Experimental and numerical investigation on SiC coating delamination from C/SiC composites

被引:22
|
作者
Jia, Jingmin [1 ,2 ]
Fang, Xufei [1 ,2 ]
Zhang, Weixu [3 ]
Feng, Xue [1 ,2 ]
机构
[1] Tsinghua Univ, Dept Engn Mech, AML, Beijing 100084, Peoples R China
[2] Tsinghua Univ, Ctr Mech & Mat, Beijing 100084, Peoples R China
[3] Xi An Jiao Tong Univ, Dept Engn Mech, State Key Lab Strength & Vibrat Mech Struct, Xian 710049, Peoples R China
基金
中国国家自然科学基金;
关键词
Coating; Delamination; Fracture; Flexural test; Finite element analysis; OXIDATION BEHAVIOR; VAPOR; TEMPERATURE; FILMS;
D O I
10.1016/j.compscitech.2015.02.012
中图分类号
TB33 [复合材料];
学科分类号
摘要
The delamination of SiC coating on C/SiC composites leads to severe oxidation of the carbon fibers and causes reliability problems of these composites during service. In this study, flexural test was conducted at room temperature to analyze the delamination behavior of SiC coating deposited on C/SiC substrate and finite element method (FEM) was adopted to simulate the interfacial crack between the SiC coating and the C/SiC substrate based on the experimental results. Results show that the fiber orientation has significant influence on the delamination of surface SiC coating. When the SiC coating is deposited parallel to the fiber orientation and interfacial delamination direction is along fiber direction, once delamination occurs, it inclines to propagate. However, when coating is prepared in other directions, the delamination inclines to be crested. The present analyses show that a proper combination of different fiber orientations can decrease the delamination of coating for better service of the materials in applications. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:210 / 216
页数:7
相关论文
共 50 条
  • [31] Oxidation resistance and thermal cycling properties of the SiCnws-SiC coating on the C/SiC composites
    Wang, Bo
    Zhang, Fan
    Hao, Jianjie
    He, Ping
    Shi, Wei
    Tan, Yi
    Li, Jiayan
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2023, 20 (03) : 1793 - 1803
  • [32] Characterization of coating cracks in oxidation-resistant SiC coating on C C composites
    Aoki, T
    Hatta, H
    Goto, K
    Fukuda, H
    HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES III, 1999, 164-1 : 283 - 286
  • [33] SiC Nanowires Toughed HfC Ablative Coating for C/C Composites
    Hejun Li
    Yongjie Wang
    Qiangang Fu
    Yanhui Chu
    JournalofMaterialsScience&Technology, 2015, 31 (01) : 70 - 76
  • [34] Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites
    Cheng, LF
    Xu, YD
    Zhang, LT
    Luan, XG
    CARBON, 2002, 40 (12) : 2229 - 2234
  • [35] Fabrication of LIG coating on SiC/SiC composites with femtosecond laser
    Zhai, Zhaoyang
    Wu, Ningqiang
    Wang, Zhilong
    Zhang, Yanfei
    Song, Danlong
    Cui, Yahui
    OPTIK, 2021, 245
  • [36] Oxidation-resistant SiC coating system of C/C composites
    Sato, N
    Shiota, I
    Hatta, H
    Aoki, T
    Fukuda, H
    FUNCTIONALLY GRADED MATERIALS 1996, 1997, : 257 - 262
  • [37] SiC Nanowires Toughed HfC Ablative Coating for C/C Composites
    Li, Hejun
    Wang, Yongjie
    Fu, Qiangang
    Chu, Yanhui
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 31 (01) : 70 - 76
  • [38] The Research of the Carbon Coating on SiC Fiber and the SiCf/SiC Composites
    刘伟峰
    王亦菲
    叶飞
    材料导报, 2007, (S1) : 237 - 238
  • [39] Experimental study and numerical modeling of pulse CVI for the production of organomorphic C/SiC composites
    Kulik, Alexey
    Bogachev, Evgeny
    Kulik, Victor
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2022, 19 (01) : 91 - 100
  • [40] Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites
    Christin, F
    ADVANCED ENGINEERING MATERIALS, 2002, 4 (12) : 903 - 912