Micro and macroscopic mechanical behaviors of high-density polyethylene under UV irradiation and temperature

被引:36
|
作者
Hsueh, Hsiang-Chun [1 ]
Kim, Jae Hyun [1 ]
Orski, Sara [2 ]
Fairbrother, Andrew [1 ]
Jacobs, Deborah [1 ]
Perry, Lakesha [1 ]
Hunston, Donald [1 ]
White, Christopher [1 ]
Sung, Lipiin [1 ]
机构
[1] NIST, Mat & Struct Syst Div, Engn Lab, Gaithersburg, MD 20899 USA
[2] NIST, Mat Sci & Engn Div, Mat Measurement Lab, Gaithersburg, MD 20899 USA
关键词
UV; Mechanical property; Accelerated weathering test; HDPE; Molar mass; DEGRADATION-INDUCED EMBRITTLEMENT; POLYMERS; DURABILITY; OXIDATION; FILMS; FTIR;
D O I
10.1016/j.polymdegradstab.2020.109098
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The macroscopic mechanical behavior of high-density polyethylene (HDPE) during photodegradation is characterized by decreases of tensile elongation-at-failure. An apparent linear relation between the elongation-at-failure and the molar mass indicates that the decrease of the elongation of HDPE over time is highly dependent on the decrease of the average molar mass. Possible preferential scission of the high molar mass chains was observed for HDPE exposed to ultraviolet (UV) irradiance higher than 40% (61 W/m(2)) of the full intensity at 50 degrees C. Tensile modulus of HDPE exposed at 50 degrees C increased with the exposure time until reaching the complete loss of ductility except the 5% UV. For 40% UV/30 degrees C as well as for 5% UV/50 degrees C, the young modulus trend cannot be evaluated with performed (small) duration. Nanomechanical test results suggest that the increased tensile modulus is due to stiffening of the entire cross-section. Furthermore, HDPE showing the complete loss of ductility exhibited significantly higher modulus in the surface regions than the core regions particularly for the UV intensity higher than 40% (61 W/m(2)), which increased crack sensitivity to cause embrittlement of the entire specimens. Published by Elsevier Ltd.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] THERMAL-MECHANICAL DEGRADATION OF HIGH-DENSITY POLYETHYLENE
    RIDEAL, GR
    PADGET, JC
    JOURNAL OF POLYMER SCIENCE PART C-POLYMER SYMPOSIUM, 1976, (57): : 1 - 15
  • [22] MECHANICAL AND FLOW PROPERTIES OF HIGH-DENSITY POLYETHYLENE LOW-DENSITY POLYETHYLENE BLENDS
    GARCIAREJON, A
    ALVAREZ, C
    POLYMER ENGINEERING AND SCIENCE, 1987, 27 (09): : 640 - 646
  • [23] Photografting of acrylic acid on high density polyethylene by UV irradiation
    Jin, Chaofeng
    Shentu, Baoqing
    Weng, Zhixue
    Huaxue Fanying Gongcheng Yu Gongyi/Chemical Reaction Engineering and Technology, 2004, 20 (02):
  • [24] Mechanical response of buried High-Density Polyethylene pipelines under normal fault motions
    Seyed Abolhasan Naeini
    Elham Mahmoudi
    Mohammad Mahdi Shojaedin
    Mohsen Misaghian
    KSCE Journal of Civil Engineering, 2016, 20 : 2253 - 2261
  • [25] The Influence of Deformation under Tension on Some Mechanical and Tribological Properties of High-Density Polyethylene
    Kujawa, Maciej
    Kowalewski, Piotr
    Wieleba, Wojciech
    POLYMERS, 2019, 11 (09)
  • [26] Mechanical response of buried High-Density Polyethylene pipelines under normal fault motions
    Naeini, Seyed Abolhasan
    Mahmoudi, Elham
    Shojaedin, Mohammad Mahdi
    Misaghian, Mohsen
    KSCE JOURNAL OF CIVIL ENGINEERING, 2016, 20 (06) : 2253 - 2261
  • [27] HIGH-DENSITY POLYETHYLENE
    BESTGEN, F
    KUNSTSTOFFE-GERMAN PLASTICS, 1989, 79 (10): : 904 - 905
  • [28] High-density polyethylene
    不详
    MODERN PLASTICS, 1996, 73 (11): : 116 - 116
  • [29] HIGH-DENSITY POLYETHYLENE
    ALVINE, R
    PLASTICS WORLD, 1971, 29 (08): : 50 - &
  • [30] HIGH-DENSITY POLYETHYLENE
    PRITCHAR.JE
    MARTINOV.RJ
    PLASTICS WORLD, 1972, 30 (11): : 44 - &