Examination of spent pressurized water reactor fuel rods after 15 years in dry storage

被引:6
|
作者
Einziger, RE
Tsai, HC
Billone, MC
Hilton, BA
机构
[1] Argonne Natl Lab, Argonne, IL 60439 USA
[2] Argonne Natl Lab, Idaho Falls, ID 83403 USA
关键词
spent fuel dry storage; fuel characterization;
D O I
10.13182/NT03-A3439
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
For approximate to 15 yr Dominion Generation's Surry Nuclear Station 15 X 15 Westinghouse pressurized water reactor (PWR) fuel was stored in a dry inert-atmosphere Castor V/21 cask at the Idaho National Environmental and Engineering Laboratory at peak cladding temperatures that decreased from similar to350 to 150degreesC. Before storage, the loaded cask was subjected to thermal-benchmark tests, during which time the peak temperatures were greater than 400degreesC. The cask was opened to examine the fuel rods for degradation and to determine if they were suitable for extended storage. No fuel rod breaches and no visible degradation or crud/oxide spallation from the fuel rod surface were observed. The results from profilometry, gas release measurements, metallographic examinations, microhardness determination, and cladding hydrogen behavior are reported in this paper. It appears that little or no fission gas was released from the fuel pellets during either the thermal-benchmark tests or the long-term storage. In the central region of the fuel column, where the axial temperature gradient in storage is small, the measured hydrogen content in the cladding is consistent with the thickness of the oxide layer. At similar to1 m above the fuel midplane, where a steep temperature gradient existed in the cask, less hydrogen is present than would be expected from the oxide thickness that developed in-reactor. Migration of hydrogen during dry storage probably occurred and may signal a higher-than-expected concentration at the cooler ends of the rod. The volume of hydrides varies azimuthally around the cladding, and at some elevations, the hydrides appear to have segregated somewhat to the inner and outer cladding surfaces. It is, however, impossible to determine if this segregation occurred in-reactor or during transportation, thermal-benchmark tests, or the dry storage period. The hydrides retained the circumferential orientation typical of prestorage PWR fuel rods. Little or no cladding creep occurred during thermal-benchmark testing and dry storage. It is anticipated that the creep would not increase significantly during additional storage because of the lower temperature after 15 yr, continual decrease in temperature from the reduction in decay heat, and concurrent reductions in internal rod pressure and stress. This paper describes the results of the characterization of the fuel and intact cladding, as well as the implications of these results for long-term (i.e., beyond 20 yr) dry-cask storage.
引用
收藏
页码:186 / 200
页数:15
相关论文
共 50 条
  • [1] Suggestion on the safety classification of spent fuel dry storage in China's pressurized water reactor nuclear power plant
    Liu, Ting
    Qu, Yunhuan
    Meng, De
    Zhang, Qiaoer
    Lu, Xinhua
    [J]. 2017 3RD INTERNATIONAL CONFERENCE ON ENVIRONMENTAL SCIENCE AND MATERIAL APPLICATION (ESMA2017), VOLS 1-4, 2018, 108
  • [2] HIGH-TEMPERATURE POST-IRRADIATION MATERIALS PERFORMANCE OF SPENT PRESSURIZED WATER-REACTOR FUEL-RODS UNDER DRY STORAGE-CONDITIONS
    EINZIGER, RE
    ATKIN, SD
    STELLRECHT, DE
    PASUPATHI, V
    [J]. NUCLEAR TECHNOLOGY, 1982, 57 (01) : 65 - 80
  • [3] LOW-TEMPERATURE RUPTURE BEHAVIOR OF ZIRCALOY-CLAD PRESSURIZED WATER-REACTOR SPENT FUEL-RODS UNDER DRY STORAGE-CONDITIONS
    EINZIGER, RE
    KOHLI, R
    [J]. NUCLEAR TECHNOLOGY, 1984, 67 (01) : 107 - 123
  • [4] Delayed hydride cracking of spent fuel rods in dry storage
    Kim, Young Suk
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2008, 378 (01) : 30 - 34
  • [5] Neutronic Characterization for a Pressurized Water Reactor Spent Fuel Assembly
    Abou Alo, Rowayda Fayez M.
    Abdelhady, Amr
    Shaat, Mohamed K.
    [J]. NUCLEAR SCIENCE AND ENGINEERING, 2024, 198 (05) : 1122 - 1130
  • [6] Transport of spent fuel after dry storage
    Dallongeville, Maurice
    Issard, Herve
    Leoni, Elisa
    Zeachandirin, Aravinda
    [J]. NUCLEAR ENGINEERING INTERNATIONAL, 2014, 59 (720): : 23 - 25
  • [7] ON THE VIBRATIONAL BEHAVIOR OF PRESSURIZED WATER-REACTOR FUEL-RODS
    PREUMONT, A
    [J]. NUCLEAR TECHNOLOGY, 1982, 58 (03) : 483 - 491
  • [8] Research on Thermal Safety of Intensive Spent Fuel Dry Storage Facility for Heavy Water Reactor
    Xu Z.
    Ren B.
    Liu Z.
    Wang Z.
    Ye Q.
    Guo W.
    [J]. Hedongli Gongcheng/Nuclear Power Engineering, 2022, 43 (02): : 181 - 188
  • [9] Hydride Reorientation and Delayed Hydride Cracking of Spent Fuel Rods in Dry Storage
    Kim, Young S.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2009, 40A (12): : 2867 - 2875
  • [10] Hydride Reorientation and Delayed Hydride Cracking of Spent Fuel Rods in Dry Storage
    Young S. Kim
    [J]. Metallurgical and Materials Transactions A, 2009, 40 : 2867 - 2875