Microstructure evolution and metallurgical characteristic of bead-on-plate TIG welding of Ti-6Al-4V alloy

被引:40
|
作者
Kumar, Kamlesh [1 ]
Masanta, Manoj [1 ]
Sahoo, Santosh Kumar [2 ]
机构
[1] Natl Inst Technol Rourkela, Dept Mech Engn, Rourkela 769008, India
[2] Natl Inst Technol, Dept Met & Mat Engn, Rourkela 769008, India
关键词
Bead-on-plate; TIG welding; Ti-6Al-4V alloy; Microstructure; Residual stress; Texture; MECHANICAL-PROPERTIES; FRICTION STIR; CORROSION BEHAVIOR; RESIDUAL-STRESSES; GRAIN-REFINEMENT; PHASE; TEXTURE; JOINTS; TENSILE;
D O I
10.1016/j.jmatprotec.2018.10.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The bead geometry of autogenous bead-on-plate tungsten inert gas (TIG) welding performed on Ti-6Al-4V alloy inside an argon inert box chamber was measured for different processing conditions. The microstructural evolution of the weldment was evaluated through optical microscopy, scanning electron microscopy (SEM), X-ray diffraction (XRD) technique. The development of residual stress and the texture in the weldment were assessed through the XRD techniques. The full penetration melting for bead-on-plate welding was obtained for high current and low scan speed combination that induces maximum heat input within the experimental domain. Owing to intense heat of the TIG arc, a complex microstructural evolution occurred in the Ti-6Al-4V alloy, which causes transformation of initial beta phase to martensitic alpha' phases. The transformation of initial alpha + beta phase to martensitic alpha' phase enhances the hardness value of the melt pool upto 365 HV0.2, and further at heat affected zone (upto 385 HV0.2) owing to grain refinement. The residual stress developed in the weld melt pool was recorded tensile type, and for increasing the welding current, due to the enhancement of induced heat, the residual stress increased from 140 to 200 MPa (for 80 A) to 240-270 MPa (for 100 A).
引用
收藏
页码:34 / 43
页数:10
相关论文
共 50 条
  • [21] Microstructure evolution and fracture behaviour for electron beam welding of Ti-6Al-4V
    Wu Huiqiang
    Feng Jicai
    He Jingshan
    Bulletin of Materials Science, 2004, 27 (4) : 387 - 392
  • [22] Experimental investigation of pug cutter embedded TIG welding of Ti-6Al-4V titanium alloy
    Deepak Kumar Gope
    Uday Kumar
    Somnath Chattopadhyaya
    Sanjoy Mandal
    Journal of Mechanical Science and Technology, 2018, 32 : 2715 - 2721
  • [23] Experimental investigation of pug cutter embedded TIG welding of Ti-6Al-4V titanium alloy
    Gope, Deepak Kumar
    Kumar, Uday
    Chattopadhyaya, Somnath
    Mandal, Sanjoy
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2018, 32 (06) : 2715 - 2721
  • [24] THE ROUGHNESS IN THE DIFFUSION WELDING OF TI-6AL-4V ALLOY
    ANDRZEJEWSKI, H
    BADAWI, KF
    ROLLAND, B
    WELDING JOURNAL, 1993, 72 (09) : S435 - S439
  • [25] Laser and TIG welding of additive manufactured Ti-6Al-4V parts
    Sen, Murat
    Kurt, Mustafa
    MATERIALS TESTING, 2022, 64 (05) : 656 - 666
  • [26] Microstructural Evolution during Friction Stir Welding of Ti-6Al-4V Alloy
    Mironov, Sergey
    Sato, Yutaka
    Kokawa, Hiroyuki
    STEEL RESEARCH INTERNATIONAL, 2010, 81 (09) : 1100 - 1103
  • [27] TIG welding of Ti6Al4V alloy: Microstructure, fractography, tensile and microhardness data
    Omoniyi, Peter
    Mahamood, Modupe
    Jen, Tien-Chien
    Akinlabi, Esther
    DATA IN BRIEF, 2021, 38
  • [28] Microstructure and properties of the oxynitrided Ti-6Al-4V alloy
    Moskalewicz, T.
    Zimowski, S.
    Kitano, Y.
    Wierzchon, T.
    Czyrska-Filemonowicz, A.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2006, 44 (03): : 133 - 138
  • [29] The microstructure and texture analysis of Ti-6Al-4V alloy through linear friction welding
    Zhao Heng
    Liu Qingbin
    Xie Yaole
    PROCEEDINGS OF THE 2015 INTERNATIONAL CONFERENCE ON MATERIALS, ENVIRONMENTAL AND BIOLOGICAL ENGINEERING, 2015, 10 : 306 - 311
  • [30] Microstructure evolution during high temperature deformation of Ti-6Al-4V alloy
    Luo, Jiao
    Li, Miaoquan
    Yu, Weixin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2010, 39 (08): : 1323 - 1328