Effect of pH on Hydrothermal Synthesis of ZrO2 Nanoparticles and their Electrocatalytic Activity for Hydrogen Production

被引:12
|
作者
Mohsen, Q. [1 ]
Al-Gethami, Wael S. [1 ]
Zaki, Z. [1 ]
Alotaibi, S. H. [1 ]
Ibrahim, Mohamed M. [1 ]
Ezzat, Mohamed [1 ]
Amin, Mohammed A. [1 ]
Kamel, M. M. [2 ]
Mostafa, Nasser Y. [2 ]
机构
[1] Taif Univ, Fac Sci, Dept Chem, Mat & Corros Grp, Taif, Saudi Arabia
[2] Suez Canal Univ, Dept Chem, Fac Sci, Ismailia 41522, Egypt
来源
关键词
Zirconia; hydrothermal; monoclinic; tetragonal; hydrogen production; ZIRCONIA; SURFACE;
D O I
10.20964/2022.07.24
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Electrolytic hydrogen production needs heavy-duty electrocatalyst to lower the overpotential to economical values. With this respect, we scrutinized the effect of pH on the phase formation, microstructure and hydrogen production activity of ZrO2 generated under hydrothermal processing. At both low and high pHs (2.61 and 14) the products are single phase monoclinic ZrO2. However, at intermediate pHs (7.0-11.0), the produces are biphasic mixture of tetragonal and monoclinic nano crystallites. The particles size slightly increases (from 11 to 14 nm) with increasing the pH up to 11. However, at pH=14.0, the particle size abruptly increases to 98 nm. The vibration spectra demonstrated that monoclinic ZrO2 comprise intense surface hydroxyl functional groups, that enhance the electrocatalytic activity of ZrO2 nanoparticles. Thus, the hydrogen evolution activity increases with increasing the monoclinic phase contents. Zr02 produced at low pH (2.61) showed the highest electrocatalytic activity.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Continuous Hydrothermal Flow Synthesis and Characterization of ZrO2 Nanoparticles Doped with CeO2 in Supercritical Water
    Li, Qingyun
    Liu, Lingyu
    Wang, Zihua
    Wang, Xuezhong
    NANOMATERIALS, 2022, 12 (04)
  • [32] Effects of ZrO2 addition on phase stability and photocatalytic activity of ZrO2/TiO2 nanoparticles
    Kim, Ji-Young
    Kim, Chan-Soo
    Chang, Han-Kwon
    Kim, Tae-Oh
    ADVANCED POWDER TECHNOLOGY, 2010, 21 (02) : 141 - 144
  • [33] HYDROTHERMAL PRECIPITATION OF ZRO2 POWDER
    SOMIYA, S
    KUMAKI, T
    HISHINUMA, K
    NAKAI, Z
    AKIBA, T
    SUWA, Y
    PROGRESS IN CRYSTAL GROWTH AND CHARACTERIZATION OF MATERIALS, 1991, 21 : 195 - 198
  • [34] The effect of oxide cracks on hydrogen ingress in ZrO2
    Li, H. -L.
    Wen, Q.
    Szpunar, J.
    DIFFUSION AND THERMODYNAMICS OF MATERIALS, 2007, 263 : 117 - +
  • [35] Synthesis of Elusive Monoclinic ZrO2 Nanostructures via Hydrothermal Treatment
    Sakshi Thakur
    Shweta Sareen
    Meenakshi Verma
    Kirtanjot Kaur
    Vishal Mutreja
    Journal of Inorganic and Organometallic Polymers and Materials, 2024, 34 : 61 - 78
  • [36] Synthesis of Elusive Monoclinic ZrO2 Nanostructures via Hydrothermal Treatment
    Thakur, Sakshi
    Sareen, Shweta
    Verma, Meenakshi
    Kaur, Kirtanjot
    Mutreja, Vishal
    JOURNAL OF INORGANIC AND ORGANOMETALLIC POLYMERS AND MATERIALS, 2024, 34 (01) : 61 - 78
  • [37] Reflux synthesis and hydrothermal processing of ZrO2 nanopowders at low temperature
    Matos, J. M. E.
    Anjos Junior, F. M.
    Cavalcante, L. S.
    Santos, V.
    Leal, S. H.
    Santos Junior, L. S.
    Santos, M. R. M. C.
    Longo, E.
    MATERIALS CHEMISTRY AND PHYSICS, 2009, 117 (2-3) : 455 - 459
  • [38] Remarkable catalytic effect of Ni and ZrO2 nanoparticles on the hydrogen sorption properties of MgH2
    Tome, Kudzaishe Caren
    Xi, Senliang
    Fu, Yuanyi
    Lu, Chang
    Lu, Ni
    Guan, Meili
    Zhou, Shixue
    Yu, Hao
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (07) : 4716 - 4724
  • [39] Synthesis of ZrO2 and TiO2 nanocrystalline powders by hydrothermal process
    Kolen'ko, YV
    Maximov, VD
    Burukhin, AA
    Muhanov, VA
    Churagulov, BR
    MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2003, 23 (6-8): : 1033 - 1038
  • [40] The effect of ZrO2 nanoparticles on TiO2-Al-C combustion synthesis system
    Dong, Q
    Tang, Q
    Li, WC
    Wu, DY
    MATERIALS LETTERS, 2002, 55 (04) : 259 - 264