Comparing the local-global deformation mechanism in different friction stir welding sequences of Ti-4Al-0.005B titanium alloy T-joints

被引:15
|
作者
Su, Yu [1 ,2 ]
Li, Wenya [1 ]
Shen, Junjun [2 ]
Fu, Banglong [2 ]
dos Santos, Jorge F. [2 ]
Klusemann, Benjamin [2 ,3 ]
Vairis, Achilles [4 ]
机构
[1] Northwestern Polytech Univ, Sch Mat Sci & Engn, State Key Lab Solidificat Proc, Shaanxi Key Lab Frict Welding Technol, Xian 710072, Shaanxi, Peoples R China
[2] Helmholtz Zentrum Hereon, Solid State Mat Proc, Inst Mat Mech, D-21502 Geesthacht, Germany
[3] Leuphana Univ Luneburg, Inst Prod & Proc Innovat, D-21335 Luneburg, Germany
[4] Hellen Mediterranean Univ, Mech Engn Dept, Iraklion 71004, Crete, Greece
关键词
Titanium alloy T-joint; Friction stir welding; Deformation mechanism; Microstructure; Tensile strength; Strain hardening rate; STRAIN-HARDENING BEHAVIOR; GRAIN-SIZE; MICROSTRUCTURE; TEXTURE; FATIGUE;
D O I
10.1016/j.msea.2021.141698
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Titanium alloy T-joints were produced using two different friction stir welding (FSW) sequences, and the localglobal deformation mechanisms until fracture were compared. Due to their differing FSW sequence characteristics, the optimal parameter ranges for the two T-joints are different. The stir zone (SZ) of the single-weld T-joint consists of lamellar alpha grains, while fine equiaxed alpha grains develop in the double-weld T-joint due to the selection of low heat input. Due to the different local microstructure zones in the joint, deformation inhomogeneity of the T-joint during tensile testing is observed. Independent of the welding sequence and for optimal process conditions, both T-joint configuration show nearly the same maximum tensile strength as the base material (BM), however at a relatively low fracture strain, below 20% of the BM. The local strain hardening rate in different zones of the T-joint was investigated. The strain hardening ability of SZ with fine grains is significantly higher than elsewhere, because the grain size contributes greatly to strain hardening behavior at low strain levels. The single-weld T-joint experienced a symmetric local strain distribution between advancing and retreating side. For the double-weld T-joint, there are significant differences between the first and the second weld area. The fracture morphologies of both T-joints are typical ductile, where the toughness of the single-weld joint is higher than that of the double-weld joint.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Low-temperature superplastic deformation mechanism of ultra-fine grain Ti-6Al-4V alloy by friction stir processing
    Qiang, Fei
    Xin, Shewei
    Tu, Xingyang
    Wang, Huan
    Guo, Ping
    Hou, Hongmiao
    Lian, Zhiwei
    Zhang, Lei
    Hou, Wentao
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 7413 - 7419
  • [42] Effect of 0.3 wt% hydrogen addition on the friction stir welding characteristics of Ti-6Al-4V alloy and mechanism of hydrogen-induced effect
    Zhou, L.
    Liu, H. J.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2010, 35 (16) : 8733 - 8741
  • [43] Relationships between microhardness, microstructure, and grain orientation in laser -welded joints with different welding speeds for Ti6Al4V titanium alloy
    Xu, Zhen-zhen
    Dong, Zhi-qiang
    Yu, Zhao-hui
    Wang, Wen-ke
    Zhang, Jian-xun
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2020, 30 (05) : 1277 - 1289
  • [44] Influence of axial load on structure and strength of a heterogeneous joint of titanium alloy Ti-6Al-4V and aluminum alloy Al-6Zn-2Mg-2Cu formed by friction stir welding
    Amirov, A. I.
    Chumaevskii, A. V.
    Sidorov, E. A.
    Savchenko, N. L.
    Kolubaev, E. A.
    RUSSIAN PHYSICS JOURNAL, 2024, 67 (12) : 2198 - 2205
  • [45] Prediction of properties of friction stir spot welded joints of AA7075-T651/Ti-6Al-4V alloy using machine learning algorithms
    Asmael, Mohammed
    Nasir, Tauqir
    Zeeshan, Qasim
    Safaei, Babak
    Kalaf, Omer
    Motallebzadeh, Amir
    Hussain, Ghulam
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2022, 22 (02)
  • [46] Influence of Heat Input on Welding Processes, Weld Formation, Microstructure, and Mechanical Properties of Double-Sided Laser Beam Welded Ti-6Al-4V Alloy T-Joints
    Ma Xuyi
    Duan Aiqin
    Lu Wei
    Wang Xuedong
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (07) : 2300 - 2307
  • [47] Influence of Heat Input on Welding Processes, Weld Formation, Microstructure, and Mechanical Properties of Double- Sided Laser Beam Welded Ti-6Al-4V Alloy T-Joints
    Ma, Xuyi
    Duan, Aiqin
    Lu, Wei
    Wang, Xuedong
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (07): : 2300 - 2307
  • [48] Achieving superior mechanical and corrosion properties in medium-thickness Ti-6Al-4 V alloy joints by back heating assisted friction stir welding below β-phase transformation temperature
    Cong, S.
    Wu, L. H.
    Wang, Z. W.
    Li, N.
    Zhu, Z.
    Wang, F. F.
    Zhang, X.
    Wang, K.
    Xue, P.
    Ni, D. R.
    Xiao, B. L.
    Ma, Z. Y.
    MATERIALS CHARACTERIZATION, 2024, 217
  • [49] Interfacial layer regulation and its effect on mechanical properties of Ti6Al4V titanium alloy and T2 copper dissimilar joints by cold metal transfer welding
    Huang, Libing
    Dong, Honggang
    Ma, Yueting
    Li, Peng
    Wang, Jiawei
    Yang, Jiang
    Wu, Baosheng
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 75 : 1100 - 1110
  • [50] Deep Understanding of the Influence of the Process Parameters During Linear Friction Welding on the Joint Quality and the Microstructural Changes of Two Mono-Material Titanium Alloy Joints: The β-Metastable Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) and the Near-α Ti-6Al-2Sn-4Zr-2Mo (Ti6242)
    Ballat-Durand, Dorick
    Bouvier, Salima
    Risbet, Marion
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2020, 51 (01): : 263 - 278