Observations during crystallisation of poly(ethylene-co-butylene naphthalene-2,6-dicarboxylate)s

被引:14
|
作者
Papageorgiou, GZ [1 ]
Karayannidis, GP [1 ]
机构
[1] Aristotle Univ Thessaloniki, Dept Chem, Div Organ Chem Technol, GR-54006 Thessaloniki, Macedonia, Greece
关键词
poly(ethylene naphthalate); poly(butylene naphthalate); isothermal crystallisation;
D O I
10.1016/S0032-3861(01)00318-4
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The crystallisation behaviour of poly(ethylene-co-butylene naphthalene-2,6-dicarboxylate)s (PEBN copolyesters) was studied by means of differential scanning calorimetry (DSC). A eutectic behaviour was found, and the composition related with the lower melting point was about 50/50 mol%. On the other hand, the crystallisation kinetics was faster for copolymers with high butylene-naphthalate content, while the slower crystallisation rates were observed for the PEEN 70/30. Crystallisation and melting of PEEN 50/50 and PEEN 70/30 copolymers are of special interest. Despite its composition, the PEEN 50/50 copolyester exhibited significant crystallinity and fast crystallisation rates. Cooling from the melt resulted in crystallisation at T-c = 106 degreesC, quite close to the glass transition temperature (T-g = 92 degreesC). On isothermal crystallisation at temperatures near T-c region, double exothermic peaks in the heat flow vs, time plot were observed. For amorphous samples, in the DSC traces on heating, a sharp cold-crystallisation peak (T-cc 125 degreesC), followed by a second exothermal peak, was observed. The relatively low melting point (T-m = 196 degreesC), comparing with those of the other PEEN copolymers was attributed to limited crystal lamellar thickness. For the PEEN 70/30, crystallisation was very slow. Even after prolonged crystallisation times, a quadruplicate melting peak was observed which was attributed to melting of metastable crystalline phases initially formed. (C) 2001 Published by Elsevier Science Ltd.
引用
收藏
页码:8197 / 8205
页数:9
相关论文
共 50 条
  • [31] Influence of the crystalline structure in the segmental mobility of semicrystalline polymers: Poly(ethylene, naphthalene-2,6-dicarboxylate)
    Nogales, A
    Denchev, Z
    Sics, I
    Ezquerra, TA
    MACROMOLECULES, 2000, 33 (25) : 9367 - 9375
  • [32] EXCIMER FLUORESCENCE OF POLY(POLYOXYTETRAMETHYLENE-GLYCOL NAPHTHALENE-2,6-DICARBOXYLATE)
    CAO, T
    ZHANG, XK
    QIAN, RY
    POLYMER JOURNAL, 1989, 21 (06) : 489 - 497
  • [33] The electret properties of poly(ethylene naphthalene-2, 6-dicarboxylate) (PEN)
    Qiu, XL
    Xia, ZF
    Wang, FP
    An, ZL
    12TH INTERNATIONAL SYMPOSIUM ON ELECTRETS (ISE 12), PROCEEDINGS, 2005, : 227 - 230
  • [34] Tie molecules, morphology and confinement effects in semi - crystalline poly(ethylene naphthalene-2,6-dicarboxylate) (PEN)
    Nikaj, E.
    Royaud, I.
    David, L.
    7TH EEIGM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS RESEARCH, 2013, 48
  • [35] Transesterification in mixtures of poly(ethylene terephthalate) and poly(ethylene naphthalene-2,6-dicarboxylate): An NMR study of kinetics and end group effects
    Collins, S
    Kenwright, AM
    Pawson, C
    Peace, SK
    Richards, RW
    MacDonald, WA
    Mills, P
    MACROMOLECULES, 2000, 33 (08) : 2974 - 2980
  • [36] Sodium Naphthalene-2,6-dicarboxylate: An Anode for Sodium Batteries
    Cabanero, Joel M., Jr.
    Pimenta, Vanessa
    Cannon, Kieran C.
    Morris, Russell E.
    Armstrong, A. Robert
    CHEMSUSCHEM, 2019, 12 (19) : 4522 - 4528
  • [37] Thermo-mechanical behavior of uniaxially drawn and crystallized poly(ethylene naphthalene-2,6-dicarboxylate) (PEN) films
    Hakme, C.
    Stevenson, I.
    David, L.
    Voice, A.
    Seytre, G.
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2007, 353 (47-51) : 4252 - 4261
  • [38] Cold crystallization of poly(ethylene naphthalene-2,6-dicarboxylate) by simultaneous measurements of X-ray scattering and dielectric spectroscopy
    Sics, I
    Ezquerra, TA
    Nogales, A
    Denchev, Z
    Alvarez, C
    Funari, SS
    POLYMER, 2003, 44 (04) : 1045 - 1049
  • [39] Cyclo-depolymerisation of poly(ethylene naphthalene-2,6-dicarboxylate) and ring-opening polymerisations of the cyclic oligomers obtained
    Hodge, P
    Yang, Z
    Ben-Haida, A
    McGrail, CS
    JOURNAL OF MATERIALS CHEMISTRY, 2000, 10 (07) : 1533 - 1537
  • [40] PHYSICAL AGING IN POLY(ETHYLENE NAPHTHALENE-2,6-DICARBOXYLATE) IN RELATION TO SORBED WATER, ENTHALPIC RELAXATION, AND MECHANICAL-PROPERTIES
    RUEDA, DR
    VARKALIS, A
    VIKSNE, A
    CALLEJA, FJB
    ZACHMANN, HG
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1995, 33 (11) : 1653 - 1661