Cyclic voltammetry study of ice formation in the PEFC catalyst layer during cold start

被引:61
|
作者
Ge, Shanhai
Wang, Chao-Yang [1 ]
机构
[1] Penn State Univ, Electrochem Engine Ctr, University Pk, PA 16802 USA
[2] Penn State Univ, Dept Mech & Nucl Engn, University Pk, PA 16802 USA
关键词
D O I
10.1149/1.2784166
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
electrochemically active Pt area during and post-subzero startup of a polymer electrolyte fuel cell (PEFC). It was found that the Pt area decreases after each cold start and the Pt area loss increases with the product water generated during cold start. We hypothesize that the Pt area loss is caused by ice precipitated between Pt particles and ionomers during cold start. After startup from a subzero temperature and warmup to 25 degrees C with all ice in the CL melted, the cell remains subject to Pt area loss, but this loss at 25 degrees C is substantially reduced. We also find that subsequent cell operation at 70 degrees C and 1 A/cm(2) for 2 h is very effective for recovering the active Pt area and cell performance. Both permanent loss in the active Pt area and cell performance degradation due to structural alteration of the cathode CL by the presence of ice increase gradually with the cold-start cycle number and become more severe for cold start from -30 degrees C than from -10 and -20 degrees C. In addition, startup from a subzero temperature appears to have no influence on the electrochemically active Pt area of the anode CL. It is suggested that the ice amount present in the CL holds a key to determine the temporary Pt area loss due to ice formation as well as permanent performance degradation resulting from cold-start cycling. (c) 2007 The Electrochemical Society.
引用
收藏
页码:B1399 / B1406
页数:8
相关论文
共 50 条
  • [21] Cold start capability and durability of electrospun catalyst layer for proton exchange membrane fuel cell
    Liu, Han
    Si, Dechun
    Ding, Han
    Wang, Shangshang
    Zhang, Jianbo
    Liu, Yong
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (19) : 11140 - 11149
  • [22] Effect of the pore structure of cathode catalyst layer on the PEM fuel cell cold start process
    Zang, Linfeng
    Hao, Liang
    Zhu, Xiaojing
    ENERGY, 2023, 271
  • [23] Ice Formation Processes in PEM Fuel Cell Catalyst Layers during Cold Startup Analyzed by Cryo-SEM
    Tabe, Yutaka
    Yamada, Kazuki
    Ichikawa, Ryosuke
    Aoyama, Yusuke
    Suzuki, Kengo
    Chikahisa, Takemi
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2016, 163 (10) : F1139 - F1145
  • [24] Study on Oxidation Resistance of Copper Plate with Organic Thin Layer by Cyclic Voltammetry
    Takagi, Juri
    Ikeda, Takuya
    Adachi, Kaoru
    Tsukahara, Yasuhisa
    KOBUNSHI RONBUNSHU, 2016, 73 (03) : 294 - 301
  • [25] Multi-objective optimization of ice distribution uniformity and startup failure time for cold start of PEMFC catalyst layer based on CTnet and PSO-GA
    Liu, Zhuwei
    Mao, Xuping
    Kang, Zehao
    Huang, Yin
    Zhang, Zhi
    Xuan, Dongji
    FUEL, 2024, 363
  • [26] Simulation modeling of the process of ice formation during the movement of a vessel in a layer of grated ice
    Ionov, Boris P.
    Pogodin, Evgeniy V.
    Sandakov, Mihail Y.
    MARINE INTELLECTUAL TECHNOLOGIES, 2023, (04): : 39 - 44
  • [27] Research of hydrate and ice formation in soils during cyclic fluctuations of temperature
    Chuvilin, EM
    Perlova, EV
    Makhonina, NA
    Yakushev, VS
    GROUND FREEZING 2000: FROST ACTION IN SOILS, 2000, : 9 - 14
  • [28] Effect of catalyst layer mesoscopic pore-morphology on cold start process of PEM fuel cells
    Ahmed Mohmed Dafalla
    Fangming Jiang
    Frontiers in Energy, 2021, 15 : 460 - 472
  • [29] Effect of catalyst layer mesoscopic pore-morphology on cold start process of PEM fuel cells
    Dafalla, Ahmed Mohmed
    Jiang, Fangming
    FRONTIERS IN ENERGY, 2021, 15 (02) : 460 - 472
  • [30] Effect of catalyst layer mesoscopic pore-morphology on cold start process of PEM fuel cells
    Ahmed Mohmed DAFALLA
    Fangming JIANG
    Frontiers in Energy, 2021, (02) : 460 - 472