Analysis of microstructure and fatigue of cast versus selective laser-melted dental Co-Cr alloy

被引:16
|
作者
Wu, Miaomiao [1 ]
Dong, Xin [1 ]
Qu, Yuntao [1 ]
Yan, Jiazhen [1 ]
Li, Ning [1 ]
机构
[1] Sichuan Univ, Sch Mech Engn, 24 South Rd,Yihuan Rd, Chengdu 610065, Sichuan, Peoples R China
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2022年 / 128卷 / 02期
关键词
MECHANICAL-PROPERTIES; HEAT-TREATMENT; MO; GROWTH; MORPHOLOGY; STRENGTH;
D O I
10.1016/j.prosdent.2022.05.011
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. The forces exerted on teeth and prostheses during mastication are repeated and dynamic, resulting in fatigue damage to dental prostheses. Most fractures of dental restorations are fatigue failure. The 4-point bend fatigue behavior of Co-Cr-Mo-W alloys manufactured by investment casting (CAST) and selective laser melting (SLM) has received little attention. Purpose. The purpose of this in vitro study was to evaluate the 4-point bend fatigue property of dental Co-Cr alloys and determine the relationship between microstructure and the 4-point bend fatigue property of Co-Cr alloys created by traditional casting and SLM. These can guide the use of Co-Cr alloy in dentistry. Material and methods. Co-Cr-Mo-W alloys were fabricated with a dimension of 45x2x2 mm by investment casting and SLM. The 3-point bend test measured the ultimate bend strength with 3 specimens in each group. The 4-point bend fatigue test evaluated the fatigue life under various stresses, with 6 specimens in each group. The specimens were mechanically ground, polished, and electrochemically etched. Scanning electron microscopy was used to identify the microstructures of both etched specimens and fracture surfaces. X-ray diffraction investigations were used to determine the phases. Significant differences in the bend strength were analyzed by using the independent samples t test (alpha=.05), and the fatigue test was analyzed with ANCOVA (alpha=.05). Results. The mean +/- standard deviation bend strength of SLM specimens was 1837 +/- 3 MPa, higher than the 1200 +/- 6 MPa for CAST specimens (P<.05). The maximum bend stress of the SLM specimens without fatigue failure was 735 MPa, which was statistically higher than the 394 MPa for CAST specimens (P<.05). The microstructure characteristics of the SLM alloy contributed to its excellent fatigue performance. In SLM alloy, the gamma phase constituted the majority with some epsilon and Laves phases, while the cast alloy possessed higher epsilon and Laves phases. The grains of SLM alloy were equiaxed and fine, and the second phases were fine and dispersive. In contrast, the cast alloy possessed clear dendrites, and the second phases were sizable. Conclusions. The SLM dental Co-Cr-Mo-W alloy had statistically better 4-point bend fatigue properties than cast alloy, which was associated with an improved microstructure.
引用
收藏
页码:218.e1 / 218.e7
页数:7
相关论文
共 50 条
  • [31] Investigating the Structure, Microstructure, and Texture in Selective Laser-Melted Sterling Silver 925
    R. J. Vikram
    L. Kollo
    K. G. Prashanth
    Satyam Suwas
    Metallurgical and Materials Transactions A, 2021, 52 : 5329 - 5341
  • [32] Investigating the Structure, Microstructure, and Texture in Selective Laser-Melted Sterling Silver 925
    Vikram, R. J.
    Kollo, L.
    Prashanth, K. G.
    Suwas, Satyam
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2021, 52 (12): : 5329 - 5341
  • [33] Hot compression behavior and microstructure of selectively laser-melted IN718 alloy
    Ahmad Mostafa
    Davood Shahriari
    Ignacio Picazo Rubio
    Vladimir Brailovski
    Mohammad Jahazi
    Mamoun Medraj
    The International Journal of Advanced Manufacturing Technology, 2018, 96 : 371 - 385
  • [34] Hot compression behavior and microstructure of selectively laser-melted IN718 alloy
    Medraj, Mamoun (mmedraj@encs.concordia.ca), 2018, Springer London (96): : 1 - 4
  • [35] Electrochemical behavior of Co-Cr and Ni-Cr dental cast alloys
    Viswanathan S. SAJI
    Han-Cheol CHOE
    TransactionsofNonferrousMetalsSocietyofChina, 2009, 19 (04) : 785 - 790
  • [36] Electrochemical behavior of Co-Cr and Ni-Cr dental cast alloys
    Saji, Viswanathan S.
    Choe, Han-Cheol
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 (04) : 785 - 790
  • [37] Effect of the Laser Scan Rate on the Microstructure, Magnetic Properties, and Microhardness of Selective Laser-Melted FeSiB
    Alleg, Safia
    Drablia, Rima
    Fenineche, Nouredine
    JOURNAL OF SUPERCONDUCTIVITY AND NOVEL MAGNETISM, 2018, 31 (11) : 3565 - 3577
  • [38] Effect of the Laser Scan Rate on the Microstructure, Magnetic Properties, and Microhardness of Selective Laser-Melted FeSiB
    Safia Alleg
    Rima Drablia
    Nouredine Fenineche
    Journal of Superconductivity and Novel Magnetism, 2018, 31 : 3565 - 3577
  • [39] Influence of erbium addition on the defects of selective laser-melted 7075 aluminium alloy
    Zhang, Xuhui
    Xiao, Zhen
    Yu, Wenhui
    Chua, Chee Kai
    Zhu, Lihua
    Wang, Zongshen
    Xue, Peng
    Tan, Shuai
    Wu, Yongling
    Zheng, Hongyu
    VIRTUAL AND PHYSICAL PROTOTYPING, 2022, 17 (02) : 406 - 418
  • [40] Ion release and biocompatibility of Co-Cr alloy fabricated by selective laser melting from recycled Co-Cr powder: An in vitro study
    Aldhohrah, Taghrid
    Yang, Jiajun
    Guo, Jiawen
    Zhang, Hui
    Wang, Yan
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (03): : 393 - 401