Ceria-tungsten-tin oxide catalysts with superior regeneration capacity after sulfur poisoning for NH3-SCR process

被引:17
|
作者
Liu, Jingjing [1 ]
Shi, Xiaoyan [1 ,2 ]
Lv, Zhihui [1 ]
Yu, Yunbo [1 ,2 ,3 ]
He, Hong [1 ,2 ,3 ]
机构
[1] Chinese Acad Sci, Res Ctr Ecoenvironm Sci, State Key Joint Lab Environm Simulat & Pollut Con, Beijing 100085, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
[3] Chinese Acad Sci, Ctr Excellence Reg Atmospher Environm, Inst Urban Environm, Xiamen 361021, Peoples R China
基金
中国国家自然科学基金;
关键词
LOW-TEMPERATURE NH3-SCR; NO OXIDATION; CALCINATION TEMPERATURE; THERMAL-DECOMPOSITION; SO2; TOLERANCE; ACTIVE-SITES; REDUCTION; SCR; RESISTANCE; NH3;
D O I
10.1039/d2cy00036a
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nowadays, there exists a trade-off between high-temperature thermal stability and low-temperature catalytic activity for metal oxide catalysts for the NH3-SCR reaction, which restricts the practical application of metal oxide catalysts on diesel vehicles for NOx emission control. In this work, we systematically investigated the relationship between catalytic performance and thermal durability over a novel Ce-W-Sn ternary oxide (CeWSnOx) catalyst by varying the calcination temperature over the range 500-900 degrees C. Instead of thermal deactivation, the NH3-SCR performance of the CeWSnOx catalyst was significantly improved by roasting treatment at temperatures as high as 800 degrees C. Additionally, in situ SO2 poisoning led to the loss of the low-temperature activity for the optimized CeWSnOx-800 catalyst. The superior thermal stability of the CeWSnOx-800 catalyst and the poor thermal stability of the formed sulfates, however, made full thermal regeneration of the sulfur-poisoned catalyst feasible below 700 degrees C. The anti-sintering characteristics, SO2 poisoning mechanism and thermal regeneration capacity after SO2 poisoning of the CeWSnOx-800 catalyst were explored in detail by different characterization methods. We expect that this study can shed some light on the development of Ce-based catalysts for NOx removal from diesel exhaust possessing high thermal stability, catalytic activity and SO2 tolerance.
引用
收藏
页码:2471 / 2481
页数:11
相关论文
共 50 条
  • [21] Impact of sulfur oxide on NH3-SCR over Cu-SAPO-34
    Wijayanti, Kurnia
    Andonova, Stanislava
    Kumar, Ashok
    Li, Junhui
    Kamasamudram, Krishna
    Currier, Neal W.
    Yezerets, Aleksey
    Olsson, Louise
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2015, 166 : 568 - 579
  • [22] Enhancing SO2 resistance in vanadium catalysts with tungsten disulfide for NH3-SCR
    Kim, Donghyeok
    Lee, Myeung-Jin
    Choi, Yejin
    Kim, Jongkyoung
    Jeong, Bora
    Ye, Bora
    Cho, Seungho
    Kim, Hong-Dae
    CHEMICAL ENGINEERING JOURNAL, 2025, 506
  • [23] Regeneration of sulfur-poisoned CeO2 catalyst for NH3-SCR of NOx
    Shi, Yun
    Tan, Shan
    Wang, Xiaoxiang
    Li, Meifang
    Li, Sujing
    Li, Wei
    CATALYSIS COMMUNICATIONS, 2016, 86 : 67 - 71
  • [24] Efficient regeneration of Cu-SSZ-13 NH3-SCR catalysts deactivated by Na, P and (Na plus P) poisoning
    Zhang, Shoute
    Tan, Jingyi
    Meng, Ying
    Tang, Xiaomin
    Shan, Yulong
    Du, Jinpeng
    Xia, Dongsheng
    Cai, Weiquan
    Li, Tao
    CHEMICAL ENGINEERING JOURNAL, 2025, 506
  • [25] In situ regeneration of commercial NH3-SCR catalysts with high-temperature water vapor
    Shi, Yao
    Zhang, Pei
    Fang, Tuotuo
    Gao, Erhao
    Xi, Fujuan
    Shou, Tianyu
    Tao, Mengna
    Wu, Siming
    Bernards, Matthew T.
    He, Yi
    Pan, Hua
    CATALYSIS COMMUNICATIONS, 2018, 116 : 57 - 61
  • [26] A dual-functional way for regenerating NH3-SCR catalysts while enhancing their poisoning resistance
    Wang, Yuejun
    Ge, Dongjie
    Chen, Meixiu
    Gao, Shan
    Wu, Zhongbiao
    CATALYSIS COMMUNICATIONS, 2018, 117 : 69 - 73
  • [27] Removal of nitrogen oxides by the NH3-SCR process:: Catalysts based on industrial residues containing iron(III) oxide
    Weisweiler, W
    Mallonn, E
    Görke, O
    CHEMIE INGENIEUR TECHNIK, 2003, 75 (1-2) : 72 - 76
  • [28] Broadening active temperature window for NH3-SCR on tungsten-promoted MnCeOx nanorod catalysts
    Cheng, Kai
    Tang, Sai
    Feng, Junlong
    An, Mingze
    Zhu, Junjiang
    Xia, Minggui
    PROCESS SAFETY AND ENVIRONMENTAL PROTECTION, 2024, 182 : 1 - 10
  • [29] Solvothermal synthesis of well-designed ceria-tin-titanium catalysts with enhanced catalytic performance for wide temperature NH3-SCR reaction
    Zhang, Guodong
    Han, Weiliang
    Zhao, Haijun
    Zong, Luyao
    Tang, Zhicheng
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2018, 226 : 117 - 126
  • [30] SO2 and Pb Poisoning and Regeneration of Mn-Ce/TiO2 Catalysts for NH3-SCR at Low Temperature
    Yan D.
    Chen Z.
    Yu Y.
    Ai S.
    Li J.
    Zhongguo Dianji Gongcheng Xuebao/Proceedings of the Chinese Society of Electrical Engineering, 2022, 42 (19): : 7143 - 7149