High Temperature Erosion-oxidation Resistance of Thermally Sprayed Nanostructured Cr3C2-25(Ni-20Cr) Coatings

被引:1
|
作者
da Cunha, Cecilio Alvares [1 ]
Correa, Olandir Vercino [1 ]
Sayeg, Isaac Jamil [2 ]
Ramanathan, Lalgudi Venkataraman [1 ]
机构
[1] CNEN SP, IPEN, Av Prof Lineu Prestes 2242,Cidade Univ, Sao Paulo, SP, Brazil
[2] Univ Sao Paulo, Inst Geociencias, Sao Paulo, SP, Brazil
关键词
Nanostructured coating; Chromium carbide; Erosion-oxidation; Hardness; Thermal spraying; SOLID PARTICLE EROSION; MECHANICAL-PROPERTIES; CARBIDE COATINGS; CORROSION; MICROSTRUCTURE; BEHAVIOR; PLASMA; FE; SUPERALLOYS; REFINEMENT;
D O I
10.1590/1980-5373-MR-2015-0611
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study reports the high temperature erosion-oxidation (E-O) behavior of conventional and nanostructured Cr3C2-25(Ni-20Cr) coatings prepared by high velocity oxygen fuel (HVOF) spraying. As-received and nanostructured Cr3C2-25(Ni-20Cr) powders with mean crystallite sizes of 145 nm and 50 nm respectively, were used to prepare 120-200 mu m thick coatings on AISI 310 samples. The E-O behavior of the coatings prepared with the as-received (AR) and nanostructured (NS) powders was determined as weight change in a custom designed rig at room temperature, 450, 700 and 800 degrees C. The Vickers microhardness, Young's Modulus and fracture toughness of the AR and NS coatings were determined, and the NS coatings exhibited higher values compared with the AR coatings. The E-O resistance of the NS coating was higher than that of AR coating at all temperatures, and particularly at 800 degrees C. The increase in E-O resistance of the NS coatings is due to its superior mechanical properties as well as to the presence of some heterogeneities in the AR coatings. The E-O mechanisms of both types of the coatings are discussed, with special attention to that at high temperatures. The results suggest that at 800 degrees C the E-O process is controlled by erosion of the oxide.
引用
收藏
页码:994 / 1002
页数:9
相关论文
共 50 条
  • [31] Resistance to slurry erosion by WC-10Co-4Cr and Cr3C2-25(Ni20Cr) coatings deposited by HVOF stainless steel F6NM
    Maekai, Ishfaq Amin
    Harmain, G. A.
    Zehab-ud-Din
    Masoodi, J. H.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 105
  • [32] Structural and mechanical properties of HVOF sprayed Cr3C2-25%NiCr coating and subsequent erosion wear resistance
    Tailor, Satish
    Vashishtha, Nitesh
    Modi, Ankur
    Modi, S. C.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (07)
  • [33] Production of Nanocrystalline Ni-20Cr Coatings for High-Temperature Applications
    Manoj Kumar
    Harpreet Singh
    Narinder Singh
    Journal of Thermal Spray Technology, 2014, 23 : 692 - 707
  • [34] High temperature erosion-oxidation of Cr3C2-NiCr thermal spray coatings under simulated turbine conditions
    Matthews, S.
    James, B.
    Hyland, M.
    CORROSION SCIENCE, 2013, 70 : 203 - 211
  • [35] Production of Nanocrystalline Ni-20Cr Coatings for High-Temperature Applications
    Kumar, Manoj
    Singh, Harpreet
    Singh, Narinder
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2014, 23 (04) : 692 - 707
  • [36] STEM analysis of the transient oxidation of a Ni-20Cr alloy at high temperature
    Ahmad, B
    Fox, P
    OXIDATION OF METALS, 1999, 52 (1-2): : 113 - 138
  • [37] Erosion corrosion of thermally sprayed Fe12Cr and Cr3C2-NiCr coatings
    Hjörnhede, A
    Olefjord, I
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 5, PTS 1 AND 2, 2001, 369-3 : 507 - 514
  • [38] High temperature oxidation of Ni-20Cr alloy under compressive stress
    Zhou, C. H.
    Zhang, H.
    Guan, X. G.
    Pan, R. Y.
    Sun, F. J.
    Mao, N. N.
    2018 INTERNATIONAL CONFERENCE ON CONSTRUCTION, AVIATION AND ENVIRONMENTAL ENGINEERING, 2019, 233
  • [39] High-temperature oxidation studies of cold-sprayed Ni-20Cr and Ni-50Cr coatings on SAE 213-T22 boiler steel
    Bala, Niraj
    Singh, Harpreet
    Prakash, Satya
    APPLIED SURFACE SCIENCE, 2009, 255 (15) : 6862 - 6869
  • [40] STEM Analysis of the Transient Oxidation of a Ni-20Cr Alloy at High Temperature
    B. Ahmad
    P. Fox
    Oxidation of Metals, 1999, 52 : 113 - 138