Mechanisms of high-temperature fatigue failure in alloy 800H

被引:21
|
作者
Rao, KBS
Schuster, H
Halford, GR
机构
[1] INST MAT ENERGY,SYST RES CTR,D-52425 JULICH,GERMANY
[2] NASA,LEWIS RES CTR,STRUCT DIV,CLEVELAND,OH 44135
关键词
D O I
10.1007/BF02649752
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The damage mechanisms influencing the axial strain-controlled low-cycle fatigue (LCF) behavior of alloy 800H at 850 degrees C have been evaluated under conditions of equal tension/compression ramp rates (fast-fast (F-F): 4 x 10(-3) s(-1) and slow-slow (S-S): 4 x 10(-5) s(-1)) and asymmetrical ramp rates (fast-slow (F-S): 4 x 10(-3) s(-1) / 4 x 10(-5) s(-1) and slow-fast (S-F): 4 x 10(-5) / 4 x 10(-3) s(-1)) in tension and compression. The fatigue life, cyclic stress response, and fracture modes were significantly influenced by the waveform shape. The fatigue lives displayed by different loading conditions were in the following order: F-F > S-S > F-S > S-F. The fracture mode was dictated by the ramp rate adopted in the tensile direction. The fast ramp rate in the tensile direction led to the occurrence of transgranular crack initiation and propagation, whereas the slow ramp rate caused intergranular initiation and propagation. The time-dependent processes and their synergistic interactions, which were at the basis of observed changes in cyclic stress response and fatigue life, were identified. Oxidation, creep damage, dynamic strain aging, massive carbide precipitation, time-dependent creep deformation, and deformation ratcheting were among the several factors influencing cyclic life. Irrespective of the loading condition, the largest effect on life was exerted by oxidation processes. Deformation ratcheting had its greatest influence on life under asymmetrical loading conditions. Creep damage accumulated the greatest amount during the slow tensile ramp under S-F conditions.
引用
收藏
页码:851 / 861
页数:11
相关论文
共 50 条
  • [21] Irradiated microstructure of alloy 800H
    Gan, J
    Cole, JI
    Allen, TR
    Shutthanandan, S
    Thevuthasan, S
    JOURNAL OF NUCLEAR MATERIALS, 2006, 351 (1-3) : 223 - 227
  • [22] Oxidation Behaviour of Alloys 800H, 3033 and 304 in High-Temperature Supercritical Water
    Bsat, Suzan
    Xiao, Bingjie
    Huang, Xiao
    Penttila, Sami
    OXIDATION OF METALS, 2018, 89 (1-2): : 151 - 163
  • [23] Temperature and strain-rate effects on low-cycle fatigue behavior of alloy 800H
    Rao, KBS
    Schiffers, H
    Schuster, H
    Halford, GR
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (02): : 255 - 267
  • [24] THE EFFECT OF AGING AND COLD-WORKING ON THE HIGH-TEMPERATURE LOW-CYCLE FATIGUE BEHAVIOR OF ALLOY 800H .2. CONTINUOUS CYCLIC LOADING
    VILLAGRANA, RE
    KAAE, JL
    ELLIS, JR
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (11): : 1849 - 1857
  • [25] Oxidation Behaviour of Alloys 800H, 3033 and 304 in High-Temperature Supercritical Water
    Suzan Bsat
    Bingjie Xiao
    Xiao Huang
    Sami Penttilä
    Oxidation of Metals, 2018, 89 : 151 - 163
  • [26] Nucleation mechanisms of dynamic recrystallization in austenitic steel alloy 800H
    Brunger, E
    Wang, X
    Gottstein, G
    SCRIPTA MATERIALIA, 1998, 38 (12) : 1843 - 1849
  • [27] High strain rate behavior of alloy 800H at high temperatures
    Shafiei, E.
    JOURNAL OF NUCLEAR MATERIALS, 2016, 473 : 1 - 5
  • [28] THE DEFORMATION CHARACTERISTICS OF ALLOY 800H AND ALLOY 617
    ELAZIM, MEA
    MOHAMED, KE
    HAMMAD, FH
    MECHANICS OF MATERIALS, 1992, 14 (01) : 33 - 46
  • [29] THE EFFECT OF CHLORINE ON THE HIGH-TEMPERATURE CORROSION OF SIO2-COATED INCOLOY 800H
    HAANAPPEL, VAC
    VANCORBACH, HD
    HOFMAN, R
    FRANSEN, T
    GELLINGS, PJ
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C9): : 921 - 930
  • [30] A SEM study of creep and thermal fatigue failure in naphtha cracking furnace tubes made of 800H alloy
    Tekin, E
    ELECTRON MICROSCOPY 1998, VOL 2: MATERIALS SCIENCE 1, 1998, : 255 - 256