Structural study on the development of high-voltage Na4Co3(PO4)2P2O7 cathode materials for sodium-ion batteries by in situ and time-resolved X-ray diffraction

被引:2
|
作者
Kim, Dong Hyun [1 ,2 ]
Kim, Ji-Young [3 ]
Cho, Min Kyung [3 ]
Kim, Hyungseok [1 ,4 ]
Kim, Sang-Ok [1 ,4 ]
Kim, Kwang-Bum [2 ]
Chung, Kyung Yoon [1 ,4 ]
机构
[1] Korea Inst Sci & Technol KIST, Energy Storage Res Ctr, Hwarangno 14 Gil 5, Seoul 02792, South Korea
[2] Yonsei Univ, Dept Mat Sci & Engn, 134 Shinchon Dong, Seoul 03722, South Korea
[3] Korea Inst Sci & Technol KIST, Adv Anal & Data Ctr, Hwarangno 14 Gil 5, Seoul 02792, South Korea
[4] Korea Univ Sci & Technol, KIST Sch, Div Energy & Environm Technol, Seoul 02792, South Korea
关键词
ELECTROCHEMICAL PROPERTIES; THERMAL-STABILITY; INSTABILITY; P2-TYPE;
D O I
10.1039/d2ta01561g
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
As the demand for energy-storage systems grows, lithium sources may become scarce and alternative materials will be required. Sodium-ion batteries (SIBs) are low cost and safe alternatives to lithium-ion batteries (LIBs). Herein, in situ and time-resolved X-ray diffraction (TR-XRD) was used to investigate the structural changes and thermal safety of Na4Co3(PO4)(2)P2O7 cathode materials for high-voltage SIBs. A range of undesirable compounds (Na2Co2P2O7, alpha-NaCoPO4, Na4Co7(PO4)(6), and beta-NaCoPO4) form during heating; therefore, an optimized heating temperature of 740 degrees C was used to obtain Na4Co3(PO4)(2)P2O7. The in situ XRD results showed the dependency of the lattice parameters of Na4Co3(PO4)(2)P2O7 on the Na content during charging and discharging. During the charging process from 4.41 to 4.47 V, lattice constant a showed a significant decrease and b showed a steep increase, whereas c showed a marginal increase. During the charging process from 4.47 to 4.7 V, lattice constant b continued to increase, whereas no significant changes were observed in a and c. The discharge process was evaluated in a reverse order. Na4Co3(PO4)(2)P2O7 exhibited a 6% volume reduction during charging and 4% volume expansion during discharging. The TR-XRD results revealed that the structure of desodiated Na4-xCo3(PO4)(2)P2O7 (x = 2) was decomposed to the Na2CoP2O7 phase at similar to 215 degrees C during heating in the presence of an electrolyte, which was lower than that without electrolyte (similar to 230 degrees C). These results provide an in-depth understanding of Na4Co3(PO4)(2)P2O7 cathode materials and may serve as a basis for the development of high-performance Na4Co3(PO4)(2)P2O7 cathode materials for SIBs.
引用
收藏
页码:17156 / 17165
页数:10
相关论文
共 50 条
  • [41] CoOx(OH)y/C nanocomposites in situ derived from Na4Co3(PO4)2P2O7 as sustainable electrocatalysts for water splitting
    Odynets, Ievgen V.
    Strutynska, Nataliia Yu.
    Li, Junzhi
    Han, Wei
    Zatovsky, Igor V.
    Klyui, N. I.
    DALTON TRANSACTIONS, 2018, 47 (44) : 15703 - 15713
  • [42] Toward Safe and Sustainable Batteries: Na4Fe3(PO4)2P2O7 as a Low Cost Cathode for Rechargeable Aqueous Na-Ion Batteries
    Fernadez-Ropero, Antonio J.
    Zarrabeitia, Maider
    Reynaud, Marine
    Rojo, Teofilo
    Casas-Cabanas, Montse
    JOURNAL OF PHYSICAL CHEMISTRY C, 2018, 122 (01): : 133 - 142
  • [43] High-voltage structural evolution and its kinetic consequences for the Na4MnV(PO4)3 sodium-ion battery cathode material
    Buryak, Nikita S.
    Anishchenko, Dmitrii, V
    Levin, Eduard E.
    Ryazantsev, Sergey, V
    Martin-Diaconescu, Vlad
    Zakharkin, Maxim, V
    Nikitina, Victoria A.
    Antipov, Evgeny, V
    JOURNAL OF POWER SOURCES, 2022, 518
  • [44] Ultrafast biphasic Na5V3(PO4)2(P2O7)2/C composite cathode for sodium-ion batteries
    Bai, Yu
    Liu, Yunyun
    Zhang, Yangyang
    Jiang, Ruisi
    Xiang, Xingde
    CHEMICAL COMMUNICATIONS, 2025, 61 (25) : 4860 - 4863
  • [45] Mo-Doped Na4Fe3(PO4)2P2O7/C Composites for High-Rate and Long-Life Sodium-Ion Batteries
    Chen, Tongtong
    Han, Xianying
    Jie, Mengling
    Guo, Zhiwu
    Li, Jiangang
    He, Xiangming
    MATERIALS, 2024, 17 (11)
  • [46] Hollow-Sphere-Structured Na4Fe3(PO4)2(P2O7)/C as a Cathode Material for Sodium-Ion Batteries
    Zhang, Li-ming
    He, Xiao-dong
    Wang, Shuo
    Ren, Nai-qing
    Wang, Jun-ru
    Dong, Jie-min
    Chen, Fei
    Li, Yi-xuan
    Wen, Zhao-yin
    Chen, Chun-hua
    ACS APPLIED MATERIALS & INTERFACES, 2021, 13 (22) : 25972 - 25980
  • [47] Thermal Stability of NASICON-Type Na3V2(PO4)3 and Na4VMn(PO4)3 as Cathode Materials for Sodium-ion Batteries
    Samigullin, Ruslan R.
    Zakharkin, Maxim V.
    Drozhzhin, Oleg A.
    Antipov, Evgeny V.
    ENERGIES, 2023, 16 (07)
  • [48] A High Voltage Cathode Material for Sodium Batteries: Na3V(PO4)2
    Kovrugin, Vadim M.
    David, Renald
    Chotard, Jean-Noel
    Recham, Nadir
    Masquelier, Christian
    INORGANIC CHEMISTRY, 2018, 57 (15) : 8760 - 8768
  • [49] Galvanostatic stimulated Na3Mn2(P2O7)(PO4) as a high-voltage cathode material for aqueous zinc-ion batteries
    Li, Jiajie
    Kuang, Quan
    Wang, Gang
    Lu, Qiuchen
    Jiang, Pan
    Fan, Qinghua
    Dong, Youzhong
    Zhao, Yanming
    ELECTROCHIMICA ACTA, 2023, 441
  • [50] Na4Co3(PO4)2P2O7, A NEW SODIUM COBALT PHOSPHATE CONTAINING A THREE-DIMENSIONAL SYSTEM OF LARGE INTERSECTING TUNNELS.
    Ruiz-Valero, C.
    Gutierrez-Puebla, E.
    Monge, A.
    Amador, U.
    Parada, C.
    Sanz, F.
    ACTA CRYSTALLOGRAPHICA A-FOUNDATION AND ADVANCES, 1996, 52 : C321 - C321