Influence of Ultrasonic Surface Rolling on Microstructure and Wear Behavior of Selective Laser Melted Ti-6Al-4V Alloy

被引:56
|
作者
Wang, Zhen [1 ]
Xiao, Zhiyu [1 ,2 ]
Huang, Chuanshou [1 ]
Wen, Liping [1 ,2 ]
Zhang, Weiwen [1 ,2 ]
机构
[1] South China Univ Technol, Natl Engn Res Ctr Near Net Shape Forming Metall M, Guangzhou 510640, Guangdong, Peoples R China
[2] South China Univ Technol, Guangdong Key Lab Adv Metall Mat Proc, Guangzhou 510640, Guangdong, Peoples R China
关键词
selective laser melting; Ti-6Al-4V; ultrasonic surface rolling process; microstructure and properties; wear; MECHANICAL-PROPERTIES; TRIBOLOGICAL PROPERTIES; FRETTING WEAR; TITANIUM; EVOLUTION; NANOINDENTATION; MARTENSITE; RESISTANCE; JOINT; TI;
D O I
10.3390/ma10101203
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The present article studied the effect of ultrasonic surface rolling process (USRP) on the microstructure and wear behavior of a selective laser melted Ti-6Al-4V alloy. Surface characteristics were investigated using optical microscope, nano-indentation, scanning electron microscope, transmission electron microscope and laser scanning confocal microscope. Results indicated that the thickness of pore-free surfaces increased to 100 similar to 200 m with the increasing ultrasonic surface rolling numbers. Severe work hardening occurred in the densified layer, resulting in the formation of refined grains, dislocation walls and deformation twins. After 1000 N 6 passes, about 15.5% and 14.1% increment in surficial Nano-hardness and Vickers-hardness was obtained, respectively. The hardness decreased gradually from the top surface to the substrate. Wear tests revealed that the friction coefficient declined from 0.74 (polished surface) to 0.64 (USRP treated surface) and the wear volume reduced from 0.205 mm(-3) to 0.195 mm(-3). The difference in wear volume between USRP treated and polished samples increased with sliding time. The enhanced wear resistance was concluded to be associated with the improvement of hardness and shear resistance and also the inhibition of delamination initiation.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Surface and property characterization of selective laser-melted Ti-6Al-4V alloy after laser polishing
    Jiejing Li
    Huayang Wu
    Haixu Liu
    Dunwen Zuo
    The International Journal of Advanced Manufacturing Technology, 2023, 128 : 703 - 714
  • [22] High temperature dry sliding wear behaviour of selective laser melted Ti-6Al-4V alloy surfaces
    Praveenkumar, K.
    Vishnu, Jithin
    Samuel, S. Calvin
    Gopal, Vasanth
    Arivarasu, Moganraj
    Lackner, Juergen M.
    Meier, Benjamin
    Karthik, D.
    Suwas, Satyam
    Swaroop, S.
    Prashanth, K. G.
    Yadav, Mayank Kumar
    Manivasagam, Geetha
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2024, 329
  • [23] Microstructure and corrosion performance of plasma electrolytic oxidation coatings on the surface of conventional and selective laser melted Ti-6Al-4V alloy
    Khorasanian, Mehdi
    Yeganeh, Mahdi
    Zaree, Seyed Reza Alavi
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2022, 10 (03)
  • [24] Wear resistance of a laser surface alloyed Ti-6Al-4V alloy
    Jiang, P
    He, XL
    Li, XX
    Yu, LG
    Wang, HM
    SURFACE & COATINGS TECHNOLOGY, 2000, 130 (01): : 24 - 28
  • [25] Study on surface properties of Ti-6Al-4V titanium alloy by ultrasonic rolling
    Ren, Zhaohui
    Li, Zhuhong
    Zhou, Shihua
    Wang, Yunhe
    Zhang, Lu
    Zhang, Ziting
    SIMULATION MODELLING PRACTICE AND THEORY, 2022, 121
  • [26] On the Texture Formation of Selective Laser Melted Ti-6Al-4V
    Simonelli, Marco
    Tse, Yau Yau
    Tuck, Chris
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (06): : 2863 - 2872
  • [27] Static coarsening behaviour of lamellar microstructure in selective laser melted Ti-6Al-4V
    Cao, Sheng
    Hu, Qiaodan
    Huang, Aijun
    Chen, Zhuoer
    Sun, Ming
    Zhang, Jiahua
    Fu, Chenxi
    Jia, Qingbo
    Lim, Chao Voon Samuel
    Boyer, Rodney R.
    Yang, Yi
    Wu, Xinhua
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 35 (08) : 1578 - 1586
  • [28] Influence of beam current on microstructure of electron beam melted Ti-6Al-4V alloy
    Laptev, Roman
    Pushilina, Natalia
    Kashkarov, Egor
    Syrtanov, Maxim
    Stepanova, Ekaterina
    Koptyug, Andrey
    Lider, Andrey
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2019, 29 (04) : 440 - 446
  • [29] On the Texture Formation of Selective Laser Melted Ti-6Al-4V
    Marco Simonelli
    Yau Yau Tse
    Chris Tuck
    Metallurgical and Materials Transactions A, 2014, 45 : 2863 - 2872
  • [30] Effect of Build Orientation on the Microstructure and Mechanical Properties of Selective Laser-Melted Ti-6Al-4V Alloy
    Hartunian, Patrick
    Eshraghi, Mohsen
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2018, 2 (04):