Delayed cracking in plasma nitriding of AISI 420 stainless steel

被引:23
|
作者
Tuckart, W.
Forlerer, E.
Lurmsn, L.
机构
[1] Univ Nacl Sur, Dept Engn, RA-8000 Bahia Blanca, Argentina
[2] CNEA Ctr Atom Constituyentes, Dept Mat, RA-1425 Buenos Aires, DF, Argentina
来源
SURFACE & COATINGS TECHNOLOGY | 2007年 / 202卷 / 01期
关键词
plasma nitriding; AISI; 420; delayed cracking;
D O I
10.1016/j.surfcoat.2007.04.107
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The phenomenon of delayed cracking in nitrided layers after DC-plasma nitriding of AIR 420 steel has been observed by optical microscopy. Prior to the plasma treatment, the samples were austenitized at 1303 K for 30 min and then oil quenched. Two tempering conditions were assessed: one group was tempered at 673 K, while another group was tempered at 943 K. All samples were subjected to sputtering, in the plasma chamber, to remove the passive oxide layer, under a 1:1 Ar/H(2) atmosphere. Finally, specimens were plasma nitrided at 673 K for 20 h, with a 1/3: N(2)/H(2) relation, at a pressure of 6.5 hPa and 700 V bias in the nitriding chamber. The nitrided layers were analyzed initially by X-ray diffraction (XRD). Detailed observations were conducted at frequent and regular intervals under optical microscopy (OM) and scanning electron microscopy (SEM) with secondary and back-scattered electrons detectors. The results revealed that after an incubation time, even without any external disturbance, cracks are formed and propagate in the nitrided layers. Both groups of samples were equally affected. The presence of precipitated particles and local residual stresses are possible causes of such a phenomenon. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:199 / 202
页数:4
相关论文
共 50 条
  • [41] Plasma nitriding of AISI 304 austenitic stainless steel with pre-shot peening
    Shen, Lie
    Wang, Liang
    Wang, Yizuo
    Wang, Chunhua
    SURFACE & COATINGS TECHNOLOGY, 2010, 204 (20): : 3222 - 3227
  • [42] Effect of Plasma Nitriding Surface Modification on the Adhesion of Food Pathogens to Stainless Steel AISI 316 and AISI 304
    Casarin, Leticia Sopena
    Casarin, Fabricio de Oliveira
    Soares, Tatiana Pacheco
    Aguzzoli, Cesar
    Figueroa, Carlos Alejandro
    Soares, Gabriel Vieira
    Brandelli, Adriano
    Tondo, Eduardo Cesar
    JOURNAL OF FOOD SAFETY, 2016, 36 (03) : 341 - 347
  • [43] Corrosion behaviour of dissimilar TIG welded austenitic stainless steel AISI 304 and martensitic stainless steel AISI 420
    Ghosh, Abhishek
    Pal, Pradip Kumar
    INDIAN JOURNAL OF ENGINEERING AND MATERIALS SCIENCES, 2020, 27 (03) : 665 - 669
  • [44] AISI 420 martensitic stainless steel low-temperature plasma assisted carburizing kinetics
    Scheuer, C. J.
    Cardoso, R. P.
    Mafra, M.
    Brunatto, S. F.
    SURFACE & COATINGS TECHNOLOGY, 2013, 214 : 30 - 37
  • [45] Effect of bias plasma on active screen nitrocarburising response of AISI 420 martensitic stainless steel
    Schramm, Alexander
    Jafarpour, Saeed M.
    Schimpf, Christian
    Biermann, Horst
    Dalke, Anke
    VACUUM, 2022, 205
  • [46] The purification of AISI 420 stainless steel in laser solid forming
    Song, Menghua
    Lin, Xin
    Liu, Fenggang
    Yang, Haiou
    Huang, Weidong
    MATERIALS & DESIGN, 2016, 89 : 1035 - 1040
  • [47] Sliding behaviour of ion nitrided AISI 420 stainless steel
    Tuckart, W
    Insausti, J
    Forlerer, E
    Iurman, L
    SURFACE ENGINEERING, 2005, 21 (5-6) : 463 - 468
  • [48] A survey on the passivity of tempered AISI 420 martensitic stainless steel
    Morshed-Behbahani, Khashayar
    Zakerin, Nika
    Najafisayar, Pooria
    Pakshir, Mahmoud
    Corrosion Science, 2021, 183
  • [49] Effect of bias plasma on active screen nitrocarburising response of AISI 420 martensitic stainless steel
    Schramm, Alexander
    Jafarpour, Saeed M.
    Schimpf, Christian
    Biermann, Horst
    Dalke, Anke
    VACUUM, 2022, 205
  • [50] Low-pressure arc plasma-assisted nitriding of AISI 304 stainless steel
    Zhao, Yanhui
    Yu, Baohai
    Dong, Limin
    Du, Hao
    Xiao, Jinquan
    SURFACE & COATINGS TECHNOLOGY, 2012, 210 : 90 - 96