Viscosity of (GeSe2)x(Sb2Se3)1-x undercooled melts

被引:17
|
作者
Kostal, Petr [1 ]
Malek, Jiri [1 ]
机构
[1] Univ Pardubice, Fac Chem Technol, Dept Chem Phys, Pardubice 53210, Czech Republic
关键词
glass transition; chalcogenides; calorimetry; viscosity and relaxation; fragility; viscosity;
D O I
10.1016/j.jnoncrysol.2007.06.009
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Viscosity of (GeSe2)(x)(Sb2Se3)(1-x) undercooled melts (x = 0.4-0.8) was measured using parallel-plate method and penetration method. By using these two techniques viscosity of the whole measurable region of undercooled melt and of the part of glass region can be measured. In this relatively broad viscosity interval (seven orders of magnitude) all measured samples show Newtonian behavior and the dependence of their viscosity on temperature can be described by a simple Arrhenius equation. The kinetic fragilities calculated from these dependencies show similar compositional dependence as heat capacity changes at glass transition measured by DSC. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:2803 / 2806