Friction and Wear Behaviors of Fe-19Cr-15Mn-0.66N Steel at High Temperature

被引:8
|
作者
Sheng, Shaolong [1 ]
Zhou, Huiling [1 ]
Wang, Xiaojing [1 ]
Qiao, Yanxin [1 ,2 ]
Yuan, Hongtao [3 ]
Chen, Jian [1 ,4 ]
Yang, Lanlan [1 ]
Wang, Dongpeng [1 ]
Liu, Zhenguang [1 ]
Zou, Jiasheng [1 ]
Zheng, Zhibin [2 ]
Li, Jingyong [1 ]
机构
[1] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engn, Zhenjiang 212003, Jiangsu, Peoples R China
[2] Guangdong Acad Sci, Inst New Mat, Guangzhou 510650, Peoples R China
[3] Shanghai Waigaoqiao Shipbldg Co Ltd, Shanghai 200137, Peoples R China
[4] Western Univ, Dept Chem, 1151 Richmond St, London, ON N6A 5B7, Canada
基金
中国国家自然科学基金;
关键词
high-nitrogen austenitic stainless steel; wear; friction coefficient; high temperature; AUSTENITIC STAINLESS-STEEL; SLIDING WEAR; TRIBOLOGICAL BEHAVIOR; HIGH-NITROGEN; NICKEL-FREE; MICROSTRUCTURE; LOAD; DEFORMATION; PERFORMANCE; MECHANISMS;
D O I
10.3390/coatings11111285
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The friction and wear behaviors of Fe-19Cr-15Mn-0.66N steel were investigated under applied loads of 5 N and 15 N at the wear-testing temperatures of 300 & DEG;C and 500 & DEG;C using a ball-on-disc tribometer. The wear tracks were evaluated by scanning electron microscopy (SEM) and laser scanning confocal microscopy (LSCM) to reveal the variation in morphologies. Energy-dispersive X-ray spectroscopy (EDS) and X-ray photoelectron spectroscopy (XPS) were used to determine the components of oxide layers formed on wear surfaces. The results demonstrated that the oxide layers are favorable for obtaining a low friction coefficient under all conditions. The average friction coefficient decreased with increasing load at 300 & DEG;C, while it increased with the increase in applied load at 500 & DEG;C. At 300 & DEG;C, severe abrasive wear characterized by grooves resulted in a high friction coefficient with 5 N applied, whereas the formation of a denser oxide layer consisting of Cr2O3, FeCr2O4, Fe2O3, etc., and the increased hardness caused by work hardening led to a decrease in friction characterized by mild adhesive wear. At 500 & DEG;C, the transformation of Fe2O3 to the relatively softer Fe3O4 and the high production of lubricating Mn2O3 resulted in a minimum average friction coefficient (0.34) when 5 N was applied. However, the softening caused by high temperature weakened the hardening effect, and thus the friction coefficient increased with 15 N applied at 500 & DEG;C.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] FRICTION AND WEAR BEHAVIORS OF A HIGH NITROGEN AUSTENITIC STAINLESS STEEL Fe-19Cr-15Mn-0.66N
    Qiao, Y-X
    Sheng, S-L
    Zhang, L-M
    Chen, J.
    Yang, L-L
    Zhou, H-L
    Wang, Y-X
    Li, H-B
    Zheng, Z-B
    [J]. JOURNAL OF MINING AND METALLURGY SECTION B-METALLURGY, 2021, 57 (02) : 285 - 293
  • [2] Cavitation erosion-corrosion behaviour of Fe-19Cr-15Mn-0.66 N high nitrogen austenitic stainless steel in sodium chloride solution
    Li, Liang
    Qiao, Yanxin
    Zhou, Huiling
    Li, Xin
    Huang, Lei
    Yang, Lanlan
    Wang, Lei
    [J]. PHYSICA SCRIPTA, 2023, 98 (06)
  • [3] Fe-19Cr-15Mn-0.66N高氮钢在空气和0.5mol/L NaCl溶液中的腐蚀磨损行为
    王兰
    张维
    葛炼伟
    王欣怡
    乔岩欣
    [J]. 腐蚀与防护, 2022, 43 (05) : 11 - 17
  • [4] Effect of aging treatment on microstructure and corrosion behavior of a Fe-18Cr-15Mn-0.66N stainless steel
    Qiao, Yanxin
    Wang, Xinyi
    Yang, Lanlan
    Wang, Xiaojing
    Chen, Jian
    Wang, Zhengbin
    Zhou, Huiling
    Zou, Jiasheng
    Wang, Fuhui
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 107 : 197 - 206
  • [5] Effect of aging treatment on microstructure and corrosion behavior of a Fe-18Cr-15Mn-0.66N stainless steel
    Yanxin Qiao
    Xinyi Wang
    Lanlan Yang
    Xiaojing Wang
    Jian Chen
    Zhengbin Wang
    Huiling Zhou
    Jiasheng Zou
    Fuhui Wang
    [J]. Journal of Materials Science & Technology, 2022, 107 (12) : 197 - 206
  • [6] Effect of Shot Peening on Friction and Wear Behaviors of Cr-Ni-Mo High Strength Steel
    Zhang, Yalong
    Wu, Luji
    He, Xiaofei
    Wang, Zhen
    Qu, Shengguan
    Qin, Haidi
    [J]. Mocaxue Xuebao/Tribology, 2023, 43 (09): : 1072 - 1082
  • [7] Mossbauer effect and neutron scattering in austenitic high nitrogen steel Fe-19Cr-19Mn-0.9N
    Nadutov, VM
    Garamus, VM
    Islamov, AK
    [J]. HIGH NITROGEN STEELS '98, 1999, 318-3 : 321 - 326
  • [8] Effect of heat treatment on wear resistance of Fe-Cr-Mn-C-N high-interstitial stainless steel
    Lee, Eunkyung
    Mishra, Brajendra
    Palmer, Bruce R.
    [J]. WEAR, 2016, 368 : 70 - 74
  • [9] Friction and wear properties of sintered Fe-Cr-Cu powder material at high temperature
    Ozaki, K
    Tanaka, T
    Goto, M
    Takeichi, Y
    Uemuka, M
    [J]. JOURNAL OF JAPANESE SOCIETY OF TRIBOLOGISTS, 2004, 49 (11) : 859 - 866
  • [10] The Microstructure Refinement and Mechanical Properties Improving of Friction Stir Processed Fe–Mn–Cr–N Steel
    Fengming Qin
    Tong Yang
    Yajie Li
    Huiqin Chen
    Xiaodong Zhao
    [J]. Metallurgical and Materials Transactions A, 2024, 55 : 2034 - 2053