The Effect of Al and Ti Transition Metals on the Wear Resistance of Ceramic Based CrN Coatings; Investigation under Ambient Air and Vacuum Conditions

被引:4
|
作者
Sert, Yasar [1 ]
Kucukomeroglu, Tevfik [1 ]
Asl, Hojjat Ghahramanzadeh [1 ]
Goz, Onur [2 ]
机构
[1] Karadeniz Tech Univ, Mech Engn Dept, Trabzon, Turkey
[2] Titanit Corp, Istanbul, Turkey
关键词
Coating; hardness; scratch; wear; vacuum condition; TRIBOLOGICAL BEHAVIOR; MECHANICAL-PROPERTIES; THERMAL-STABILITY; FRICTION; OXIDATION; STEEL; ALCRN; TEMPERATURE; ADHESION; ENERGY;
D O I
10.1177/14644207211046122
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, CrN, CrAlN and CrAlTiN coatings were deposited using the cathodic arc evaporation technique. The structural investigations of these CrN based coatings were performed by scanning electron microscopy, energy dispersive spectroscopy, atomic force microscopy, X-ray diffractometer. The hardness and adhesion strength values of coatings were determined via Vickers type microhardness tester and progressive load scratch tester, respectively. The wear performance of samples was established at ambient air and vacuum condition. All coatings grew in the "T zone" growth model and had a dense and columnar structure. The XRD patterns presented predominantly (220), (110), and (111) reflections. It was demonstrated that the quaternary coating had a higher texture parameter as 0.68, which was related to the highest thickness and hardness. Also, CrAlTiN coatings with the smallest mean crystallite size of similar to 87 nm showed the best hardness, and this ensured relatively high scratch resistance. CrN and CrAlTiN coatings improved wear performance under ambient air condition but were not striking as under vacuum condition. The quaternary coating had a superior performance in the vacuum condition, but due to the high sensitivity of Ti to oxygen, it fell behind the CrN coating under ambient air condition.
引用
收藏
页码:455 / 472
页数:18
相关论文
共 50 条
  • [41] Investigation under conditions of accelerated anodic corrosion of the effect of TiO2 substitution by CeO2 on the stability of Ir-based ceramic coatings
    Alves, VA
    da Silva, LA
    de Oliveira, E
    Boodts, JFC
    ELECTROCHEMICAL METHODS IN CORROSION RESEARCH VI, PTS 1 AND 2, 1998, 289-2 : 655 - 666
  • [42] Wear Resistance of Fe-Based Amorphous Powder Deposited Coatings in Air, Water, and SBF Solution: Effect of Layer Number
    Ji, Xiulin
    Luo, Chanyuan
    Juan, Jin
    Zhao, Jianhua
    Zhang, Yingtao
    TRIBOLOGY TRANSACTIONS, 2022, 65 (03) : 531 - 541
  • [43] Effect of laser cladding Al3Ti-based coatings on the wear and corrosion resistances of AA6063 aluminum alloy
    He, Huan
    Guo, Weihua
    Xiao, Min
    Pang, Xingzhi
    Shen, Xiaoming
    Fu, Yuechun
    Zeng, Jianmin
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING, PTS 1-3, 2013, 652-654 : 1897 - 1903
  • [44] Effect of CeO2 on Microstructure and Wear Resistance of TiC Bioinert Coatings on Ti6Al4V Alloy by Laser Cladding
    Chen, Tao
    Liu, Defu
    Wu, Fan
    Wang, Haojun
    MATERIALS, 2018, 11 (01):
  • [45] Effect of Al content on the structure and oxidation resistance of Y and Al modified silicide coatings prepared on Nb-Ti-Si based alloy
    Zhang, Ping
    Guo, Xiping
    CORROSION SCIENCE, 2013, 71 : 10 - 19
  • [46] Catalytic aerobic oxidation of 2-chloroethyl ethylsulfide, a mustard simulant, under ambient conditions - Effect of solvents, ligands, and transition metals on reactivity
    Boring, E
    Geletii, Y
    Hill, CL
    JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 2001, 176 (1-2) : 49 - 63
  • [47] Tool wear monitoring in milling of titanium alloy Ti-6Al-4 V under MQL conditions based on a new tool wear categorization method
    Hu, Meng
    Ming, Weiwei
    An, Qinglong
    Chen, Ming
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 104 (9-12): : 4117 - 4128
  • [48] Tool wear monitoring in milling of titanium alloy Ti–6Al–4 V under MQL conditions based on a new tool wear categorization method
    Meng Hu
    Weiwei Ming
    Qinglong An
    Ming Chen
    The International Journal of Advanced Manufacturing Technology, 2019, 104 : 4117 - 4128
  • [49] Dynamics of the transition resistance of Al-(Ti, Ni, Mo)-Si type contacts under conditions of non-stationary electrical loads
    Skvortsov, Arkadiy A.
    Koryachko, Marina V.
    Kuleshova, Svetlana I.
    Rybakova, Margarita R.
    JOURNAL OF APPLIED PHYSICS, 2022, 131 (08)
  • [50] Effect of Al content on corrosion resistance of (Ti1-xAlx)N coatings under NaCl deposit in wet oxygen at 600°C
    Feng, Changjie
    Li, Mingsheng
    Xin, Li
    Zhu, Shenglong
    Wang, Fuhui
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 1055 - +