Residual lifetime assessment of thermal power plant superheater header

被引:8
|
作者
Yasniy, O. [1 ]
Pyndus, Yu. [1 ]
Iasnii, V. [1 ]
Lapusta, Y. [2 ]
机构
[1] Ternopil Ivan Puluj Natl Tech Univ, Ruska 56, UA-46001 Ternopol, Ukraine
[2] Clermont Univ, UMR UBP CNRS IFMA 6602, Inst Pascal, BP 265, F-63175 Aubiere, France
关键词
Stress intensity factors; Finite element analysis; Fatigue crack growth; Life assessment; Fatigue; COLLECTOR; STEEL;
D O I
10.1016/j.engfailanal.2017.07.028
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The safe operation of thermal power plants (TPPs) is largely determined by the reliability of main components of steam systems of power units, to which belong the headers of boiler superheaters. The aim of this study is to estimate the residual lifetime of superheater header starting from the initial defect size and up to the maximum allowable one. The above-mentioned lifetime is affected by the fluctuations of temperature under steady mode of operation of TPP superheater header. Superheaters headers operate in a steamy environment under the pressure of 15.5 MPa at temperature of 545 degrees C. The header is a thick-walled cylinder made of 12Cr1MoV steel with a length of 2314 mm, outer diameter of 325 mm and thickness of 50 mm. To estimate the residual lifetime of the header, the steam temperature in header was measured and digitized. The temperature range of the header under quasi-stable operational mode was divided into three classes: (1) Delta t < 10 degrees C; (2) 10 degrees C < Delta t < 30 degrees C; (3) Delta t > 30 degrees C. The local minima and maxima were determined based on the obtained steam temperature history. The residual durability was evaluated taking into account the effect of thermo-mechanical stresses and also the stresses caused by internal steam pressure. The stress intensity factors (SIFs) at the crack tip in the ligament between the holes of superheater collector were estimated by FEM. The SIF of mode I (K-I) were determined along the fronts of modelled semi-elliptical cracks. The SIF correction function at the midpoint of the semi-elliptical crack front in the ligament between holes of the superheater header versus the crack depth and the temperature difference between the external and internal surfaces under a constant internal pressure of steam was obtained. Based on the analysis of header defects, the proposed front shape was taken in the form of the semi-ellipse. The crack growth at 500 degrees C was modelled by Paris and NASGRO equations. With the increase of temperature difference between the external and internal header surfaces from 10 degrees C to 50 degrees C, the number of cycles, that is necessary for the crack to reach 35 mm in depth, decreases approximately in 25 times. It was calculated, that the average value of temperature fluctuations is 15 degrees C for the Class 1, and is 46.2 degrees C for the Class 2. The lifetime of header can be extended due to the decrease of fluctuations of temperature range and their frequency.
引用
收藏
页码:390 / 403
页数:14
相关论文
共 50 条
  • [41] Life assessment of tertiary superheater tube in a thermal powerplant
    Sudasna, C
    Tareelap, N
    Poolthong, N
    Tongsri, R
    Loha, V
    Srisukhumbowornchai, N
    Thavarungkul, N
    HIGH TEMPERATURE CORROSION AND MATERIALS CHEMISTRY IV, 2003, 2003 (16): : 264 - 277
  • [42] Residual lifetime assessment of cold-reheater pipe in coal-fired power plant through accelerated degradation test
    Kim, Myung-Yeon
    Chu, Dong-Ju
    Lee, Young-Kook
    Shim, Jae-Hyeok
    Jung, Woo-Sang
    RELIABILITY ENGINEERING & SYSTEM SAFETY, 2019, 188 : 330 - 335
  • [43] Root Cause Analysis of Failure in Superheater Tubes in a Power Plant
    A. Bahrami
    S. M. Rafiaei
    M. Yazdan Mehr
    Metallography, Microstructure, and Analysis, 2019, 8 : 275 - 280
  • [44] Power Generation and Superheater Upgrade Project at the Burnaby MSW Plant
    Montenay Inc., 5150 Riverbend Drive, Burnaby
    BC
    V3N 4V3, Canada
    不详
    WA
    98034, United States
    North Am. Waste-to-Energy Conf., NAWTEC, 1600, (23-31):
  • [45] A STUDY ON BURST ACCIDENT OF SUPERHEATER TUBE IN A BIOMASS POWER PLANT
    Li, Yuchun
    Zhang, Hongliang
    He, Yuwu
    Lin, Musong
    INTERNATIONAL JOURNAL OF POWER AND ENERGY SYSTEMS, 2015, 35 (03): : 120 - 126
  • [46] A case study on failure of superheater tubes in an industrial power plant
    Dehnavi, F.
    Eslami, A.
    Ashrafizadeh, F.
    ENGINEERING FAILURE ANALYSIS, 2017, 80 : 368 - 377
  • [47] Reducing superheater corrosion in wood-fired power plant
    Henderson, PJ
    Andersson, C
    Kassman, H
    Högberg, J
    BALTICA VI: LIFE MANAGEMENT AND MAINTENANCE FOR POWER PLANTS, VOL 1 AND 2, 2004, 233-234 : 143 - 154
  • [48] Root Cause Analysis of Failure in Superheater Tubes in a Power Plant
    Bahrami, A.
    Rafiaei, S. M.
    Mehr, M. Yazdan
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2019, 8 (02) : 275 - 280
  • [49] Power generation and superheater upgrade project at the Burnaby MSW plant
    Lakowski, L
    Anderson, R
    Richter, R
    Berz, MD
    Britt, ML
    La Fond, JF
    NAWTEC11: PROCEEDINGS OF THE 11TH ANNUAL NORTH AMERICAN WASTE TO ENERGY CONFERENCE, 2003, : 23 - 31
  • [50] Failure Analysis of Superheater Tubes Cracking of a Boiler in a Power Plant
    Sun, Zhiwei
    Fan, Yuling
    Xu, Shugen
    Song, Mingda
    Zhang, Yuan
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2018, 7 (01) : 92 - 100