The influence of thermo-oxidative degradation on the measured interface strength of glass fibre-polypropylene

被引:48
|
作者
Yang, L. [1 ]
Thomason, J. L. [1 ]
Zhu, W. [2 ]
机构
[1] Univ Strathclyde, Dept Mech Engn, Glasgow G1 1XJ, Lanark, Scotland
[2] Univ W Scotland, Sch Engn, Paisley PA1 2BE, Renfrew, Scotland
关键词
Glass fibres; Thermoplastic resin; Adhesion; Mechanical testing; REINFORCED POLYAMIDE 6,6; RESIDUAL THERMAL-STRESSES; COMPOSITES; LENGTH; MICROBOND; DIAMETER; CRYSTALLIZATION; PERFORMANCE; OXIDATION; ADHESION;
D O I
10.1016/j.compositesa.2011.05.011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
It has previously been found that thermal-oxidative degradation of the matrix can strongly affect the apparent interfacial shear strength (IFSS) in glass fibre-polypropylene (GF-PP) measured using the micro-bond method. In this work, different approaches were employed to further investigate this phenomenon. Hot-stage microscopy was used to establish a profile for dimensional loss of molten PP microdroplets during heat treatment. Under a given thermal load this reduction was found to be related to the initial droplet dimensions. A nanoindentation test was employed to directly probe the mechanical properties of the PP microdroplets, which also exhibited strong dimensional dependence in terms of property deterioration caused by the degradation. Characterisation of thermal mechanical properties and crystallinity was carried out on macroscopic PP samples to assist in elucidating how the polymer degradation affected the measured IFSS. Comparison of the degraded and non-degraded PP microbond samples for IFSS clearly showed the effect of thermal-oxidative degradation on adhesion. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1293 / 1300
页数:8
相关论文
共 50 条
  • [31] Mechanism of thermo-oxidative degradation of polyamide
    Li, RF
    Hu, XZ
    ACTA POLYMERICA SINICA, 2000, (02) : 136 - 141
  • [32] Pyrolysis and thermo-oxidative degradation of polycyclopentadiene
    Radhakrishnan, TS
    JOURNAL OF APPLIED POLYMER SCIENCE, 2000, 76 (05) : 635 - 641
  • [33] CHARACTERIZATION OF POLYESTERS - THERMO-OXIDATIVE DEGRADATION
    UGLEA, C
    CORDUNEANU, I
    NEGULESCU, I
    MONATSHEFTE FUR CHEMIE, 1984, 115 (03): : 349 - 356
  • [34] INFLUENCE OF MECHANICALLY INITIATED PROCESSES UPON KINETICS OF THERMO-OXIDATIVE DEGRADATION AND DURABILITY OF ORIENTED POLYPROPYLENE SUBJECTED TO A LOAD
    LIVANOVA, NM
    RAPOPORT, NY
    MILLER, VB
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A, 1978, 20 (08): : 1893 - 1898
  • [35] Long term thermo-oxidative degradation and stabilization of polypropylene (PP) and the implications for its recyclability
    Gijsman, Pieter
    Fiorio, Rudinei
    POLYMER DEGRADATION AND STABILITY, 2023, 208
  • [36] INFLUENCE OF STRUCTURAL FACTORS AND CONDITIONS OF THERMO-OXIDATIVE DESTRUCTION UPON POLYPROPYLENE DURABILITY
    LIVANOVA, NM
    RAPOPORT, NY
    MILLER, VB
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA B, 1978, 20 (07): : 503 - 507
  • [37] Thermo-oxidative degradation of isotactic polypropylene at high temperatures: phenolic antioxidants versus HAS
    Gensler, R
    Plummer, CJG
    Kausch, HH
    Kramer, E
    Pauquet, JR
    Zweifel, H
    POLYMER DEGRADATION AND STABILITY, 2000, 67 (02) : 195 - 208
  • [38] THE INFLUENCE OF THERMO-OXIDATIVE DEGRADATION ON THE BEHAVIOR OF EPOXY SHAPE MEMORY POLYMERS
    Dasharathi, Kannan
    Shaw, John A.
    PROCEEDINGS OF THE ASME CONFERENCE ON SMART MATERIALS ADAPTIVE STRUCTURES AND INTELLIGENT SYSTEMS, 2014, VOL 2, 2014,
  • [39] The thermo-oxidative stability and flammability of wood/polypropylene composites
    Slawomir Borysiak
    Journal of Thermal Analysis and Calorimetry, 2015, 119 : 1955 - 1962
  • [40] Thermo-oxidative stability of polypropylene/layered silicate nanocomposites
    Dominkovics, Zita
    Jozsef Hari
    Fekete, Erika
    Pukanszky, Bela
    POLYMER DEGRADATION AND STABILITY, 2011, 96 (04) : 581 - 587