Corrosion and cavitation erosion resistance enhancement of cast Ni-Al bronze by laser surface melting

被引:37
|
作者
Song, Q. N. [1 ,2 ]
Tong, Y. [2 ]
Li, H. L. [2 ]
Zhang, H. N. [2 ]
Xu, N. [2 ]
Zhang, G. Y. [2 ]
Bao, Y. F. [2 ]
Liu, W. [3 ]
Liu, Z. G. [3 ]
Qiao, Y. X. [3 ]
机构
[1] Hohai Univ, Engn Res Ctr Dredging Technol, Minist Educ, Changzhou 213022, Jiangsu, Peoples R China
[2] Hohai Univ, Coll Mech & Elect Engn, Changzhou 213022, Jiangsu, Peoples R China
[3] Jiangsu Univ Sci & Technol, Coll Mat Sci & Engn, Zhenjiang 212003, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Laser surface melting; Ni-Al bronze; Microstructure; Corrosion; Cavitation erosion; Synergy; NICKEL-ALUMINUM-BRONZE; MECHANICAL-PROPERTIES; AS-CAST; BEHAVIOR; COPPER; ALLOYS; MICROSTRUCTURE; SEAWATER; LAYER; NAB;
D O I
10.1007/s42243-021-00674-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Laser surface melting (LSM) was applied on a cast Ni-Al bronze (NAB), which was a crucial material for marine ship propellers. A 720 mu m-thick LSM layer with fine equiaxed and dendritic microstructures was obtained. After immersion for 30 days, the corrosion rate of cast NAB was reduced by 25% after LSM. Preferential corrosion occurred and deep corrosion pits appeared at alpha + kappa(III) microstructure for the cast NAB. LSM NAB underwent general corrosion, and a much more protective film formed on the surface because of the homogenized microstructure. The mass loss of the cast NAB was approximately 2.1 times larger than that of LSM NAB after cavitation erosion (CE) in 3.5 wt.% NaCl solution for 5 h. For the two materials, the mechanical impact effect was dominantly responsible for CE damage. Therefore, the improved hardness and homogenized microstructure contributed to the improved CE resistance of LSM NAB. CE destructed the film, shifted the open circuit potential toward a more negative value, and raised the current density by an order of magnitude. Corrosion at the cast eutectoid microstructure and the dendrites of LSM NAB facilitates the degradation under the cavitation attack. CE-corrosion synergy was largely caused by corrosion-enhanced-CE.
引用
收藏
页码:359 / 369
页数:11
相关论文
共 50 条
  • [21] Improvement in cavitation erosion resistance of a copper-based propeller alloy by laser surface melting
    Tang, CH
    Cheng, FT
    Man, HC
    SURFACE & COATINGS TECHNOLOGY, 2004, 182 (2-3): : 300 - 307
  • [22] CAVITATION EROSION OF LASER-SURFACE-MELTED SELF-QUENCHED FE-AL BRONZE
    CRISCI, RJ
    DRAPER, CW
    PREECE, CM
    APPLIED OPTICS, 1982, 21 (10): : 1730 - 1731
  • [24] On cavitation erosion behavior of friction stir processed surface of cast nickel aluminium bronze
    Thapliyal, Shivraman
    Dwivedi, Dheerendra Kumar
    WEAR, 2017, 376 : 1030 - 1042
  • [25] LASER CLADDING OF NI-AL BRONZE ON AL-ALLOY AA333
    LIU, Y
    MAZUMDER, J
    SHIBATA, K
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1994, 25 (05): : 749 - 759
  • [26] Corrosion behavior of wire-arc additive manufactured and as-cast Ni-Al bronze in 3.5 wt% NaCl solution
    Xu, Cheng
    Peng, Yong
    Chen, Liang-Yu
    Zhang, Tian-Yang
    He, Shen
    Wang, Ke-Hong
    CORROSION SCIENCE, 2023, 215
  • [27] Friction stir processing of a cast manganese-aluminum bronze for improving corrosion and cavitation erosion resistances
    Song, Q. N.
    Tong, Y.
    Li, H. L.
    Xu, N.
    Xu, C. B.
    Bao, Y. F.
    Yin, L.
    Qiao, Y. X.
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2020, 8 (02):
  • [28] Effect of a Uniform Magnetic Field on Corrosion of Ni-Al Bronze in 3.5 wt% NaCl
    Krogstad, Hedda Nordby
    Johnsen, Roy
    Coey, Michael
    CORROSION, 2018, 74 (02) : 197 - 209
  • [30] Effects of Surface Modifications on Rotating Bending Fatigue of Ni-Al Bronze Alloy
    Lu, Guan-Xun
    Chen, Tai-Cheng
    Shiue, Ren-Kae
    Tsay, Leu-Wen
    METALS, 2025, 15 (01)