Effect of Cryogenic Treatment Prior to Rolling on Micro-structure and Mechanical Properties of AZ31 Magnesium Alloy

被引:5
|
作者
Huang Zhiquan [1 ]
Wei Jianchun [2 ]
Huang Qingxue [1 ]
Ma Lifeng [1 ]
Gao Xiangyu [1 ]
Yue Zhaohan [1 ]
机构
[1] Taiyuan Univ Sci & Technol, Minist Educ, Heavy Machinery Engn Res Ctr, Taiyuan 030024, Peoples R China
[2] Guangxi Liuzhou Iron & Steel Grp Co Ltd, Liuzhou 545002, Peoples R China
基金
中国国家自然科学基金;
关键词
AZ31 magnesium alloy; cryogenic treatment; second phase particles; fracture morphology; WEAR BEHAVIOR; STEEL; DEFORMATION; AZ91;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of cryogenic treatment prior to hot rolling on the strength, toughness and ductility of as-cast AZ31 magnesium alloy plates were investigated. The cryogenic treatment conditions were -60 degrees C/12 h, -120 degrees C/12 h, -180 degrees C/I2 h, -60 degrees C/2 h, and -180 degrees C/2 h. Experimental results show that appropriate cryogenic treatment conditions can significantly refine the grain size and the improve strength, toughness and ductility. A large number of twins appear in both kinds of samples cryogenically treated for 2 h. The sample experienced cryogenic treatment for 12 h at -60 degrees C followed by rolling process shows the finest and most uniform and increase in yield strength by 25.8%. Meanwhile, a four-time increase in extension rate (3.06% to 12.31%) is attains. The tensile fracture present a mixed-mode fracture, which is characteristic of brittle and ductile fracture mechanisms.
引用
收藏
页码:2942 / 2948
页数:7
相关论文
共 50 条
  • [21] Effect of Aging on the Microstructure and Mechanical Properties of Magnesium Alloy AZ31
    H. Kerenciler
    S. Gündüz
    M. Akif Erden
    M. Türkmen
    H. Karabulut
    Metal Science and Heat Treatment, 2016, 58 : 179 - 184
  • [22] Effect of rolling deformation on microstructure of AZ31 magnesium alloy
    Chen, Jing-Yi
    Zhang, Bo-Ping
    Tu, Yi-Fan
    Li, Peng-Xi
    Suzuki, Hirowo G.
    AICAM 2005, 2006, 11-12 : 649 - +
  • [23] Effects of differential speed rolling on microstructure and mechanical properties of AZ31 magnesium alloy
    Huang, Xinsheng
    Suzuki, Kazutaka
    Kwon, Yong-Jai
    Watazu, Akira
    Shigematsu, Ichinori
    Saito, Naobumi
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 1759 - +
  • [24] Microstructure and Mechanical Properties of AZ31 Magnesium Alloy Sheet Processed by Asymmetry Rolling
    Song Guangsheng
    Jiang Jingqian
    Chen Shuaifeng
    Zhang Shihong
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (11) : 3512 - 3517
  • [25] Mechanical properties and texture evolution during hot rolling of AZ31 magnesium alloy
    孙宏飞
    梁书锦
    王尔德
    Transactions of Nonferrous Metals Society of China, 2009, 19 (S2) : 349 - 354
  • [26] Mechanical properties and texture evolution during hot rolling of AZ31 magnesium alloy
    Sun Hong-fei
    Liang Shu-jin
    Wang Er-de
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 : S349 - S354
  • [27] Hot rolling of AZ31 magnesium alloy and its effects on microstructure and mechanical properties
    Chen, B
    Lin, DL
    Zeng, XQ
    Lu, C
    MAGNESIUM - SCIENCE, TECHNOLOGY AND APPLICATIONS, 2005, 488-489 : 619 - 622
  • [28] Mechanical properties and formability of AZ31 magnesium alloy processed by differential speed rolling
    Huang, Xinsheng
    Suzuki, Kazutaka
    Watazu, Akira
    Shigematsu, Ichinori
    Saito, Naobumi
    ECO-MATERIALS PROCESSING AND DESIGN VIII, 2007, 544-545 : 395 - +
  • [29] EFFECT OF INITIAL TEMPERATURE ON THE MICROSTRUCTURE AND PROPERTIES OF CRYOGENIC ROLLED AZ31 MAGNESIUM ALLOY
    Wu, Zhenyu
    Zhi, Chenchen
    Ma, Lifeng
    Zheng, Zebang
    Zhu, Yanchun
    Jia, Weitao
    MATERIALI IN TEHNOLOGIJE, 2022, 56 (05): : 571 - 577
  • [30] The effect of surface mechanical attrition treatment on texture evolution and mechanical properties of AZ31 magnesium alloy
    Peng, Jinhua
    Zhang, Zhen
    Guo, Peng
    Liu, Zhao
    Li, Yaozu
    Zhou, Wei
    Wu, Yucheng
    MATERIALS CHARACTERIZATION, 2019, 148 : 26 - 34