The Effect of Die Spacer Thickness on Retentive Strength of all Zirconium Crowns (An In vitro Study)

被引:0
|
作者
Taha, Farah Adnan [1 ]
Ibraheem, Adel Farhan [1 ]
机构
[1] Univ Baghdad, Coll Dent, Dept Conservat Dent, Baghdad, Iraq
来源
INTERNATIONAL JOURNAL OF MEDICAL RESEARCH & HEALTH SCIENCES | 2019年 / 8卷 / 01期
关键词
Die spacer; Retention; CAD CAM; Zirconia; OXIDE CERAMIC CROWNS; CEMENT;
D O I
暂无
中图分类号
R-3 [医学研究方法]; R3 [基础医学];
学科分类号
1001 ;
摘要
Aim: The purpose of this study was to evaluate the effect of different die-spacer thicknesses on the retentive strength of all zirconium crowns using self-adhesive resin cement (Relyx Unicem). Materials and method: A total of 24 freshly extracted sound human maxillary first premolar teeth were mounted and then received a standardized preparation for full contour zirconia crown restorations with a deep chamfer finishing line, planner occlusal reduction, 6 degrees overall taper. The teeth were scanned directly using Sirona Omnicam digital intra-oral scanner. Preparations surface areas were measured using Auto CAD architecture software. Teeth were then randomly assigned into 3 main groups according to the die spacer thickness selected during the designing phase by in Lab SW 16.1 designing program (n=8): Group A: 80 mu m; Group B: 100 mu m and Group C: 120 mu m. Monolithic zirconia crowns were constructed using Sirona In-Lab MC X5 milling unit. Each group was cemented with Relyx Unicem self-adhesive luting cement. Statistical analyses: The data were statistically analyzed using 1-way ANOVA and Post-hoc Bonferroni test at 0.05 level of significance. Results: The statistical analysis showed that die spacer thickness had a significant effect on the crown retentive stress and the highest mean of retentive stresses was recorded for Group A (7.4 +/- 0.7 SD) while Group C recorded the lowest mean of retentive stresses (5.5 +/- 0.8 SD). In addition, the predominant mode of failure was type 3 (cement principally on ceramic). Conclusion: Within the limitations of this study, the use of 80 mu m spacer thickness resulted in significally higher retention values than 100 mu m and 120 mu m spacer. In contrast, there was no significant difference in retention between 100 mu m and 120 mu m.
引用
收藏
页码:22 / 27
页数:6
相关论文
共 50 条
  • [41] Effect of metal type and surface treatment on in vitro tensile strength of copings cemented to minimally retentive preparations
    Abreu, Amara
    Loza, Maria A.
    Elias, Augusto
    Mukhopadhyay, Siuli
    Rueggeberg, Frederick A.
    JOURNAL OF PROSTHETIC DENTISTRY, 2007, 98 (03): : 199 - 207
  • [42] In vitro study on marginal and internal fit of CAD/CAM all-ceramic crowns
    Nakamura, T
    Tanaka, H
    Kinuta, S
    Akao, T
    Okamoto, K
    Wakabayashi, K
    Yatani, H
    DENTAL MATERIALS JOURNAL, 2005, 24 (03) : 456 - 459
  • [43] Marginal Fit of All-Ceramic Crowns Before and After Cementation: An In Vitro Study
    Halici, Saniye Eren
    Hekimoglu, Canan
    Ersoy, Orkun
    INTERNATIONAL JOURNAL OF PERIODONTICS & RESTORATIVE DENTISTRY, 2018, 38 (03) : E41 - E48
  • [44] Impact of Gluma Desensitizer on the tensile strength of zirconia crowns bonded to dentin: an in vitro study
    Stawarczyk, Bogna
    Hartmann, Leonie
    Hartmann, Rahel
    Roos, Malgorzata
    Ender, Andreas
    Oezcan, Mutlu
    Sailer, Irena
    Haemmerle, Christoph H. F.
    CLINICAL ORAL INVESTIGATIONS, 2012, 16 (01) : 201 - 213
  • [45] Fracture Strength of Monolithic Zirconia Crowns with Modified Vertical Preparation: A Comparative In Vitro Study
    Abdulazeez, Marwah Ismael
    Majeed, Manhal A.
    EUROPEAN JOURNAL OF DENTISTRY, 2022, 16 (01) : 209 - 214
  • [46] Impact of Gluma Desensitizer on the tensile strength of zirconia crowns bonded to dentin: an in vitro study
    Bogna Stawarczyk
    Leonie Hartmann
    Rahel Hartmann
    Malgorzata Roos
    Andreas Ender
    Mutlu Özcan
    Irena Sailer
    Christoph H. F. Hämmerle
    Clinical Oral Investigations, 2012, 16 : 201 - 213
  • [47] An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain
    Webber, B
    McDonald, A
    Knowles, J
    JOURNAL OF PROSTHETIC DENTISTRY, 2003, 89 (02): : 154 - 160
  • [48] The in vitro effect of pulpal pressure and luting agent on tensile bond strength of complete cast crowns
    Ozturk, AN
    Belli, S
    Eskitascioglu, G
    JOURNAL OF PROSTHETIC DENTISTRY, 2004, 91 (03): : 253 - 257
  • [49] Comparative Evaluation of the Effect of Laser Etching on the Shear Bond Strength of Crowns Cemented with Two Different Luting Agents: An In Vitro Study
    Dahiya, Ankur
    Gandhi, Paresh
    Baba, Nadim Z.
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2017, 30 (05) : 485 - 486
  • [50] Effect of Graphene Oxide Nanoparticles on the Flexural Strength of all Ceramics- An In-vitro Study
    Yogitha, K.
    Mohamed, Kasim
    Krishnamurthy, Preetha
    JOURNAL OF CLINICAL AND DIAGNOSTIC RESEARCH, 2023, 17 (02) : ZC29 - ZC32