Performance evaluation of thermally reduced ex situ wheat husk biocarbon-assisted dissimilar AA7075 T651-magnesium AZ31B friction stir welded joints

被引:1
|
作者
Babu, T. V. B. [1 ]
Selvam, M. Amala Justus [2 ]
Devanathan, C. [3 ]
机构
[1] Vel Tech Rangarajan Dr, Dept Mech Engn, Sagunthala R&D Inst Sci & Technol, Chennai, Tamil Nadu, India
[2] Vel Tech Rangarajan Dr, Dept Automobile Engn, Sagunthala R&D Inst Sci & Technol, Chennai, Tamil Nadu, India
[3] Rajalakshmi Engn Coll, Dept Mech Engn, Chennai, Tamil Nadu, India
关键词
FSW; Biocarbon; Solid lubricant; Mechanical properties; Impact; Microstructure; MAGNESIUM; ALUMINUM; FSW;
D O I
10.1007/s13399-022-03409-w
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The emerging industrial need requires effective energy efficient materials and processing technologies that can be made engineering better. In this present study, a new attempt has been made to improve the effortless joining process of AA7075 T651-AZ31B base materials by using non-consumable rotating tool with novel biolubricant (biocarbon). The biocarbon was thermally reduced (TRB) from wheat straw via low temperature pyrolysis process at 450 degrees C. The fine biocarbon particles of sizes of about 1-3 mu m are then surface modified to prevent the clustering effect using a silane chemical. The sound weld joints were prepared with the help of vertical machining centre as lap joint format. According to the result, the thermal reduction on the biocarbon particle makes the particle lesser impurities. The ordered structure biocarbon effectively offered the lubrication effect and improved the microstructure. The weld made with 1 vol% of biocarbon scored the highest tensile strength of 348 MPa, % of elongation of 28, microhardness of 106 Hv, and Charpy impact toughness of 23.4 J respectively. Similarly, the wear properties show improved wear resistance for large biocarbon particle dispersed weld. The microstructure of welded portion shows highly refined and typically smaller grains. The heat-affected zone (HAZ) and thermo-mechanically treated zone (TMTZ) are typically occupied lesser orbit from the weld pool. The weld bead microstructure reveals improved joining geometry for biocarbon-assisted welds even after more trials. These high strength and joint efficient dissimilar welded joints could be used in automotives, airlines, and shipping where joining of high strength alloys frequently done.
引用
收藏
页码:14075 / 14081
页数:7
相关论文
共 22 条
  • [21] Mathematical modeling, optimization and prediction of friction stir spot welding parameters for dissimilar joining AA2024-T6 aluminium and AZ31B magnesium alloy in lap weld configuration
    Rajendran, C.
    Sonar, Tushar
    Ivanov, Mikhail
    Xu, Jinyang
    Manoram, R. B.
    Muthukumaran, D. Selva
    Amarnath, V.
    INTERNATIONAL JOURNAL OF INTERACTIVE DESIGN AND MANUFACTURING - IJIDEM, 2025, 19 (01): : 275 - 289
  • [22] Effect of TiO2 nanoparticles addition on microstructure and mechanical properties of dissimilar friction stir welded AA6063-T4 aluminum alloy and AZ31B-O magnesium alloy
    Asl, Nima Sharifi
    Mirsalehi, Seyyed Ehsan
    Dehghani, Kamran
    JOURNAL OF MANUFACTURING PROCESSES, 2019, 38 : 338 - 354