Erosion in Gas-Turbine Grade Ceramic Matrix Composites

被引:22
|
作者
Kedir, N. [1 ,2 ]
Gong, C. [1 ]
Sanchez, L. [1 ]
Presby, M. J. [1 ,3 ]
Kane, S. [1 ]
Faucett, D. C. [1 ]
Choi, S. R. [1 ]
机构
[1] Naval Air Syst Command, Patuxent River, MD 20670 USA
[2] Purdue Univ, Sch Mat Engn, W Lafayette, IN 47907 USA
[3] Univ Akron, Dept Mech Engn, Akron, OH 44325 USA
关键词
erosion; erosion damage; ceramic matrix composite (CMC); gas-turbine grade CMCs; erosion mechanism; FOREIGN OBJECT DAMAGE; PROJECTILES; STRENGTH;
D O I
10.1115/1.4040848
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Erosion behavior of a large number of gas-turbine grade ceramic matrix composites (CMCs) was assessed using fine to medium grain garnet erodents at velocities of 200 and 300 m/s at ambient temperature. The CMCs used in the current work were comprised of nine different SiC/SiCs, one SiC/C, one C/SiC, one SiC/MAS, and one oxide/oxide. Erosion damage was quantified with respect to erosion rate and the damage morphology was assessed via scanning electron microscopy (SEM) and optical microscopy in conjunction with three-dimensional (3D) image mapping. The CMCs response to erosion appeared to be very complicated due to their architectural complexity, multiple material constituents, and presence of pores. Effects of architecture, material constituents, density, matrix hardness, and elastic modulus of the CMCs were taken into account and correlated to overall erosion behavior. The erosion of monolithic ceramics such as silicon carbide and silicon nitrides was also examined to gain a better understanding of the governing damage mechanisms for the CMC material systems used in this work.
引用
收藏
页数:9
相关论文
共 50 条
  • [21] Durability of Oxide/Oxide Ceramic Matrix Composites in Gas Turbine Combustors
    van Roode, Mark
    Bhattacharya, Arun K.
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 2013, 135 (05):
  • [22] CERAMIC AIR SEAL DEVELOPMENT FOR GAS-TURBINE ENGINES
    NEWHART, JE
    GLATZ, JW
    AMERICAN CERAMIC SOCIETY BULLETIN, 1977, 56 (03): : 313 - 313
  • [23] CERAMIC BEARINGS FOR USE IN GAS-TURBINE ENGINES - DISCUSSION
    CHIU, YP
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1989, 111 (01): : 154 - 155
  • [24] STATUS OF THE AUTOMOTIVE CERAMIC GAS-TURBINE DEVELOPMENT PROGRAM
    ITOH, T
    KIMURA, H
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1993, 115 (01): : 42 - 50
  • [25] FABRICATION AND ENGINE TESTING OF A GAS-TURBINE CERAMIC FLAMEHOLDER
    NELSON, WA
    AMERICAN CERAMIC SOCIETY BULLETIN, 1980, 59 (08): : 828 - 828
  • [26] AUTOMOTIVE GAS-TURBINE HAS NEW CERAMIC COMPONENTS
    YAMAGUCHI, J
    AUTOMOTIVE ENGINEERING, 1984, 92 (01): : 95 - 96
  • [27] THERMAL SHOCK TESTING OF CERAMIC GAS-TURBINE MATERIALS
    KATZ, RN
    SEATON, CC
    FISHER, EA
    AMERICAN CERAMIC SOCIETY BULLETIN, 1973, 52 (08): : 645 - 645
  • [28] IMPROVING GAS-TURBINE PERFORMANCE WITH METAL AND CERAMIC COATINGS
    MOCK, JA
    MATERIALS ENGINEERING, 1976, 84 (05): : 76 - 77
  • [29] CERAMIC BEARINGS FOR USE IN GAS-TURBINE ENGINES - CLOSURE
    SEROVI, GK
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1989, 111 (01): : 156 - 157
  • [30] HIGH-TEMPERATURE EROSION RESISTANCE OF COATINGS FOR GAS-TURBINE
    TABAKOFF, W
    HAMED, A
    METWALLY, M
    PASIN, M
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1992, 114 (02): : 242 - 249