Corrosion failure of titanium tubes of a heat exchanger for the heating of dissolving lye

被引:7
|
作者
Romanovski, Valentin [1 ,2 ]
Hedberg, Yolanda S. [3 ,4 ]
Paspelau, Andrei [5 ]
Frantskevich, Vitali [5 ]
Noel, James J. [3 ,4 ]
Romanovskaia, Elena [6 ]
机构
[1] Natl Univ Sci & Technol MISIS, Sci & Res Ctr Funct Nanoceram, Lenin Av 4, Moscow 119049, Russia
[2] Natl Acad Sci Belarus, Inst Gen & Inorgan Chem, Surganova St 9-1, Minsk 220072, BELARUS
[3] Univ Western Ontario, Dept Chem, London, ON N6A 5B7, Canada
[4] Univ Western Ontario, Surface Sci Western, London, ON N6G 0J3, Canada
[5] Belarusian State Technol Univ, Sverdlova St 13, Minsk 220006, BELARUS
[6] Univ Virginia, Dept Mat Sci & Engn, Charlottesville, VA 22904 USA
关键词
Titanium; Corrosion; Heat-exchanger; Chlorine; Sylvinite ore; Cracking; TEMPERATURE; CONDENSERS; LEAKAGE;
D O I
10.1016/j.engfailanal.2021.105722
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Corrosion of titanium heat exchangers in the processing of sylvinite ore is undesirable from economic, safety, and process sustainability perspectives. Triggered by an industrial case, we investigated the extent of corrosion during simulated contact with sylvinite ore (in dissolving lye) in relevant conditions. Detailed characterization of the failed tubes and corrosion products was carried out to understand the mechanism of failure. Corrosion of titanium (Grade 2) tubes was investigated at room temperature, 60, 70, 80, and 90 degrees C. After electrochemical and surface morphology analysis, we found that pitting corrosion of the titanium tube material sharply increased above 80 degrees C in the simulated sylvinite ore environment (pH 7.1). The failure analysis revealed extensive degradation by transgranular cracking through both the oxide and metal matrix, likely caused by a combination of the high temperature, pressure, possible vibrations, the build-up of lye deposits causing crevices, the high salt content of the lye, and possibly metal (copper, iron, zinc) impurities/deposits in or on the titanium metal, which can catalyze hydrogen evolution.
引用
收藏
页数:9
相关论文
共 50 条
  • [21] FAILURE ANALYSIS OF BRASS HEAT EXCHANGER TUBES.
    Serra, Eduardo T.
    Sebrao, Mauro Z.
    Praktische Metallographie/Practical Metallography, 1987, 24 (04): : 186 - 189
  • [22] Failure Analysis of Ethanol Vaporizer Heat Exchanger Tubes
    Sanders, S. A.
    Iwand, H. C.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2013, 13 (03) : 328 - 332
  • [23] Failure analysis of AISI 321 tubes of heat exchanger
    Corte, J. S.
    Rebello, J. M. A.
    Areiza, M. C. L.
    Tavares, S. S. M.
    Araujo, M. D.
    ENGINEERING FAILURE ANALYSIS, 2015, 56 : 170 - 176
  • [24] Failure of heat exchanger tubes due to localized damage
    Malik, MM
    Salam, I
    Tauqir, A
    ENGINEERING PLASTICITY FROM MACROSCALE TO NANOSCALE PTS 1 AND 2, 2003, 233-2 : 151 - 156
  • [25] Failure of heat exchanger tubes in cooling water applications
    van Wijngaarden, R
    RISK, ECONOMY AND SAFETY, FAILURE MINIMISATION AND ANALYSIS: FAILURES 2000, 2000, : 123 - 133
  • [27] ANTI-CORROSION COATINGS FOR HEAT-EXCHANGER TUBES
    BAKALYUK, YK
    PROSKURK.EV
    POLYARUS.VA
    SOLOVEV, GD
    TKACHENK.AS
    SIDORENK.IS
    COKE & CHEMISTRY USSR, 1972, (08): : 58 - 60
  • [28] Failure analysis of stress corrosion cracking in heat exchanger tubes during start-up operation
    Xu, Shugen
    Wang, Chong
    Wang, Weiqiang
    ENGINEERING FAILURE ANALYSIS, 2015, 51 : 1 - 8
  • [29] Failure of hydrocracker heat exchanger tubes in an oil refinery by polythionic acid-stress corrosion cracking
    Tawancy, H. M.
    ENGINEERING FAILURE ANALYSIS, 2009, 16 (07) : 2091 - 2097
  • [30] Effects of Zn Coating and Heat Treatment on the Corrosion of Aluminum Heat Exchanger Tubes
    Cho, Soo Yeon
    Kim, Jae Jung
    Jang, Hee Jin
    CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2019, 18 (01): : 24 - 32