Effect of Overaging on the Cyclic Deformation Behavior of an AA6061 Aluminum Alloy

被引:13
|
作者
Liu, Kun [1 ]
Mirza, Foisal Ahmed [1 ]
Chen, Xiao Grant [1 ]
机构
[1] Univ Quebec Chicoutimi, Dept Appl Sci, 555 Blvd Univ, Chicoutimi, PQ G7H 2B1, Canada
来源
METALS | 2018年 / 8卷 / 07期
基金
加拿大自然科学与工程研究理事会;
关键词
6061 aluminum alloys; aging treatments; precipitates; cyclic deformation; fatigue life; STRESS-STRAIN RESPONSE; MG-SI ALLOYS; MECHANICAL-PROPERTIES; FATIGUE PROPERTIES; PRECIPITATION SEQUENCE; FRACTURE-BEHAVIOR; MAGNESIUM ALLOY; MICROSTRUCTURE; TEMPERATURE; TENSILE;
D O I
10.3390/met8070528
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present work encompasses the effect of overaging on the strain-controlled low-cycle fatigue (LCF) behavior of an extruded AA6061 aluminum alloy at varying strain amplitudes. During the T7 aging treatment, the size of precipitates increased from 60 nm under T6 conditions to 220 nm after aging for 48 h at 200 degrees C, leading to a decrease in the monotonic tensile strength. During the LCF tests, nearly symmetrical hysteresis loops can be observed in the mid-life cycle under all test conditions, whereas the first-cycle hysteresis loops were moderately inflected under long-aging conditions. With increasing aging time, the cyclic peak stresses decreased and the plastic strain increased. Nearly ideal Masing behavior was exhibited under T6 conditions, while it was lost under T7 overaging conditions. The cyclic stress responses were similar under all tested conditions, involving stabilization at low strain amplitudes and softening at high strain amplitudes, with initial hardening for the first few cycles. Compared to the T6 condition, the fatigue life increased with increasing T7 aging time. Various LCF parameters were estimated based on the Coffin-Manson and Basquin relationships and on the LCF experimental results. The relationship between the fatigue life, strength, and microstructure of the investigated AA6061 aluminum alloy under various aging conditions was discussed.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] A study on the combined effect of aging and severe plastic deformation on the mechanical properties of AA6061 alloy
    Muralidharan, S.
    Kumar, S. Arun
    Iqbal, U. Mohammed
    3RD INTERNATIONAL CONFERENCE ON ADVANCES IN MECHANICAL ENGINEERING (ICAME 2020), PTS 1-6, 2020, 912
  • [42] Microstructure and Mechanical Properties of Cold Roll-Bonded Layered AA6061/AA5052/AA6061/AA5052 Aluminum Alloy Sheet
    Jo, Sang-Hyeon
    Park, Bo-Bae
    Lee, Seong-Hee
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2022, 32 (03): : 161 - 167
  • [43] Effect of SPD Processing on the Strength and Conductivity of AA6061 Alloy
    Qi, Yuanshen
    Kosinova, Anna
    Lakin, Eugene
    Popov, Vladimir V., Jr.
    Rabkin, Eugen
    Lapovok, Rimma
    ADVANCED ENGINEERING MATERIALS, 2019, 21 (08)
  • [44] Effects of strain localization on the corrosion behavior of ultra-fine grained aluminum alloy AA6061
    Ly, Ramatou
    Hartwig, Karl T.
    Castaneda, Homero
    CORROSION SCIENCE, 2018, 139 : 47 - 57
  • [45] Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy
    Zaid, B.
    Saidi, D.
    Benzaid, A.
    Hadji, S.
    CORROSION SCIENCE, 2008, 50 (07) : 1841 - 1847
  • [46] Tribological behavior of friction stir processed AA6061 aluminium alloy
    Shaik, Dilkush
    Sudhakar, I
    Bharat, G. C. S. G.
    Varshini, V.
    Vikas, S.
    MATERIALS TODAY-PROCEEDINGS, 2021, 44 : 860 - 864
  • [47] Post-weld Oxidation Behavior of AA6061 Al Alloy
    CheLah, Nur Azida
    Jalar, Azman
    Othman, Norinsan Kamil
    NEW MATERIALS, APPLICATIONS AND PROCESSES, PTS 1-3, 2012, 399-401 : 2087 - 2090
  • [48] MICROSTRUCTURE AND HARDNESS OF EXTRUSION WELDING ON HOLLOW PANEL AA6061 ALUMINUM ALLOY
    Sutowijoyo, A. B. P.
    Putri, E. D. W. S.
    Muhayat, N.
    Prabowo, A. R.
    Depari, Y. P. D. S.
    Triyono
    METALURGIJA, 2025, 64 (1-2): : 17 - 19
  • [49] Properties of AA6061 aluminum alloy reinforced with different intermetallics and ceramics particles
    da Costa, Cesar Edil
    de Aguiar, Luana
    Borras, Vicente Amigo
    ADVANCED POWDER TECHNOLOGY V, 2006, 530-531 : 255 - +