Fracture resistant and wear corrosion performance of CrN/ZrN bilayers deposited onto AISI 420 stainless steel

被引:15
|
作者
de Sanchez, N. A. [1 ,4 ]
Jaramillo, H. E. [1 ,4 ]
Vivas, Z. [1 ,2 ]
Aperador, W. [3 ]
Amaya, C. [4 ]
Caiced, J. C. [4 ]
机构
[1] Univ Autonoma Occidente, Dept Energet & Mech, Dept Engn Basic Sci, Sci & Engn Mat Grp, Cali, Colombia
[2] COLCIENCIAS, Young Res, Cali, Colombia
[3] CDT ASTIN SENA, Engn & Mat Dev Grp, Cali, Colombia
[4] CENM, Excellence Ctr Novel Mat, Cali, Colombia
来源
关键词
bilayers; atomic force microscopy; corrosion; mechanical properties; magnetron sputtering; stainless steel;
D O I
10.4028/www.scientific.net/AMR.38.63
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
CrN/ZrN (1, 8, 15, and 30) bilayers were deposited onto AISI 420 steel substrates at 250 degrees C and 6.6x10(-3) mbar with gas ratio Ar/N2 50:3.0 as gas mixture and bias -60V were applied. AFM analysis presented different morphologies, showing that the coatings with 15 bilayers had an average grain size of 49 nm; while the 30-bilayer coating exhibited grain sizes of 99 nm. Coating thicknesses were 3 mu m, approximately. The Vickers Test revealed that coatings with 8, 15, and 30 bilayers bore better impact resistance than coatings with I bilayer. This result is considered, bearing in mind that in many bilayers propagation of fissures is slower, because the presence of layer inter-phases leads to fissures straying in other directions. Slight corrosion specks are present, but mass loss was around 40 mg. in one bilayer, a higher value than for the coatings with 15 bilayers that was near 18 mg. Homogeneity, grain size, fracture resistance, and corrosion resistance of the coatings with 15 and 30 bilayers are suitable for mechanical applications of these types of coatings, as shown in mechanical measurements. These results indicate that for engineering applications under corrosive environments, the use of these types of bilayer coatings on AISI 420 stainless steel is highly recommended.
引用
收藏
页码:63 / +
页数:3
相关论文
共 50 条
  • [41] FRICTIONAL AND WEAR PROPERTIES OF HARD CARBON DEPOSITED ONTO STAINLESS-STEEL
    MIYAKE, S
    TAKAHASHI, S
    WATANABE, I
    YOSHIHARA, H
    JOURNAL OF JAPAN SOCIETY OF LUBRICATION ENGINEERS, 1986, 31 (03): : 169 - 176
  • [42] CORROSION RESISTANCE OF [TiN/AlTiN]n MULTILAYERS DEPOSITED ONTO AISI 1045 STEEL
    Aperador, William
    Amaya, Cesar
    Espana, Claudia
    DYNA-COLOMBIA, 2011, 78 (165): : 183 - 189
  • [43] Investigating the erosive wear characteristics of AISI 420 martensitic stainless steel after surface hardening by boriding
    Cakir, Oguzhan
    Demirsoz, Recep
    Ozdemir, Mehmet Tayyip
    Korkmaz, Mehmet Erdi
    Gupta, Munish Kumar
    Gunay, Mustafa
    Ross, Nimel Sworna
    Nag, Akash
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 2292 - 2302
  • [44] Characterization of Hydrophobic Silane Film Deposited on AISI 304 Stainless Steel for Corrosion Protection
    Akinlabi, E. T.
    Baruwa, A. D.
    Oladijo, O. P.
    Maledi, N.
    Chinn, J.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (10) : 6330 - 6339
  • [45] Highly corrosion resistant stainless steel with Si implanted/deposited phase
    Nishimura, R
    Yamakawa, K
    Ishiga, J
    Matsumoto, Y
    Nagano, H
    MATERIALS CHEMISTRY AND PHYSICS, 1998, 54 (1-3) : 289 - 292
  • [46] Characterization of Hydrophobic Silane Film Deposited on AISI 304 Stainless Steel for Corrosion Protection
    E. T. Akinlabi
    A. D. Baruwa
    O. P. Oladijo
    N. Maledi
    J. Chinn
    Journal of Materials Engineering and Performance, 2019, 28 : 6330 - 6339
  • [47] The corrosion and wear behavior of TiN and TiAlN coated AISI 316 L stainless steel
    Yusuf Kayali
    Protection of Metals and Physical Chemistry of Surfaces, 2014, 50 : 412 - 419
  • [48] STUDY OF CORROSION BEHAVIOR AND WEAR OF COATINGS IN BILAYERS OF W/WC GROWN IN THE AISI 304 STEEL
    Jaramillo, H. E.
    Alba, N.
    Teran, G.
    Villamil, B.
    HOMBRE Y LA MAQUINA, 2007, (28): : 88 - 97
  • [49] Microstructure and wear performance of arc-deposited Ti-N-O coatings on AISI 304 stainless steel
    Hsu, Cheng-Hsun
    Huang, Kuan-Hao
    Lin, Ya-Huei
    WEAR, 2013, 306 (1-2) : 97 - 102
  • [50] The corrosion and wear behavior of TiN and TiAlN coated AISI 316 L stainless steel
    Kayali, Yusuf
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2014, 50 (03) : 412 - 419