Development of structural ceramics having large crack-healing ability and fracture toughness

被引:0
|
作者
Takahashi, K [1 ]
Yokouchi, M [1 ]
Lee, SK [1 ]
Ando, K [1 ]
机构
[1] Yokohama Natl Univ, Yokohama, Kanagawa 2408501, Japan
来源
SMART MATERIALS III | 2005年 / 5648卷
关键词
crack healing; alumina; SiC whiskers; fracture toughness;
D O I
10.1117/12.580719
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al2O3 reinforced by SiC whiskers (Al2O3/SiC-W) was hot pressed to investigate the crack-healing behavior. Semi-elliptical surface cracks of 50 to 450 mu m in surface length were introduced using a Vickers indenter. The specimens containing pre-cracks were crack-healed at temperatures between 1000 degrees C and 1300 degrees C for 1h in air, and their strengths were measured by three-point bending tests at room temperature and elevated temperatures between 400 degrees C and 1300 degrees C. The results show that Al2O3/SiC-W possesses considerable crack-healing ability. The surface cracks with length of 2c = 100 mu m. could be healed by crack-healing at 1200 degrees C or 1300 degrees C. for 1h in air. The maximum crack size that can be healed for Al2O3/SiC-W is 2c = 200 mu m. Fracture toughness of the material was also determined. As expected, the SiC whiskers made their Al2O3 tougher.
引用
收藏
页码:276 / 283
页数:8
相关论文
共 50 条
  • [21] The crack-healing and strength recovery mechanisms for the new developed Ti(C,N)-TiSi2-WC composite ceramic tool materials with crack-healing ability
    Cui, Xinyao
    Huang, Chuanzhen
    Shi, Zhenyu
    Liu, Hanlian
    Li, Shijie
    Han, Youlong
    Ji, Lianggang
    Wang, Zhen
    Xu, Longhua
    Huang, Shuiquan
    CERAMICS INTERNATIONAL, 2023, 49 (22) : 35382 - 35391
  • [22] Preparation and characterization of a silicon oxycarbide coating with crack-healing capability for silicon carbide ceramics
    Kang, Kyunghoon
    Yun, Jondo
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2011, 12 (05): : 583 - 587
  • [23] Accurate measurement of fracture toughness in structural ceramics
    Wang, Anzhe
    Hu, Ping
    Zhang, Xinghong
    Han, Wenbo
    Chen, Guiqing
    Han, Jiecai
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (13) : 4207 - 4212
  • [24] Effect of difference in crack-healing ability on fatigue behavior of alumina/silicon carbide composites
    Sugiyama, Ryo
    Yamane, Kazuya
    Nakao, Wataru
    Takahashi, Koji
    Ando, Kotoji
    JOURNAL OF INTELLIGENT MATERIAL SYSTEMS AND STRUCTURES, 2008, 19 (03) : 411 - 415
  • [25] Structural reorganization and crack-healing properties of hydrogels based on dynamic diselenide linkages
    Xu, Hao
    Suzuki, Nao
    Takahashi, Akira
    Ohishi, Tomoyuki
    Goseki, Raita
    Xie, Xu-Ming
    Otsuka, Hideyuki
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2020, 21 (01) : 450 - 460
  • [26] Fracture toughness of ceramics by the surface crack in flexure (SCF) method
    Quinn, GD
    Gettings, RJ
    Kubler, JJ
    FRACTURE MECHANICS OF CERAMICS, VOL 11: R-CURVE BEHAVIOR, TOUGHNESS DETERMINATION, AND THERMAL SHOCK, 1996, 11 : 203 - 218
  • [27] Refinements to the surface crack in flexure method for fracture toughness of ceramics
    Quinn, GD
    EURO CERAMICS VII, PT 1-3, 2002, 206-2 : 633 - 636
  • [28] Development of Yttrium Titanate/Nickel Nanocomposites with Self Crack-Healing Ability and Potential Application as Thermal Barrier Coating Material
    Son Thanh Nguyen
    Nakayama, Tadachika
    Takeda, Masatoshi
    Nguyen Ngoc Hieu
    Takahashi, Tsuyoshi
    MATERIALS TRANSACTIONS, 2020, 61 (08) : 1510 - 1516
  • [29] NEW CERAMICS SURFACE REINFORCING TREATMENT USING A COMBINATION OF CRACK-HEALING AND ELECTRON BEAM IRRADIATION
    Nakao, Wataru
    Chiba, Youhei
    Ando, Kotoji
    Iwata, Keisuke
    Nishi, Yoshitake
    CORROSION, WEAR, FATIGUE, AND RELIABILITY OF CERAMICS, 2009, 29 (03): : 75 - +
  • [30] [Crack-healing plus proof test]: A new methodology to guarantee the structual integrity of ceramics component
    Ando, K
    Shirai, Y
    Nakatani, M
    Kobayashi, Y
    Sato, S
    EURO CERAMICS VII, PT 1-3, 2002, 206-2 : 815 - 818