Hot corrosion studies on fully austenitic stainless steel in air oxidation and simulated waste heat incinerator environment at 600 °C, 650 °C and 700 °C

被引:7
|
作者
Roshith, P. [1 ]
Arivarasu, M. [2 ]
机构
[1] Vellore Inst Technol, Sch Mech Engn, Vellore, Tamil Nadu, India
[2] Vellore Inst Technol, Ctr Innovat Mfg Res, Vellore, Tamil Nadu, India
关键词
hot corrosion; thermogravimetric chart; air oxidation; molten salt hot corrosion; RESISTANCE; BEHAVIOR; CHLORIDE; ALLOYS;
D O I
10.1088/2053-1591/ab61ab
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The purpose of the current study is to compare the hot corrosion performance of SMO 254 exposed to air oxidation and molten salt with a eutectic mixture of 40 wt% Na2SO4 + 40 wt% K2SO4 + 10 wt% NaCl + 10 wt% KCl at 600 degrees C, 650 degrees C and 700 degrees C under cyclic conditions for 50 h period. Kinetics of corrosion were analyzed by thermogravimetric method. By using SEM/EDS, the hot corroded specimens were investigated for surface scales and cross-sectional elemental analysis by point, line mapping methods. An accelerated rate of corrosion rate was noticed in the specimen exposed to molten salt at 700 degrees C, and the lowest rate of corrosion rate was observed in the specimen subjected to air oxidation at 600 degrees C. XRD analysis is done to analyze the corrosion products in the oxide scale.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Evolution of intergranular corrosion resistance for HR3C heat-resistant austenitic stainless steel at elevated temperature
    Du, H.
    Cheng, Y.
    Hou, L.
    Li, Y.
    Wei, Y.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2017, 52 (05) : 343 - 348
  • [32] Cyclic Oxidation of Fe–18Cr–21Mn–0.65N Austenitic Stainless Steel at 400–700 °C
    Sharvan Kumar
    G. S. Mahobia
    Transactions of the Indian Institute of Metals, 2020, 73 : 2457 - 2470
  • [33] Effect of vanadium addition on the corrosion behavior of S30432 austenitic heat-resistant steel aged at 650 °C for different times
    Youwang Tu
    Lihui Zhu
    Renyuan Zhou
    Haibo Hu
    Yingpu Huang
    Journal of Materials Science, 2022, 57 : 14096 - 14118
  • [34] Effect of vanadium addition on the corrosion behavior of S30432 austenitic heat-resistant steel aged at 650 °C for different times
    Tu, Youwang
    Zhu, Lihui
    Zhou, Renyuan
    Hu, Haibo
    Huang, Yingpu
    JOURNAL OF MATERIALS SCIENCE, 2022, 57 (29) : 14096 - 14118
  • [35] TEM studies of the oxide scales formed on type 316 stainless steel during annealing at 600 °C in a vacuum and air
    Zielinski, W
    Kurzydlowski, KJ
    SCRIPTA MATERIALIA, 2000, 43 (01) : 33 - 37
  • [36] Potentiodyanmic corrosion behavior of Fe-18Cr-21Mn-0.65 N austenitic stainless steel exposed at 400-700 °C
    Kumar, Sharvan
    Jaiswal, Dheeraj
    Behera, C. K.
    Mahobia, G. S.
    MATERIALS CHEMISTRY AND PHYSICS, 2022, 290
  • [37] Air Oxidation and Hot Corrosion Behavior of Bare and CO2 Laser-Welded Superalloy A-286 at 700 °C
    S. M. Muthu
    M. Arivarasu
    Transactions of the Indian Institute of Metals, 2019, 72 : 1607 - 1612
  • [38] Air Oxidation and Hot Corrosion Behavior of Bare and CO2 Laser-Welded Superalloy A-286 at 700°C
    Muthu, S. M.
    Arivarasu, M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (06) : 1607 - 1612
  • [39] The role of grain boundaries in the initial oxidation behavior of austenitic stainless steel containing alloyed Cu at 700 °C for advanced thermal power plant applications
    Kim, Ju-Heon
    Kim, Byung Kyu
    Kim, Dong-Ik
    Choi, Pytick-Pa
    Raabe, Dierk
    Yi, Kyung-Woo
    CORROSION SCIENCE, 2015, 96 : 52 - 66
  • [40] Effect of TiC particles on the oxidation behavior of 2Cr13 stainless steel in a simulated marine environment at 550°C
    Xu, Yang
    Wu, Qianlin
    Zheng, Haitian
    Huang, Liangjun
    Zhong, Ning
    Fan, Chunhua
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2020, 71 (08): : 1321 - 1329