Elevated-Temperature Mechanical Properties of Lead-Free Sn-0.7Cu-xSiC Nanocomposite Solders

被引:13
|
作者
Mohammadi, A. [1 ]
Mahmudi, R. [1 ]
机构
[1] Univ Tehran, Coll Engn, Sch Met & Mat Engn, Tehran, Iran
关键词
Lead-free solder; nanocomposite solder; SiC nanoparticles; shear punch test; SHEAR-PUNCH; MICROSTRUCTURE; TENSILE; AG; NANOPARTICLES; STRENGTH; ALLOY; CREEP; CU; MICROHARDNESS;
D O I
10.1007/s11664-017-5923-9
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Mechanical properties of Sn-0.7 wt.%Cu lead-free solder alloy reinforced with 0 vol.%, 1 vol.%, 2 vol.%, and 3 vol.% 100-nm SiC particles have been assessed using the shear punch testing technique in the temperature range from 25 degrees C to 125 degrees C. The composite materials were fabricated by the powder metallurgy route by blending, compacting, sintering, and finally extrusion. The 2 vol.% SiC-containing composite showed superior mechanical properties. In all conditions, the shear strength was adversely affected by increasing test temperature, and the 2 vol.% SiC-containing composite showed superior mechanical properties. Depending on the test temperature, the shear yield stress and ultimate shear strength increased, respectively, by 3 MPa to 4 MPa and 4 MPa to 5.5 MPa, in the composite materials. The strength enhancement was mostly attributed to the Orowan particle strengthening mechanism due to the SiC nanoparticles, and to a lesser extent to the coefficient of thermal expansion mismatch between the particles and matrix in the composite solder. A modified shear lag model was used to predict the total strengthening achieved by particle addition, based on the contribution of each of the above mechanisms.
引用
收藏
页码:1721 / 1729
页数:9
相关论文
共 50 条
  • [31] Properties and microstructure of Sn–0.7Cu–0.05Ni lead-free solders with rare earth Nd addition
    Shuang Liu
    Song-bai Xue
    Su-juan Zhong
    Ying-ying Pei
    Hua-wei Sun
    Journal of Materials Science: Materials in Electronics, 2019, 30 : 1400 - 1410
  • [32] Temperature dependence of anelastic properties in Sn–Ag–Cu system and Sn-3.5Ag alloys of lead-free solders
    Y. Nakamura
    T. Ono
    Journal of Materials Science, 2005, 40 : 3267 - 3269
  • [33] Mechanical properties and corrosion analysis of lead-free Sn-0.7Cu solder CSI joints on Cu substrate
    Sonawane, Pushkaraj D.
    Raja, V. K. Bupesh
    Gupta, Manoj
    MATERIALS TODAY-PROCEEDINGS, 2021, 46 : 1101 - 1105
  • [34] Properties of Sn-Zn alloys as lead-free solders
    School of Materials Science and Engineering, Nanchang University, Nanchang 330031, China
    Zhongguo Youse Jinshu Xuebao, 2006, 12 (1993-1998):
  • [35] Experimental and theoretical analysis of the classification of Sn0.3Ag0.7Cu lead-free solders powder
    Dong, L. L.
    Jin, Q.
    Liu, X.
    Ahangarkani, M.
    Zheng, C. H.
    Zhang, Y. S.
    VACUUM, 2018, 156 : 277 - 282
  • [36] Microstructures and Properties of Sn-Bi-In Low-temperature Lead-free Solders
    Li Qin
    Lei Yongping
    Fu Hanguang
    Lin Jian
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (10) : 3038 - 3042
  • [37] Interfacial reactions of Sn-58Bi and Sn-0.7Cu lead-free solders with Alloy 42 substrate
    Yen, Yee-Wen
    Syu, Ruo-Syun
    Chen, Chih-Ming
    Jao, Chien-Chung
    Chen, Guan-Da
    MICROELECTRONICS RELIABILITY, 2014, 54 (01) : 233 - 238
  • [38] Thermodynamic characteristics, microstructure and mechanical properties of Sn-0.7Cu-xIn lead-free solder alloy
    Tian, Shuang
    Li, Saipeng
    Zhou, Jian
    Xue, Feng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 742 : 835 - 843
  • [39] Mechanical characterization of Sn-Ag-based lead-free solders
    Amagai, M
    Watanabe, M
    Omiya, M
    Kishimoto, K
    Shibuya, T
    MICROELECTRONICS RELIABILITY, 2002, 42 (06) : 951 - 966