Accelerated Concrete-Cylinder Test for Alkali-Silica Reaction

被引:4
|
作者
Liu, Kai-Wei [1 ]
Mukhopadhyay, Anol K. [2 ]
机构
[1] Texas A&M Univ, Zachry Dept Civil Engn, 199 Spence St 501H CE TTI, College Stn, TX 77843 USA
[2] Texas A&M Univ, Texas A&M Transportat Inst, 199 Spence St 501B CE TTI, College Stn, TX 77843 USA
关键词
alkali-silica reaction; accelerated concrete test; validation of ASR mix; PORE SOLUTION; PORTLAND-CEMENT; PASTE; ASR;
D O I
10.1520/JTE20140334
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The concrete-prism test (CPT, e.g., ASTM C1293-08b [ASTM C1293-08b: Standard Test Method for Determination of Length Change of Concrete Due to Alkali-Silica Reaction, Annual Book of ASTM Standards, ASTM International, West Conshohocken, PA, 2013]) has been considered as the best index for alkali-silica reaction (ASR) field performance, but alkali leaching and test duration are still of concern. Reduction of test duration by increasing testing temperature (e.g., 60 degrees C) was proposed by several researchers to develop an accelerated version of the concrete-prism test (ACPT). However, it has been found that there is a significant reduction in expansion associated with more alkali leaching in the ACPT compared to the concrete-prism test (CPT). An accelerated concrete-cylinder test (ACCT) has been proposed in this study with no involvement of errors because of operation and temperature change along with arresting alkali leaching. The linear expansion of the ACCT measured at a temperature of 60 degrees C over a period of 1 month have been correlated with the 1-yr ASTM C1293 test to evaluate the ASR reactivity of aggregates. Cylinders made with highly reactive borosilicate glass balls were tested first to validate the proposed approach before any concrete-cylinder testing. The results indicate that (1) an expansion limit of 0.04 % using 0.82 % Na2O equivalent (Na2Oe) cement without alkali boosting after a testing period of 28 days is proposed for the ACCT to diagnose ASR aggregate reactivity, and (2) the proposed method can serve as an alternative to validate the ASR-resistant mix design (e.g., fly-ash contents).
引用
收藏
页码:1229 / 1238
页数:10
相关论文
共 50 条
  • [31] DIFFUSION-REACTION MODEL FOR ALKALI-SILICA REACTION IN CONCRETE
    Liaudat, Joaquin
    Lopez, Carlos M.
    Carol, Ignacio
    COMPUTATIONAL PLASTICITY XII: FUNDAMENTALS AND APPLICATIONS, 2013, : 479 - 489
  • [32] Alkali-Silica Reaction in Concrete with Previously Inert Aggregates
    Deschenes, Richard A.
    Hale, W. Micah
    JOURNAL OF PERFORMANCE OF CONSTRUCTED FACILITIES, 2017, 31 (02)
  • [34] Mitigation of alkali-silica reaction in US highway concrete
    Folliard, Kevin J.
    Thomas, Michael D. A.
    Fournier, Benoit
    Drimalas, Thano
    Ahlstrom, Gina
    PROCEEDINGS OF THE INSTITUTION OF CIVIL ENGINEERS-CONSTRUCTION MATERIALS, 2016, 169 (04) : 215 - 222
  • [36] DAMAGE OF CONCRETE BY SULFATE ATTACK AND ALKALI-SILICA REACTION
    Collepardi, M.
    ADVANCES IN CONCRETE STRUCTURAL DURABILITY, PROCEEDINGS OF ICDCS2008, VOLS 1 AND 2, 2008, : 3 - 9
  • [37] Macroscopic and Mesoscopic Approach to the Alkali-Silica Reaction in Concrete
    Grymin, Witold
    Koniorczyk, Marcin
    Pesavento, Francesco
    Gawin, Dariusz
    COMPUTER METHODS IN MECHANICS (CMM2017), 2018, 1922
  • [38] Novel admixtures for mitigation of alkali-silica reaction in concrete
    Kaladharan, Gopakumar
    Szeles, Tiffany
    Stoffels, Shelley M.
    Rajabipour, Farshad
    CEMENT & CONCRETE COMPOSITES, 2021, 120
  • [39] Coatings and overlays for concrete affected by alkali-silica reaction
    Giannini, E. R.
    Bentivegna, A. F.
    Folliard, K. J.
    CONCRETE SOLUTIONS, 2012, : 823 - 831
  • [40] Prestressed concrete members affected by alkali-silica reaction
    Rogers, C.A.
    Tharmabala, T.
    Concrete International, 1990, 12 (08) : 35 - 39