Liquation and post-weld heat treatment cracking in Rene 80 laser repair welds

被引:35
|
作者
Rush, Matthew T. [1 ]
Colegrove, Paul A. [1 ]
Zhang, Zhu [2 ]
Broad, David [2 ]
机构
[1] Cranfield Univ, Welding Engn & Laser Proc Res Ctr, Cranfield MK43 0AL, Beds, England
[2] Doncasters Grp Ltd, Burton Upon Trent DE14 2WR, Staffs, England
基金
英国工程与自然科学研究理事会;
关键词
Liquation cracking; Nickel superalloy; Laser welding; Strain-age cracking; Post weld heat treatment cracking; Rene; 80; Repair welding; PWHT cracking; NICKEL-BASED SUPERALLOY; INCONEL 738LC SUPERALLOY; WELDABILITY; DEPOSITION;
D O I
10.1016/j.jmatprotec.2011.09.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An extensive experimental study on a nickel-based superalloy, Rene 80 using autogenous laser welding has been undertaken to determine the effect of the process parameters and weld bead geometry on cracking in the as-welded and post-weld heat treated conditions. Little cracking was observed in the as-welded condition with low powers and beam diameters around 2.5 mm. Welding speed had little effect on the incidence of cracking in the as-welded condition. Investigation of the aspect ratio (penetration divided by width) indicated that little cracking occurred in the as-welded condition when the aspect ratio was approximately 0.5. The same effect was observed with the post-weld heat treated samples. An analysis of the microstructures indicated that the cracking was caused primarily by liquation in the as-welded condition and was exacerbated by post-weld heat treatment cracking during the subsequent heat treatment. Finally the study resolved some of the contradictory findings in the literature on the effect of process parameters on the incidence of cracking in the as-welded and post-weld heat treated conditions. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:188 / 197
页数:10
相关论文
共 50 条
  • [21] Effects of post-weld heat treatment on power beam welds in Waspaloy and Udimet 720Li
    Sekhar, NC
    Reed, RC
    TRENDS IN WELDING RESEARCH, PROCEEDINGS, 2003, : 773 - 777
  • [22] Cracking susceptibility after post-weld heat treatment in Haynes 282 nickel based superalloy
    L. O. Osoba
    A. K. Khan
    S. O. Adeosun
    Acta Metallurgica Sinica (English Letters), 2013, 26 : 747 - 753
  • [23] Effect of preweld microstructure on HAZ liquation cracking of Rene 80 superalloy
    Shahsavari, H. A.
    Kokabi, A. H.
    Nategh, S.
    MATERIALS SCIENCE AND TECHNOLOGY, 2007, 23 (05) : 547 - 555
  • [24] Effect of post-weld heat treatment on fusion boundary microstructure in dissimilar metal welds for subsea service
    Fink, Carolin
    Alexandrov, Boian T.
    MATERIALS TESTING, 2017, 59 (06) : 547 - 554
  • [25] RESIDUAL STRESS RELIEF IN POST-WELD HEAT TREATMENT
    Dong, Pingsha
    Hong, Jeong K.
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2008, VOL 6, PT A AND B, 2009, : 321 - 329
  • [26] Liquation cracking in heat affected zone in ni superalloy welds
    Chaturvedi, M. C.
    2006 BIMW: 2006 Beijing International Materials Week, Pts 1-4: MAGNESIUM - ALUMINIUM MATERIALS - AEROSPACE MATERIALS - SUPERCONDUCTING AND FUNCTIONAL MATERIALS, 2007, 546-549 : 1163 - 1170
  • [27] Reduction of environmentally induced cracking of laser-welded shape memory NiTi wires via post-weld heat-treatment
    Chan, C. W.
    Man, H. C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 588 : 388 - 394
  • [28] Influences of post-weld heat treatment on fatigue crack growth behaviour of strength mismatched HSLA steel welds
    Ravi, S
    Balasubramanian, V
    Nasser, SN
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2004, 9 (03) : 246 - 252
  • [29] Effects of post-weld heat treatment cycles on microstructure and mechanical properties of electric resistance welded pipe welds
    Chung, P. C.
    Ham, Yoonjin
    Kim, Sanghoon
    Lim, Jeongho
    Lee, Changhee
    MATERIALS & DESIGN, 2012, 34 : 685 - 690
  • [30] Finite element analysis for the verification of post-weld heat treatment of 9Cr-1Mo welds
    Cheng, W
    Shiwa, M
    Komura, I
    Gotoh, Y
    Takahashi, N
    REVIEW OF PROGRESS IN QUANTITATIVE NONDESTRUCTIVE EVALUATION, VOLS 24A AND 24B, 2005, 760 : 1204 - 1211