Thermal stability of bulk nanocrystalline Ti-10V-2Fe-3Al alloy

被引:11
|
作者
Chen, Wei [1 ,2 ]
Sun, Qiaoyan [1 ]
Xiao, Lin [1 ]
Sun, Jun [1 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
[2] Xi An Jiao Tong Univ, State Key Lab Mech Struct Strength & Vibrat, Xian 710049, Peoples R China
基金
中国博士后科学基金;
关键词
Ti-10V-2Fe-3Al alloy; Nanocrystalline; Thermal stability; Microstructure; Vickers hardness; SEVERE PLASTIC-DEFORMATION; TO-RUTILE TRANSFORMATION; NANOSTRUCTURED MATERIALS; MECHANICAL-PROPERTIES; TITANIA POWDERS; GRAIN-GROWTH; BEHAVIOR; REFINEMENT; MICROSTRUCTURE; COPPER;
D O I
10.1016/j.msea.2012.01.001
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Thermal stability of the nanocrystalline Ti-10V-2Fe-3Al alloy produced by cold-forging and corresponding hardness variations were investigated. When the annealing temperature was lower than 400 degrees C, the primary features were the decline of lattice defect density and the increase of lattice ordering level in the vicinity of grain boundaries, named as grain boundary relaxation. The nanocrystalline grains grew slowly. In comparison, when the annealing temperature was higher than 400 degrees C, the decomposition of the deformation-induced alpha '' martensites and the subsequent rapid grain growth were observed. Vickers hardness measurement shows an initial hardening followed by a softening with the increase of annealing temperature. The hardening peak appeared at 400 degrees C. The critical grain growth temperature, i.e.. T-cgg, in the nanocrytalline Ti-10V-2Fe-3Al alloy, was slightly lower than those in other nanocrystalline alloys. That could be attributed to the martensitic decomposition-induced grain growth in this alloy. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:223 / 230
页数:8
相关论文
共 50 条
  • [41] Compositions of ω and α in Ti-10V-2Fe-3Al alloy analyzed by TEM-EDX system
    Yamamoto, A
    Tsubakino, H
    NON-AEROSPACE APPLICATIONS OF TITANIUM, 1998, : 53 - 60
  • [42] Effect of α Composite Layer on the Microstructure and Mechanical Properties of Ti-10V-2Fe-3Al Alloy
    Bai Xinfang
    Zhao Yongqing
    Zeng Weidong
    Jia Zhiqiang
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (01) : 12 - 17
  • [43] Fabrication and characterization of anodic oxide films on a Ti-10V-2Fe-3Al titanium alloy
    Liu, Jian-hua
    Yi, Jun-lan
    Li, Song-mei
    Yu, Mei
    Xu, Yong-zhen
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2009, 16 (01) : 96 - 100
  • [44] Influence of hot rolling deformation on microstructure and properties of Ti-10V-2Fe-3Al alloy
    Shang, Guo-Qiang
    Zhu, Zhi-Shou
    Kou, Hong-Chao
    Wang, Xin-Nan
    Fei, Yue
    Chang, Hui
    Li, Jin-Shan
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2013, 34 (03): : 108 - 113
  • [45] Correlation of dynamic response with adiabatic shearing behavior in Ti-10V-2Fe-3Al alloy
    Ding, Qingwen
    Ren, Yu
    Tan, Chengwen
    Zhang, Jing
    Yu, Xiaodong
    MATERIALS AND DESIGN, PTS 1-3, 2011, 284-286 : 1542 - 1545
  • [46] Study of the Effect of Carbon on the Deformation Behavior and Microstructure of a Ti-10V-2Fe-3Al Alloy
    Zhelnina, A. V.
    Kalienko, M. S.
    Shchetnikov, N. V.
    PHYSICS OF METALS AND METALLOGRAPHY, 2021, 122 (02): : 154 - 160
  • [47] Evolution of adiabatic shear bands in the beta titanium alloy Ti-10V-2Fe-3Al
    Winter, S.
    Scholze, M.
    Wagner, M. F-X
    19TH CHEMNITZ SEMINAR ON MATERIALS ENGINEERING, 2017, 181
  • [49] Effect of α composite layer on the microstructure and mechanical properties of Ti-10V-2Fe-3Al alloy
    Bai, Xinfang
    Zhao, Yongqing
    Zeng, Weidong
    Jia, Zhiqiang
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2015, 44 (01): : 12 - 17
  • [50] Effect of heat treatment on hardness and electrical resistivity of Ti-10V-2Fe-3Al alloy
    Sugiura, Y
    Hamai, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1998, 84 (06): : 458 - 463