COATINGS MODIFIED WITH BORON NITRIDE NANOPARTICLES
    Kandeva, M.
    Kamburov, V.
    Zadorozhnaya, E.
    Kalitchin, Zh.
    JOURNAL OF ENVIRONMENTAL PROTECTION AND ECOLOGY, 2018, 19 (04): : 1690 - 1703
  • [30] Wear behaviour of silicon carbide/electroless nickel composite coatings at high temperature
    Staia, MH
    Conzoño, A
    Cruz, MR
    Roman, A
    Lesage, J
    Chicot, D
    Mesmacque, G
    SURFACE ENGINEERING, 2002, 18 (04) : 265 - 269