Microstructure and thermal stability of arc-evaporated Cr-C-N coatings

被引:14
|
作者
Almer, J
Odén, M
Håkansson, G
机构
[1] Lulea Tekn Univ, Div Engn Mat, SE-97187 Lulea, Sweden
[2] Argonne Natl Lab, Adv Photon Source, Argonne, IL 60439 USA
[3] Bodycote Varmebehandling AB, SE-58271 Linkoping, Sweden
关键词
D O I
10.1080/14786430310001646727
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The role of C incorporation in the microstructure and thermal stability of arc-evaporated Cr-C-N coatings is explored via reactive growth in a mixed C2H4-N-2 environment. C is found to react more readily than N at both the Cr cathode and the coating surfaces, so that a C2H4-to-N-2 flow ratio of only 1% yields a C-to-N ratio of approximately 10% within the coatings. The as-deposited microstructures consist primarily of the delta-Cr(C, N) phase and possess high compressive residual stresses, which decrease with increasing C content. Post-deposition annealing up to 700degreesC results in depletion of lattice defects, and concomitant reductions in stress and coating hardness, together with phase transformations which suggest metastable phase formation during growth. Apparent activation energies for this lattice defect are found to be in the range expected for bulk diffusion of N and C (2.4-2.8 eV). The results suggest that inclusion of small amounts of C in this system offers the ability to reduce internal stresses while maintaining defect-related hardness increases, permitting growth of thicker and thus more wear-resistant coatings.
引用
收藏
页码:611 / 630
页数:20
相关论文
共 50 条
  • [21] Properties and applications of ionplated coatings in the system CR-C-N
    Schulz, H.
    Bergmann, E.
    Dupont, F.
    Vide, les Couches Minces, 1991, (259 Supp):
  • [22] Arc-evaporated nanocomposite zirconium-based boronitride coatings
    Chapusot, V.
    Pierson, J. F.
    Lapostolle, F.
    Billard, A.
    MATERIALS CHEMISTRY AND PHYSICS, 2009, 114 (2-3) : 780 - 784
  • [23] Investigation on structure and properties of arc-evaporated HfAlN hard coatings
    Franz, R.
    Mitterer, C.
    Lechthaler, M.
    Polzer, C.
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2010, 28 (04): : 528 - 535
  • [24] Thermal stability of arc evaporated Al-Cr-O and Al-Cr-O/Al-Cr-N multilayer coatings
    Raab, R.
    Koller, C. M.
    Kolozsvari, S.
    Ramm, J.
    Mayrhofer, P. H.
    SURFACE & COATINGS TECHNOLOGY, 2018, 352 : 213 - 221
  • [25] Cr-C-N coatings deposited with different reactive carbon carrier gases in the arc PVD process
    Aachen Univ of Technology, Aachen, Germany
    Surf Coat Technol, 1-3 (416-421):
  • [26] Cr-C-N coatings deposited with different reactive carbon carrier gases in the arc PVD process
    Lugscheider, E
    Knotek, O
    Barimani, C
    Guerreiro, S
    Zimmermann, HK
    SURFACE & COATINGS TECHNOLOGY, 1997, 94-5 (1-3): : 416 - 421
  • [27] Influence of Fe impurities on structure and properties of arc-evaporated AlCrN coatings
    Muehlbacher, M.
    Franz, R.
    Paulitsch, J.
    Rudigier, H.
    Polcik, P.
    Mayrhofer, P. H.
    Mitterer, C.
    SURFACE & COATINGS TECHNOLOGY, 2013, 215 : 96 - 103
  • [28] Micro- and bonding structure of arc-evaporated AlCrVN hard coatings
    Franz, R.
    Neidhardt, J.
    Sartory, B.
    Tessadri, R.
    Mitterer, C.
    THIN SOLID FILMS, 2008, 516 (18) : 6151 - 6157
  • [29] Oxidation behaviour and tribological properties of arc-evaporated ZrAlN hard coatings
    Franz, R.
    Lechthaler, M.
    Polzer, C.
    Mitterer, C.
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (8-9): : 2337 - 2345
  • [30] MOCVD of hard metallurgical coatings: Examples in the Cr-C-N system
    Maury, F
    ELECTROCHIMICA ACTA, 2005, 50 (23) : 4525 - 4530