Oxidation behavior of ferritic-martensitic and ODS steels in supercritical water

被引:148
|
作者
Bischoff, Jeremy [1 ]
Motta, Arthur T. [1 ]
机构
[1] Penn State Univ, Dept Mech & Nucl Engn, University Pk, PA 16802 USA
基金
美国国家科学基金会;
关键词
HIGH-TEMPERATURE OXIDATION; BI EUTECTIC ALLOY; FE-9CR-1MO STEEL; CORROSION BEHAVIOR; AQUEOUS CORROSION; ZIRCONIUM ALLOY; OXIDE; MECHANISM; SURFACE; IRON;
D O I
10.1016/j.jnucmat.2012.03.009
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ferritic-martensitic and ODS alloys are primary candidates for application as cladding and structural materials in the Generation IV Supercritical Water Reactor. One of the main in-service degradation mechanisms for these alloys is uniform corrosion. This article analyzes the oxide microstructure formed on these alloys to better understand their oxidation behavior. Corrosion tests were performed in both steam and supercritical water (SCW) at 500 and 600 degrees C. The oxide microstructure was analyzed using microbeam synchrotron radiation diffraction and fluorescence associated with electron microscopy. The oxide forms a three-layer structure with an outer layer containing only Fe3O4, an inner layer containing a non-uniform (Fe,Cr)(3)O-4 spinel structure, and a diffusion layer containing a mixture of metal grains and chromium-rich precipitates. A marker experiment located the original water-metal interface as the outer-inner layer interface implying a mechanism where iron migrates outwards to form the outer layer and oxygen diffuses inwards to form the inner layer. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:261 / 276
页数:16
相关论文
共 50 条
  • [31] Fatigue behaviour of ODS ferritic-martensitic Eurofer steel
    Kubena, I.
    Kruml, T.
    Spaetig, P.
    Baluc, N.
    Oksiuta, Z.
    Petrenec, M.
    Obrtlik, K.
    Polak, J.
    FATIGUE 2010, 2010, 2 (01): : 717 - 724
  • [32] Oxidation behavior of an 11Cr ferritic-martensitic steel after Ar-ions irradiation in supercritical water
    Huang, Xi
    Shen, Yinzhong
    JOURNAL OF NUCLEAR MATERIALS, 2015, 461 : 1 - 9
  • [33] Influence of Ar-ions irradiation on the oxidation behavior of ferritic-martensitic steel P92 in supercritical water
    Huang, Xi
    Shen, Yinzhong
    Zhu, Jun
    JOURNAL OF NUCLEAR MATERIALS, 2015, 457 : 18 - 28
  • [34] TEM characterization of structure and composition of nanosized ODS particles in reduced activation ferritic-martensitic steels
    Klimiankou, M
    Lindau, R
    Möslang, A
    JOURNAL OF NUCLEAR MATERIALS, 2004, 329 : 347 - 351
  • [35] A comparative assessment of the fracture toughness behavior of ferritic-martensitic steels and nanostructured ferritic alloys
    Byun, Thak Sang
    Hoelzer, David T.
    Kim, Jeoung Han
    Maloy, Stuart A.
    JOURNAL OF NUCLEAR MATERIALS, 2017, 484 : 157 - 167
  • [36] Irradiation behavior of ferritic-martensitic 9-12%Cr steels
    Horsten, MG
    van Osch, EV
    Gelles, DS
    Hamilton, ML
    EFFECTS OF RADIATION ON MATERIALS: 19TH INTERNATIONAL SYMPOSIUM, 2000, 1366 : 579 - 593
  • [37] Corrosion of ferritic-martensitic steel HT9 in supercritical water
    Ren, X.
    Sridharan, K.
    Allen, T. R.
    JOURNAL OF NUCLEAR MATERIALS, 2006, 358 (2-3) : 227 - 234
  • [38] Ferritic-martensitic steels for fission and fusion applications
    Cabet, C.
    Dalle, E.
    Gaganidze, E.
    Henry, J.
    Tanigawa, H.
    JOURNAL OF NUCLEAR MATERIALS, 2019, 523 : 510 - 537
  • [39] 2-PHASE FERRITIC-MARTENSITIC STEELS
    GOLOVANENKO, SA
    FONSHTEIN, NM
    METAL SCIENCE AND HEAT TREATMENT, 1984, 26 (11-1) : 811 - 816
  • [40] The Features of Martensitic Transformation in 12% Chromium Ferritic-Martensitic Steels
    Bazaleeva, Kseniya
    Golubnichiy, Alexander
    Chernov, Anton
    Ni, Andrey
    Mendagaliyev, Ruslan
    MATERIALS, 2021, 14 (16)