Effect of Fe additions on microstructure and mechanical properties of a multi-component Nb-16Si-22Ti-2Hf-2Al-2Cr alloy at room and high temperatures

被引:29
|
作者
Zhang, S. M. [1 ]
Zhou, J. R. [1 ]
Sha, J. B. [1 ]
机构
[1] Beihang Univ, Sch Mat Sci & Engn, Beijing 100191, Peoples R China
基金
中国国家自然科学基金;
关键词
Intermetallics; (aluminides; silicides); Fracture toughness; Mechanical properties; Casting; Heat treatment; Microstructure; IN-SITU COMPOSITES; SILICIDE-BASED COMPOSITES; FRACTURE-TOUGHNESS; STRENGTH; TI; ENGINES;
D O I
10.1016/j.intermet.2014.10.013
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The phase constitutions, microstructural evolutions, and mechanical properties of Nb-16Si-22Ti-2Hf-2Al-2Cr-xFe alloys (where x = 1, 2, 4, 6 at.%, hereafter referred to as 1Fe, 2Fe, 4Fe and 6Fe alloys, respectively) prepared by arc-melting were investigated. It was observed that the nominal Fe content affected the solidification path of the multi-component alloy. The as-cast 1Fe alloy primarily consisted of a dendritic-like Nb-SS phase and (alpha+gamma)-Nb5Si3 silicide, and the as-cast 2Fe and 4Fe alloys primarily consisted of an Nb-SS phase, (alpha+gamma)-Nb5Si3 silicide and (Fe + Ti)-rich region. In addition to the Nb-SS phase, a multi-component Nb4FeSi silicide was present in the as-cast 6Fe alloy. When heat-treated at 1350 C for 100 h, the 1Fe and 6Fe alloys almost exhibited the same microstructures as the corresponding as-cast samples; for the 2Fe and 4Fe alloys, the (Fe + Ti)-rich region decomposed, and Nb4FeSi silicide formed. The fracture toughness of the as-cast and heat-treated Nb-16Si-22Ti-2Hf-2Al-2Cr-xFe samples monolithically decreased with the nominal Fe contents. It is interesting that at room temperature, the strength of the heat-treated samples was improved by the Fe additions, whereas at 1250 degrees C and above, the strength decreased, suggesting the weakening role of the Nb4FeSi silicide on the high-temperature strength. As the nominal Fe content increased from 1 at% to 6 at.%, for example, the 0.2% yield strength increased from 1675 MPa to 1820 MPa at room temperature; also, the strength decreased from 183 MPa to 78 MPa at 1350 degrees C. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:146 / 155
页数:10
相关论文
共 50 条
  • [31] The microstructure evolution of directionally solidified Nb-22Ti-14Si-4Cr-2Al-2Hf alloy during heat treatment
    Yuan Sainan
    Jia Lina
    Su Linfen
    Ma Limin
    Zhang Hu
    INTERMETALLICS, 2013, 38 : 102 - 106
  • [32] Effect of multi-stage heat treatment on mechanical properties and microstructure transformation of Ti-48Al-2Cr-2Nb alloy
    Yim, Seungkyun
    Bian, Huakang
    Aoyagi, Kenta
    Chiba, Akihiko
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 816
  • [33] Effect of chemical composition and heat treatment on microstructure and mechanical properties of Nb-xTi-16Si-3Cr-3Al-2Hf-yZr alloy
    Kang, Yongwang
    Guo, Fengwei
    Li, Ming
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 760 : 118 - 124
  • [34] Effect of Cr Additions on Toughness, Strength, and Oxidation Resistance of an Nb-4Si-20Ti-6Hf Alloy at Room and/or High Temperatures
    Jiangbo Sha
    Jun Liu
    Chungen Zhou
    Metallurgical and Materials Transactions A, 2011, 42 : 1534 - 1543
  • [35] Effect of Cr Additions on Toughness, Strength, and Oxidation Resistance of an Nb-4Si-20Ti-6Hf Alloy at Room and/or High Temperatures
    Sha, Jiangbo
    Liu, Jun
    Zhou, Chungen
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (06): : 1534 - 1543
  • [36] Effect of N addition on microstructure and high temperature mechanical properties of Ti-48Al-2Cr-2Nb (at. %) intermetallic alloy
    Ghorbani, Hamid Reza
    Kermanpur, Ahmad
    Rezaeian, Ahmad
    Siahboumi, Abbas Ahmadi
    Taebi, Mohammad Ali
    MATERIALS TODAY COMMUNICATIONS, 2020, 25 (25):
  • [37] Microstructure Evolution and Mechanical Properties of a Directionally Solidified Nb-Ti-Si-Cr-Al-Hf-Dy Alloy
    Sheng, Liyuan
    INTERNATIONAL SYMPOSIUM ON MATERIALS APPLICATION AND ENGINEERING (SMAE 2016), 2016, 67
  • [38] Microstructure evolution and room temperature deformation of a unidirectionally solidified Nb-22Ti-16Si-3Ta-2Hf-7Cr-3Al-0.2Ho (at.%) alloy
    Cheng, G. M.
    He, L. L.
    INTERMETALLICS, 2011, 19 (02) : 196 - 201
  • [39] Nb-16Si-22Ti-2Cr-2Al-2Hf-xFe合金热加工性能研究
    褚楚
    徐严谨
    侯红亮
    骆良顺
    苏彦庆
    郭景杰
    傅恒志
    稀有金属材料与工程, 2019, 48 (05) : 1481 - 1487
  • [40] Effect of nitrogen addition and aging treatment on microstructure and high temperature mechanical properties of Ti-48Al-2Cr-2Nb (at%) intermetallic alloy
    Ghorbani, Hamid Reza
    Kermanpur, Ahmad
    Rezaeian, Ahmad
    Sadeghi, Fazlollah
    Siahboumi, Abbas Ahmadi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 904