Paint-bake response of AZ80 and AZ31 Mg alloys

被引:0
|
作者
Sha Ming-hong [1 ]
Shi Guo-dong [1 ]
Wang Yu [1 ]
Qiao Jun [1 ]
机构
[1] Univ Sci & Technol Liaoning, Sch Mat Sci & Engn, Anshan 114051, Peoples R China
基金
中国国家自然科学基金;
关键词
AZ80 Mg alloy; AZ31 Mg alloy; tensile strength; precipitation; age hardening; MECHANICAL-PROPERTIES; ALUMINUM-ALLOYS; MAGNESIUM ALLOY; PRECIPITATION; BEHAVIOR; CU;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Aging behaviors of extruded and rolled AZ80 and AZ31 Mg alloys were investigated under conditions similar to the paint-bake cycle currently used in automotive industry. Artificial aging at 170 degrees C from 0.5 to 12 h was conducted on solution-treated specimens to study the effects of aging on mechanical properties. SEM observations and EDS data show that beta-phase of Al12Mg17 precipitates continuously or discontinuously from alpha-Mg matrix and distributes along grain boundaries of the AZ80 alloy during artificial aging. Data of tensile tests and Vickers hardness tests show that an optimum mechanical property is achieved after baking at 170 degrees C for 6-8 h when Vickers hardness, tensile strength, and elongation are increased by 6.35%, 15.30%, and 7.88%, respectively, while the AZ31 alloy does not exhibit significant hardening behavior over the aging period.
引用
收藏
页码:S571 / S575
页数:5
相关论文
共 50 条
  • [31] Deformation and fracture behavior of hot extruded Mg alloys AZ31
    Lu, Liwei
    Liu, Tianmo
    Chen, Yong
    Wang, Zhongchang
    MATERIALS CHARACTERIZATION, 2012, 67 : 93 - 100
  • [32] A comparative corrosion behavior of Mg, AZ31 and AZ91 alloys in 3.5% NaCl solution
    Singh, I. B.
    Singh, M.
    Das, S.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2015, 3 (02) : 142 - 148
  • [33] Enhanced strength and ductility of AZ80 Mg alloys by spray forming and ECAP
    Tang, Lingling
    Zhao, Yonghao
    Islamgaliev, R. K.
    Tsao, Chi Y. A.
    Valiev, R. Z.
    Lavernia, E. J.
    Zhu, Y. T.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 670 : 280 - 291
  • [34] ULTRAFINE GRAIN EVOLUTION IN Mg ALLOYS, AZ31, AZ61, AZ91 BY MULTI DIRECTIONAL FORGING
    Miura, H.
    Yang, X.
    Sakai, T.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2013, 33 (01) : 92 - 96
  • [35] Forging characteristics of AZ31 Mg alloy
    Chino, Y
    Mabuchi, M
    Shimojima, K
    Yamada, Y
    Wen, C
    Miwa, K
    Nakamura, M
    Asahina, T
    Higashi, K
    Aizawa, T
    MATERIALS TRANSACTIONS, 2001, 42 (03) : 414 - 417
  • [36] Modified AZ80 magnesium alloys for biomedical applications
    Erinc, M.
    Zhang, X.
    Sillekens, W. H.
    MAGNESIUM TECHNOLOGY 2010, 2010, : 641 - +
  • [37] Corrosion behavior of hydroxyapatite coated AZ31 and AZ91 Mg alloys by electrostatic spray coating
    Baslayici, Serkan
    Bugdayci, Mehmet
    Benzesik, Kagan
    Yucel, Onuralp
    Acma, Mahmut Ercan
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2022, 113 (02) : 93 - 100
  • [38] Microstructure and corrosion properties of lanthanum-added AZ31 Mg alloys
    İsmail Hakkı Kara
    Hayrettin Ahlatçı
    Yunus Türen
    Yavuz Sun
    Arabian Journal of Geosciences, 2018, 11
  • [39] Cavity growth rate in superplastic 5083 Al and AZ31 Mg alloys
    Chino, Y
    Iwasaki, H
    Mabuchi, M
    JOURNAL OF MATERIALS RESEARCH, 2004, 19 (11) : 3382 - 3388
  • [40] Advances in microarc oxidation coated AZ31 Mg alloys for biomedical applications
    Zhang, Lei
    Zhang, Junqing
    Chen, Cheng-fu
    Gu, Yanhong
    CORROSION SCIENCE, 2015, 91 : 7 - 28