Effect of Minor Alloying Elements (C, Ni, Cr, Mo) on the Long-Term Corrosion Behaviors of Ultrahigh-Strength Automotive Steel Sheet in Neutral Aqueous Environment

被引:8
|
作者
Bang, Hye Rin [1 ]
Park, Jin-seong [1 ]
Seong, Hwan Goo [2 ]
Kim, Sung Jin [1 ]
机构
[1] Sunchon Natl Univ, Dept Adv Mat Engn, Sunchon 57922, South Korea
[2] POSCO Tech Res Labs, Gwangyang 57807, South Korea
来源
基金
新加坡国家研究基金会;
关键词
ultrahigh-strength steel; carbon; nickel; chromium; molybdenum; corrosion; HYDROGEN DIFFUSION BEHAVIORS; RESISTANCE; TOUGHNESS; EMBRITTLEMENT; MORPHOLOGY;
D O I
10.3365/KJMM.2022.60.1.35
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study examined the effects of minor alloying elements (C, Ni, Cr, and Mo) on the long-term corrosion behaviors of ultrahigh-strength automotive steel sheets with a tensile strength of more than 1800 MPa. A range of experimental and analytical results showed that the addition of Ni, Cr, and Mo decreased the corrosion current density and weight loss in electrochemical and immersion tests, respectively, in a neutral aqueous condition. This suggests that the minor addition of elements to steel can result in improved corrosion resistance even for long-term immersion periods. This is closely associated with the formation of thin and stable corrosion scale on the surface, which was enriched with the alloying elements (Ni, Cr, and Mo). On the other hand, their beneficial effects did not persist during the prolonged immersion periods in steel with a higher C content, suggesting that the beneficial effects of the minor addition of Ni, Cr, and Mo were overridden by the detrimental effects of a higher C content as the immersion time was increased. Based on these results, lower C and the optimal use of Ni, Cr, and Mo are suggested as a desirable alloy design strategy for developing ultrahigh-strength steel sheets that can be exposed frequently to a neutral aqueous environment. (Received August 17, 2021; Accepted November 18, 2021)
引用
收藏
页码:35 / 45
页数:11
相关论文
共 29 条
  • [21] Effect of long-term aging on near-threshold fatigue crack growth of Ni-Cr-Mo-V steel welds
    Du, Yan-Nan
    Zhu, Ming-Liang
    Liu, Xia
    Xuan, Fu-Zhen
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 226 : 228 - 237
  • [22] Abnormal Structure in Long-term Used Mod.9Cr-1Mo Steel Welded Joint and Its Effect on Creep Strength
    Zhang, Shengde
    Tokunaga, Hayato
    Kanai, Masayuki
    Yaguchi, Masatsugu
    Tamura, Koji
    Minami, Yusuke
    Zairyo/Journal of the Society of Materials Science, Japan, 2023, 72 (07): : 542 - 549
  • [23] The cumulative effect of alloying elements N, W, Mo and Cu on the corrosion behaviour of 17Cr-13Ni stainless steel in 2 N H2SO4
    Belfrouh, A
    Masson, C
    Vouagner, D
    DeBecdelievre, AM
    Prakash, NS
    Audouard, JP
    CORROSION SCIENCE, 1996, 38 (10) : 1639 - 1648
  • [24] Effect of long-term aging on microstructure and local behavior in the heat-affected zone of a Ni-Cr-Mo-V steel welded joint
    Zhu, Ming-Liang
    Wang, De-Qiang
    Xuan, Fu-Zhen
    MATERIALS CHARACTERIZATION, 2014, 87 : 45 - 61
  • [25] Effect of W and Mo contents on the microstructural evolution and properties in the 9% Cr martensitic rotor steel during long-term aging at 630 °C
    Qiu, Jiajia
    He, Xikou
    Liu, Zhengdong
    Tang, Zhengxin
    Wang, Xitao
    He, Jinshan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 152 - 164
  • [26] The cumulative effect of alloying elements N, W, Mo and Cu on the corrosion behaviour of 17Cr-13Ni stainless steel in 2N H2SO4
    Lab. de Chim. Appl. et Genie Chim., Université Claude Bernard, Lyon 1, 69622 Villeurbanne Cedex, France
    不详
    Corros Sci, 10 (1639-1648):
  • [27] EFFECT OF MO AND W ON LONG-TERM CREEP-RUPTURE STRENGTH OF 12-PERCENT-CR HEAT-RESISTING STEEL CONTAINING V, NB AND B
    FUJITA, T
    SATO, T
    TAKAHASHI, N
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1978, 18 (02) : 115 - 124
  • [28] Effect of Reactor Irradiation on Long-term Strength and Creep of OCr16Ni15Mo3Mb Steel in Plane Stressed State - 2. Long-term Strength Criterion with Consideration of the Initial Material Structure Parameter.
    Khristov, G.P.
    Kosov, B.D.
    Problemy Prochnosti, 1981, (07):
  • [29] Long-term salt spray corrosion behaviors of HVOF-sprayed WC-Cr3C2-Ni coatings before and after vacuum sealing with silicone resin
    Wei, Ziyu
    Qin, Jiyue
    Wang, Kailin
    Hong, Sheng
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2023, 117